Selective Dissolution below the Critical Potential and Back Alloying in Copper-Gold Alloy
Source abstract
Abstract
Below the critical potential, selective dissolution of Cu from Cu-18 atom % Au proceeds via Cu transport through an essentially planar Au-rich product layer, which over time increases to hundreds of atom layers in thickness. Transmission electron micrographs (TEM) taken after the selective dissolution (at and subsequent (current-off) back alloying processes reveal nearly uniform Moiré patterns characteristic of the superposition of two layers with similar crystal structures, i.e. , the Cu-depleted (Au-rich) product layer and the parent alloy. The Moiré fringe spacing decreases with the time of Cu dissolution (for ∼60 s), indicating solid-solution Au enrichment in the product layer during dissolution. The Moiré patterns give no indication of discrete islands of residual Au. The decreasing Cu dissolution rate follows the parabolic law for the first 60 s with an effective diffusivity of Cu in the product layer of at 23°C. The TEMs also show a few pits, whose diameter is in the <10 nm range and whose number increases with time, which may account for the higher rate of Cu dissolution (than given by the parabolic law) after 1 min. © 2001 The Electrochemical Society. All rights reserved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nanoporous metals and alloys · Electrodeposition and Electroless Coatings · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.