journal article·2016-10

Cellular lattices of biomedical Co-Cr-Mo-alloy fabricated by electron beam melting with the aid of shape optimization

Yuichiro Koizumi, Arata Okazaki, Akihiko Chiba, Takahiko Kato, Akihiro Takezawa

Publisher page

Abstract

Abstract With a view to developing a highly biocompatible and highly reliable material for artificial hip joints, cellular lattice structures with high strength and low Young’s modulus ( E ) were designed using computational shape optimization. These structures were fabricated from a biomedical Co-Cr-Mo alloy via electron beam melting. As a starting point for shape optimization, inverse body-centered-cubic (iBCC)-based structures with different porosities and aspects were fabricated. The strength tended to increase with increasing E . Then, the structures were re-designed using shape optimization based on the traction method, targeting a simultaneous increase in yield strength with retention of the low E . The shapes were optimized through minimization of the maximum local von Mises stress and control of E to 3/2 or 2/3 of the original value, while maintaining constant porosity. The re-designed cellular structures were fabricated and subjected to mechanical testing. The E values of the porous structures were comparable to the design values, but the strength of the cellular lattice with E = 2/3 (design value) was lower than expected. This discrepancy was attributed to inhomogeneities in the microstructures and their impact on the lattice mechanical properties. Thus, shape optimization considering crystal orientation is a significant challenge for future research, but this approach has considerable potential.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Cellular and Composite Structures · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Manufacture,-characterisation-and-application-of-cellular-metals-and-metal-foams10.1016/S0079-6425(00)00002-5 ↗
2. Biologic fixation of total hip implants10.2106/00004623-200412002-00015 ↗
3. Park · 2000
4. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
5. Biocompatibility of lotus-type stainless steel and titanium in alveolar bone10.1002/adem.200600124 ↗
6. Fabrication of porous copper with directional pores through thermal decomposition of compounds10.1007/s11661-007-9402-4 ↗
7. Processing and characterization of porous titanium for implants by using NaCl as space holder10.1016/j.jmatprotec.2011.12.015 ↗
8. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
9. Bioactive Ti metal analogous to human cancellous bone: fabrication by selective laser melting and chemical treatments10.1016/j.actbio.2010.09.034 ↗
10. Next-generation biomedical implants using additive manufacturing of complex, cellular and functional mesh arrays10.1098/rsta.2010.0010 ↗
11. Open-cellular Co-base and Ni-base superalloys fabricated by electron beam melting10.3390/ma4040782 ↗
12. Cellular Ti-6Al-4V structures with interconnected macro porosity for bone implants fabricated by selective electron beam melting10.1016/j.actbio.2008.03.013 ↗
13. Generating optimal topologies in structural design using a homogenization method10.1016/0045-7825(88)90086-2 ↗
14. Bendsøe · 2003
15. Sokołowski · 1992
16. Topology optimization for the extruded three dimensional structure with constant cross section10.1299/jsmea.47.198 ↗
17. Topology optimization of an additive layer manufactured (ALM) aerospace part
18. Topology optimization: a tool for the tailoring of structures and materials10.1098/rsta.2000.0528 ↗
19. Efficient design-optimization of variable-density hexagonal cellular structure by additive manufacturing: theory and validation10.1115/1.4028724 ↗
20. Structural and mechanical evaluations of a topology optimized titanium interbody fusion cage fabricated by selective laser melting process10.1002/jbm.a.31231 ↗
21. An integrated approach of topology optimized design and selective laser melting process for titanium implants materials10.3233/BME-130765 ↗
22. Development of porous material using topology optimization and metal 3D printing
23. Domain optimization analysis in linear elastic problems (approach using traction method)
24. Gibson · 1997
25. Structural topology optimization with strength and heat conduction constraints10.1016/j.cma.2014.04.003 ↗
26. Build direction dependence of microstructure and high-temperature tensile property of Co–Cr–Mo alloy fabricated by electron beam melting10.1016/j.actamat.2013.10.017 ↗
27. Phase and grain size inhomogeneity and their influences on creep behavior of Co-Cr-Mo alloy additive manufactured by electron beam melting10.1016/j.actamat.2014.11.012 ↗
28. Effect of phase transformation on tensile behavior of Co-Cr-Mo alloy fabricated by electron-beam melting10.2497/jjspm.61.234 ↗
29. Prototyping of Co-Cr-Mo alloy flat spiral spring by electron beam melting10.2497/jjspm.61.243 ↗
30. Selective electron beam melting of cellular titanium: mechanical properties10.1002/adem.200800137 ↗
31. Next generation orthopaedic implants by additive manufacturing using electron beam melting10.1155/2012/245727 ↗
32. Computational study and experimental validation of porous structures fabricated by electron beam melting: a challenge to avoid stress shielding10.1016/j.msec.2014.08.050 ↗
33. The mechanics of two-dimensional cellular materials
34. Cellular titanium by selective electron beam melting10.1002/adem.200700025 ↗
35. Phase and grain size inhomogeneity and their influences on creep behavior of Co–Cr–Mo alloy additive manufactured by electron beam melting10.1016/j.actamat.2014.11.012 ↗
36. Anomalous strengthening behavior of Co–Cr–Mo alloy single crystals for biomedical applications10.1016/j.scriptamat.2016.06.016 ↗
37. Enhanced Mechanical Properties of As-Forged Co–Cr–Mo–N Alloys with Ultrafine-Grained Structures10.1007/s11661-012-1288-0 ↗
38. Grain refinement of biomedical Co-27Cr-5Mo-0.16N alloy by reverse transformation10.1016/j.matlet.2009.10.001 ↗
39. Effect of Building Position on Phase Distribution in Co–Cr–Mo Alloy Additive Manufactured by EBM10.2497/jjspm.63.10 ↗
40. Role of strain-induced martensitic transformation on extrusion and intrusion formation during fatigue deformation of biomedical Co–Cr–Mo–N alloys10.1016/j.actamat.2014.08.039 ↗
41. Asymmetric slip trace formation in tension/compression cyclic deformation of biomedical Co–Cr–Mo–N alloy with negative stacking fault energy10.1016/j.scriptamat.2013.10.015 ↗
42. Microstructures and mechanical properties of Co-29Cr-6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗