journal article·2020-12

Tribological properties of Al/diamond composites produced by cold spray additive manufacturing

Chaoyue Chen, Yingchun Xie, Xingchen Yan, Mansur Ahmed, Rocco Lupoi, Jiang Wang, Zhongming Ren, Hanlin Liao, Shuo Yin

Publisher page

Abstract

Abstract A range of Al/diamond metal matrix composites using advanced core-shell structured diamond powders was fabricated employing solid-state cold spray additive manufacturing technology. Cold spray technique combined with core-shell structured diamond particles has demonstrated excellent capability to produce dense Al/diamond composites with superior tribological properties. The core-shell structured diamond was easier to deposit than pure Al by cold spray, particularly under low particle impact velocity, implying high potentials as preferential feedstock for cold spray. The wear-resistance performance of the Al/diamond composites produced by nitrogen and helium were investigated. Wear test illustrated that the Al/diamond composites had superior wear-resistance properties comparable to the selective laser meting Inconel 625 and 17−4PH alloys. Higher diamond contents in the composites resulted in better wear resistance. Based on the worn track analysis via X-ray computed tomography, the role of the diamond reinforcement in improving the wear-resistance performance was also clarified.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Interfacial structure evolution of Ti-coated diamond particle reinforced Al matrix composite produced by gas pressure infiltration10.1016/j.compositesb.2017.01.047 ↗
2. Interfacial nano-engineering in Al/diamond composites for thermal management by in situ diamond surface gas desorption10.1016/j.scriptamat.2016.01.004 ↗
3. Reinforcement architectures and thermal fatigue in diamond particle-reinforced aluminum10.1016/j.actamat.2010.08.004 ↗
4. Tailoring interfacial bonding states of highly thermal performance diamond/Al composites: spark plasma sintering vs. Vacuum hot pressing10.1016/j.compositesa.2016.09.012 ↗
5. Fabrication of diamond/aluminum composites by vacuum hot pressing: process optimization and thermal properties10.1016/j.compositesb.2012.11.014 ↗
6. Effect of particle size on the thermal and mechanical properties of aluminum composites reinforced with SiC and diamond10.1016/j.matdes.2015.11.028 ↗
7. Microstructure and thermal properties of Al/W-coated diamond composites prepared by powder metallurgy10.1016/j.matdes.2016.01.085 ↗
8. Processing of Al/SiC composites in continuous solid–liquid co-existent state by SPS and their thermal properties10.1016/j.compositesb.2012.02.004 ↗
9. Thermal conductivity of diamond particle dispersed aluminum matrix composites fabricated in solid–liquid co-existent state by SPS10.1016/j.compositesb.2011.03.028 ↗
10. Effect of metalloid silicon addition on densification, microstructure and thermal–physical properties of Al/diamond composites consolidated by spark plasma sintering10.1016/j.matdes.2014.06.065 ↗
11. A study on graphitization of diamond in copper–diamond composite materials10.1016/S0167-577X(03)00433-6 ↗
12. Beneficial effects of laser irradiation on the deposition process of diamond/Ni60 composite coating with cold spray10.1016/j.apsusc.2015.01.029 ↗
13. Effects of diamond size on the deposition characteristic and tribological behavior of diamond/Ni60 composite coating prepared by supersonic laser deposition10.1016/j.diamond.2015.06.014 ↗
14. Diamond–tungsten based coating–copper composites with high thermal conductivity produced by Pulse Plasma sintering10.1016/j.matdes.2015.03.056 ↗
15. Diamond/aluminum composites processed by vacuum hot pressing: microstructure characteristics and thermal properties10.1016/j.diamond.2012.10.008 ↗
16. Nucleation and growth mechanisms of interfacial Al4C3 in Al/diamond composites10.1016/j.jallcom.2015.10.075 ↗
17. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
18. A review of mechanical properties of additively manufactured Inconel 718
19. On the study of tailorable interface structure in a diamond/Al12Si composite processed by selective laser melting10.1016/j.mtla.2019.100242 ↗
20. Cold spraying – a materials perspective10.1016/j.actamat.2016.06.034 ↗
21. Cold spray additive manufacturing and repair: fundamentals and applications
22. Effect of hot isostatic pressing (HIP) on microstructure and mechanical properties of Ti6Al4V alloy fabricated by cold spray additive manufacturing
23. Deposition of FeCoNiCrMn high entropy alloy (HEA) coating via cold spraying10.1016/j.jmst.2018.12.015 ↗
24. Advanced diamond-reinforced metal matrix composites via cold spray: properties and deposition mechanism10.1016/j.compositesb.2017.01.009 ↗
25. Cold spraying of thermally softened Ni-coated FeSiAl composite powder: microstructure characterization, tribological performance and magnetic property10.1016/j.matdes.2018.09.025 ↗
26. Effect of the powder particle structure and substrate hardness during vacuum cold spraying of Al2O310.1016/j.ceramint.2016.12.085 ↗
27. Microstructure of kinetic spray coatings: a review10.1007/s11666-015-0223-5 ↗
28. High velocity impact induced microstructure evolution during deposition of cold spray coatings: a review10.1016/j.surfcoat.2014.06.006 ↗
29. Review of relationship between particle deformation, coating microstructure, and properties in high-pressure cold spray10.1007/s11666-017-0575-0 ↗
30. Cold spray as an emerging technology for biocompatible and antibacterial coatings: state of art10.1007/s10853-015-9013-1 ↗
31. Solid-state additive manufacturing and repairing by cold spraying: a review10.1016/j.jmst.2017.09.015 ↗
32. A novel spiral trajectory for damage component recovery with cold spray10.1016/j.surfcoat.2016.10.096 ↗
33. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
34. Cold gas dynamic spray technology: a comprehensive review of processing conditions for various technological developments till to date
35. The use of Al–Al2O3 cold spray coatings to improve the surface properties of magnesium alloys10.1016/j.surfcoat.2009.07.032 ↗
36. Microstructure and performance of cold sprayed Al-SiC composite coatings with high fraction of particulates10.1016/j.surfcoat.2016.11.047 ↗
37. Microstructure, mechanical property and wear performance of cold sprayed Al5056/SiCp composite coatings: effect of reinforcement content10.1016/j.apsusc.2013.10.132 ↗
38. The erosion performance of particle reinforced metal matrix composite coatings produced by co-deposition cold gas dynamic spraying10.1016/j.apsusc.2016.10.155 ↗
39. Effect of vacuum heat treatment on microstructure and microhardness of cold-sprayed TiN particle-reinforced Al alloy-based composites10.1016/j.matdes.2010.06.002 ↗
40. Characterizations of cold sprayed TiN particle reinforced Al2319 composite coating10.1016/j.jmatprotec.2007.09.045 ↗
41. Mechanical and microstructural behavior of nanocomposites produced via cold spray10.1016/j.compositesb.2014.07.023 ↗
42. Large sized cubic BN reinforced nanocomposite with improved abrasive wear resistance deposited by cold spray10.1016/j.matdes.2015.06.009 ↗
43. Microstructure, mechanical properties and corrosion performance of 7075 Al matrix ceramic particle reinforced composite coatings produced by the cold gas dynamic spraying process10.1016/j.surfcoat.2013.07.020 ↗
44. Synthesis of nanodiamond-reinforced aluminum metal matrix composites using cold-spray deposition10.1016/j.carbon.2015.01.010 ↗
45. Preparation of diamond reinforced metal powders as thermal spray feedstock using ball milling10.1016/j.surfcoat.2015.12.022 ↗
46. Metallurgical bonding between metal matrix and core-shelled reinforcements in cold sprayed composite coating10.1016/j.scriptamat.2019.09.023 ↗
47. Cold spray deposition of a WC-25Co cermet onto Al7075-T6 and carbon steel substrates10.1016/j.actamat.2012.10.011 ↗
48. Particle acceleration, and heat transfer in cold spray: a review10.1007/s11666-016-0406-8 ↗
49. Effect of substrate temperature on interfacial bonding for cold spray of Ni onto Cu10.1007/s10853-015-9304-6 ↗
50. Influence of particle velocity on adhesion of cold-sprayed splats10.1007/s11666-009-9327-0 ↗
51. Advanced deposition characteristics of kinetic sprayed bronze/diamond composite by tailoring feedstock properties10.1016/j.compscitech.2008.11.015 ↗
52. Novel nanoprocessing route for bulk graphene nanoplatelets reinforced metal matrix nanocomposites10.1016/j.scriptamat.2012.03.013 ↗
53. Studies on wear rate and micro-hardness of the Al/Al2O3/Gr hybrid composites produced via powder metallurgy10.1016/j.compositesb.2014.07.008 ↗
54. Simulation and quantitative assessment of homogeneous and inhomogeneous particle distributions in particulate metal matrix composites10.1046/j.1365-2818.2001.00766.x ↗
55. Fabrication of aluminum–alumina metal matrix composites via cold gas dynamic spraying at low pressure followed by friction stir processing10.1016/j.msea.2012.06.066 ↗
56. Investigation of Al-Al2O3 cold spray coating formation and properties10.1007/s11666-007-9086-8 ↗
57. Synthesis of nanodiamond-reinforced aluminum metal composite powders and coatings using high-energy ball milling and cold spray10.1016/j.carbon.2013.07.001 ↗
58. New insights into the in-process densification mechanism of cold spray Al coatings: low deposition efficiency induced densification10.1016/j.jmst.2018.09.045 ↗
59. Strengthened peening effect on metallurgical bonding formation in cold spray additive manufacturing10.1007/s11666-019-00854-4 ↗