Contour design to improve topographical and microstructural characteristics of Alloy 718 manufactured by electron beam-powder bed fusion technique
Source abstract
Abstract
Abstract Additive manufacturing (AM) processes are being frequently used in industry as they allow the manufacture of complex parts with reduced lead times. Electron beam-powder bed fusion (EB-PBF) as an AM technology is known for its near-net-shape production capacity with low residual stress. However, the surface quality and geometrical accuracy of the manufactured parts are major obstacles for the wider industrial adoption of this technology, especially when enhanced mechanical performance is taken into consideration. Identifying the origins of surface features such as satellite particles and sharp valleys on the parts manufactured by EB-PBF is important for a better understanding of the process and its capability. Moreover, understanding the influence of the contour melting strategy, by altering process parameters, on the surface roughness of the parts and the number of near-surface defects is highly critical. In this study, processing parameters of the EB-PBF technique such as scanning speed, beam current, focus offset, and number of contours (one or two) with the linear melting strategy were investigated. A sample manufactured using Arcam-recommended process parameters (three contours with the spot melting strategy) was used as a reference. For the samples with one contour, the scanning speed had the greatest effect on the arithmetical mean height (Sa), and for the samples with two contours, the beam current and focus offset had the greatest effect. For the samples with two contours, a lower focus offset and lower scan speed (at a higher beam current) resulted in a lower Sa; however, increasing the scan speed for the samples with one contour decreased Sa. In general, the samples with two contours provided a lower Sa (∼22 %) but with slightly higher porosity (∼8 %) compared to the samples with one contour. Fewer defects were detected with a lower scanning speed and higher beam current. The number of defects and the Sa value for the samples with two contours manufactured using the linear melting strategy were ∼85 % and 16 %, respectively, lower than those of the reference samples manufactured using the spot melting strategy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Strand · 2016
2. Influence of laser exposure time and point distance on 75-μm-thick layer of selective laser melted Alloy 71810.1007/s00170-017-1019-1 ↗
3. Effects of processing on microstructure and mechanical properties of a titanium alloy (Ti–6Al–4V) fabricated using electron beam melting (EBM), part 1: distance from build plate and part size10.1016/j.msea.2013.02.064 ↗
4. Effects of processing on microstructure and mechanical properties of Ti-6Al-4V fabricated using electron beam melting (EBM), part 2: energy input, orientation, and location
5. Fabrication and microstructural characterisation of additive manufactured Ti-6Al-4V parts by electron beam melting10.1080/17452759.2015.1008643 ↗
6. Effect of melt scan rate on microstructure and macrostructure for electron beam melting of Ti-6Al-4V
7. Surface oxidation behavior of Ti–6Al–4V manufactured by Electron Beam Melting (EBM®)10.1016/j.jmapro.2014.08.005 ↗
8. Sames V · 2015
9. Microstructure development in electron beam-melted Inconel 718 and associated tensile properties10.1007/s11837-016-1812-6 ↗
10. Additive manufacturing of nickel-based superalloy Inconel 718 by selective electron beam melting: processing window and microstructure10.1557/jmr.2014.192 ↗
11. Grain structure evolution in Inconel 718 during selective electron beam melting10.1016/j.msea.2016.05.046 ↗
12. Karimi Neghlani · 2018
13. Influence of successive thermal cycling on microstructure evolution of EBM-manufactured alloy 718 in track-by-track and layer-by-layer design10.1016/j.matdes.2018.09.038 ↗
14. Influence of build layout and orientation on microstructural characteristics of electron beam melted Alloy 71810.1007/s00170-018-2621-6 ↗
15. Isothermal oxidation behavior of EBM-additive manufactured Alloy 718
16. Characterization of H13 steel produced via electron beam melting10.1108/13552540410512516 ↗
17. Design of novel materials for additive manufacturing—isotropic microstructure and high defect tolerance10.1038/s41598-018-19376-0 ↗
18. Effect of melt parameters on density and surface roughness in electron beam melting of gamma titanium aluminide alloy10.1108/RPJ-12-2014-0187 ↗
19. Effects of processing parameters on surface roughness of additive manufactured Ti-6Al-4V via electron beam melting
20. Evaluation of the surface roughness of additive manufacturing parts based on the modelling of cusp geometry
21. Influence on surface characteristics of electron beam melting process (EBM) by varying the process parameters10.1063/1.5008036 ↗
22. The effect of EBM process parameters upon surface roughness10.1108/RPJ-10-2013-0102 ↗
23. Microstructures and surface roughness of EBM produced Ti-6A1-4V
24. EBM-manufactured single tracks of Alloy 718 : influence of energy input and focus offset on geometrical and microstructural characteristics10.1016/j.matchar.2018.11.033 ↗
25. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
26. Surface roughness of Ti-6Al-4V parts obtained by SLM and EBM: effect on the high cycle fatigue life10.1016/j.proeng.2018.02.010 ↗
27. Characterization and analysis of surface notches on Ti-alloy plates fabricated by additive manufacturing techniques10.1088/2051-672X/3/4/044006 ↗
28. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
29. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
30. Analysis of laser–melt pool–powder bed interaction during the selective laser melting of a stainless steel10.2351/1.4983259 ↗
31. 2 – powder bed fusion processes: an overview
32. Balling phenomena in direct laser sintering of stainless steel powder: metallurgical mechanisms and control methods10.1016/j.matdes.2009.01.013 ↗
33. The influence of process parameters on the surface roughness of a 3D-printed Co–Cr dental alloy produced via selective laser melting10.3390/app6120401 ↗
34. Selective laser melting of Inconel 625 using pulse shaping
35. The effect of laser power and scan speed on melt Pool characteristics of pure titanium and Ti-6Al-4V alloy for selective laser melting
36. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
37. 2019
38. Influence of the focus offset on the defects, microstructure, and mechanical properties of an Inconel 718 superalloy fabricated by electron beam additive manufacturing10.1016/j.jallcom.2018.12.070 ↗
39. Experimental analysis of spatter generation and melt-pool behavior during the powder bed laser beam melting process10.1016/j.jmatprotec.2017.08.012 ↗
40. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
41. Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: a review10.1007/s11465-015-0341-2 ↗
42. Microstructure and anisotropic mechanical properties of EBM manufactured Inconel 718 and effects of post heat treatments10.1016/j.msea.2017.03.085 ↗
43. Körner · 2014
44. Weld metal solidification I: grain structure
45. Kou · 2003
46. Investigations of MX and γ′/γ″ precipitates in the nickel-based superalloy 718 produced by electron beam melting10.1016/j.msea.2007.07.012 ↗
47. Understanding grain evolution in additive manufacturing through modeling