Abstract Metal additive manufacturing processes allow for the production of highly dense parts with increased geometric freedom and less waste than traditional manufacturing techniques. However, one of the biggest challenges in using these parts is the relatively high surface roughness inherent to the manufacturing process. This roughness negatively affects fatigue properties and necessitates the use of post-processing surface treatments. Several methods are presented for improving local surface properties of laser powder bed fusion parts using electrospark deposition (ESD), hammer peening and heat-treatment processes. An optimized surface roughness reduction of 82% and near-surface hardness increase of 85% is obtained. Post-processed Hastelloy X parts reach > 107 cycles during fatigue testing at 350 MPa, in comparison to failure at 105 cycles in the as-built condition. The improvement in mechanical properties obtained with a combined ESD and peening process shows potential for the selective enhancement of critical surface regions in additive manufactured parts.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Coatings · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Fatigue characteristics of steels manufactured by selective laser melting10.1016/j.ijfatigue.2018.12.029 ↗
2. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
3. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
4. Measurements of the boundary layer development along a turbine blade with rough surfaces
5. Performance degradation due to blade surface roughness in a single-stage axial turbine10.1115/1.1811097 ↗
6. Aerodynamic losses of a cambered turbine vane: influences of surface roughness and freestream turbulence intensity10.1115/1.2185125 ↗
7. Surface roughness of selective laser melted Ti-6Al-4V alloy components
8. Identification and characterization of spatter particles and their effect on surface roughness, density and mechanical response of 17-4 PH stainless steel laser powder-bed fusion parts10.1016/j.msea.2019.04.026 ↗
9. On the effect of spatter particles distribution on the quality of Hastelloy X parts made by laser powder-bed fusion additive manufacturing10.1016/j.jmapro.2018.11.012 ↗
10. Orientation dependency for microstructure, geometric accuracy and mechanical properties of selective laser melting AlSi10Mg lattices10.1016/j.jallcom.2019.03.344 ↗
11. Investigation of the accuracy and roughness in the laser powder bed fusion process10.1080/17452759.2018.1426368 ↗
12. The influence of process parameters on vertical surface roughness of the AlSi10Mg parts fabricated by selective laser melting10.1016/j.jmatprotec.2018.10.015 ↗
13. Optimization of scan strategies in selective laser melting of aluminum parts with downfacing areas10.1115/1.4028620 ↗
14. Towards understanding side-skin surface characteristics in laser powder bed fusion10.1557/jmr.2020.125 ↗
15. Machining of additively manufactured parts: implications for surface integrity10.1016/j.procir.2016.02.066 ↗
16. Surface integrity of machined additively manufactured Ti alloys10.1016/j.jmatprotec.2018.04.030 ↗
17. Machinability of nickel-base super alloys: a general review10.1016/S0924-0136(97)00429-9 ↗
18. Comparison of selective laser melting Post-processes based on amplitude and functional surface roughness parameters
19. Laser polishing of parts built up by selective laser sintering10.1016/j.ijmachtools.2007.01.013 ↗
20. Laser polishing of additive manufactured CoCr alloy components with complex surface geometry10.1016/j.jmatprotec.2018.06.019 ↗
21. Finishing of additively manufactured metal parts by abrasive flow machining
22. CFD simulation of the abrasive flow machining process10.1016/j.procir.2015.03.091 ↗
23. Effects of different surface modifications on the fatigue life of selective laser melted 15–5 PH stainless steel10.1016/j.msea.2019.138109 ↗
24. Electropolishing and electropolishing-related allowances for powder bed selectively laser-melted Ti-6Al-4V alloy components10.1016/j.jmatprotec.2016.11.014 ↗
25. Dissolution effects with different microstructures of inconel 718 on surface integrity in electrochemical machining10.1149/2.0761816jes ↗
26. Electrochemical surface finishing10.1149/2.F05143if ↗
27. Design and functional testing of a novel balloon-expandable cardiovascular stent in CoCr alloy produced by selective laser melting10.1016/j.jmapro.2020.03.060 ↗
28. Additive manufacturing of laser cutting nozzles by SLM: processing, finishing and functional characterization10.1108/RPJ-05-2017-0106 ↗
29. Influence of layer thickness and post-process treatments on the fatigue properties of CoCr scaffolds produced by laser powder bed fusion
30. On the effectiveness of different surface finishing techniques on A357.0 parts produced by laser-based powder bed fusion: surface roughness and fatigue strength10.3390/met9121284 ↗
31. Donachie · 2002
32. Effect of microstructure on tensile properties of electrospark deposition repaired Ni-superalloy10.1016/j.msea.2018.05.049 ↗
33. Effect of direct aging on heat-affected zone and tensile properties of electrospark-deposited alloy 71810.1007/s11661-018-4997-1 ↗
34. Davis · 1997
35. Influence of solution heat treatment on microstructure and tensile properties of Inconel 718 formed by high-deposition-rate laser metal deposition10.1016/j.jallcom.2017.11.004 ↗
36. Vit · 2015
37. A study on the effect of a dynamic contact force control for improving electrospark coating properties10.1016/j.surfcoat.2010.02.006 ↗
38. Intensification of the anodic erosion in electrospark alloying by the employment of pulse group10.1016/j.surfcoat.2007.12.037 ↗
39. Weaver · 2017
40. A review of mechanical properties of additively manufactured Inconel 718
41. Analysis of microstructure in electro-spark deposited IN718 superalloy10.1016/j.matchar.2016.07.025 ↗
42. Dendritic coarsening model for rapid solidification of Ni-superalloy via electrospark deposition10.1016/j.jmatprotec.2018.03.023 ↗
43. Reed · 1971
44. Spatter and oxide formation in laser powder bed fusion of Inconel 718
45. Oxide films in laser additive manufactured Inconel 71810.1016/j.actamat.2013.07.039 ↗
46. The effect of pulse energy on the defects and microstructure of electro-spark-Deposited inconel 71810.1007/s11661-019-05332-8 ↗
47. High resolution low kV EBSD of heavily deformed and nanocrystalline Aluminium by dictionary-based indexing10.1038/s41598-018-29315-8 ↗
48. The quenching stress in thermally sprayed coatings10.1016/0040-6090(91)90029-W ↗
49. Quantitative deformation studies using electron back scatter patterns10.1016/0956-7151(91)90037-2 ↗
50. A current T-T-T diagram for wroughtalloy 718
51. Phase precipitation and time–temperature-transformation diagram of Hastelloy X10.1016/S0921-5093(00)01049-2 ↗
52. Long-term ageing characteristics of Hastelloy alloy X10.1007/BF00700780 ↗
53. Laser powder bed fusion of Hastelloy X: effects of hot isostatic pressing and the hot cracking mechanism10.1016/j.msea.2018.07.008 ↗
54. Modelling the influence of machined surface roughness on the fatigue life of aluminium alloy10.1016/j.ijfatigue.2008.06.003 ↗
55. Estimating the fatigue stress concentration factor of machined surfaces10.1016/S0142-1123(02)00012-9 ↗
56. Fatigue life estimation of additive manufactured parts in the as‐built surface condition
57. An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel10.1016/S0142-1123(01)00205-5 ↗
58. Influence of microstructure on fatigueproperties of alloy 718
59. Fatigue crack growth resistant microstructures in polycrystalline Ni-base superalloys for aeroengines10.1016/S0142-1123(98)00087-5 ↗
60. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
61. The effect of lavesphase on the mechanicalproperties of wrought and cast + HIP inconel 718
62. The influence of Laves phases on the high-cycle fatigue behavior of laser additive manufactured Inconel 71810.1016/j.msea.2017.03.098 ↗