Tensile properties of Ti-6Al-4V as-built by laser metal deposition: The relationship between heat affected zone bands, strain localization and anisotropy in ductility
Source abstract
Abstract
Expanded structural applications of additively fabricated or repaired components rely on a thorough understanding of relationships between the anisotropic microstructure and macroscopic mechanical properties. In the present study, Ti‐6Al‐4V as-built by laser metal deposition using a powder feedstock was investigated through an extensive characterization of microstructure, porosity and tensile properties along different loading directions. While no significant anisotropy in strength was noticed, the ductility was observed to vary significantly depending on the loading direction. Higher ductility along the build direction was found to result from strain delocalization using in-situ tensile tests combined with digital image correlation. Differences in mesoscale strain localization patterns stem from a specific distribution of α’ plates in relation to HAZ bands. In addition, the influence of a variety of other features including the crystallographic textures, the β grain morphology, the distance to the free surface, the porosity and the argon shielding during manufacturing on tensile properties was also examined and discussed in light of existing literature.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. Titanium alloys for aerospace applications
2. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
3. Opportunities and issues in the application of titanium alloys for aerospace components10.3390/met10060705 ↗
4. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
5. Analysis of microstructure and mechanical properties of additive repaired Ti–6Al–4V by Direct Energy Deposition10.1016/j.msea.2020.140604 ↗
6. Effect of processing conditions on the microstructure, porosity, and mechanical properties of Ti-6Al-4V repair fabricated by directed energy deposition10.1016/j.jmatprotec.2018.08.041 ↗
7. Remanufacturing of turbine blades by laser direct deposition with its energy and environmental impact analysis10.1016/j.jclepro.2014.05.084 ↗
8. Controlling of residual stress in additive manufacturing of Ti6Al4V by finite element modeling
9. Selective laser melting produced Ti-6Al-4V: post-process heat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
10. Mechanical properties of additive manufactured titanium (Ti–6Al–4V) blocks deposited by a solid-state laser and wire10.1016/j.matdes.2011.06.062 ↗
11. Heat treatment of Ti6Al4V produced by Selective Laser Melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
12. Effects of post heat treatments on microstructures and mechanical properties of selective laser melted Ti6Al4V alloy10.3390/met11101593 ↗
13. Influence of deposition strategy on the microstructure and fatigue properties of laser metal deposited Ti-6Al-4V powder on Ti-6Al-4V substrate10.1016/j.ijfatigue.2019.105236 ↗
14. Influence of powder characteristics on formation of porosity in additive manufacturing of Ti-6Al-4V components10.1007/s11665-017-2796-2 ↗
15. Influence of various process conditions on surface finishes induced by the direct metal deposition laser technique on a Ti–6Al–4V alloy10.1016/j.jmatprotec.2012.11.015 ↗
16. Laser metal deposition of Ti6Al4V—a brief review10.3390/app10030764 ↗
17. Microstructure and mechanical properties of additive manufactured Ti-6Al-4V components by annular laser metal deposition in a semi-open environment10.1016/j.optlastec.2020.106640 ↗
18. Microstructures of laser-deposited Ti–6Al–4V10.1016/j.matdes.2003.09.009 ↗
19. Understanding the microstructure formation of Ti-6Al-4V during direct laser deposition via in-situ thermal monitoring10.1007/s11837-015-1767-z ↗
20. In situ investigation of phase transformations in Ti-6Al-4V under additive manufacturing conditions combining laser melting and high-speed micro-X-ray diffraction10.1038/s41598-017-16760-0 ↗
21. High speed synchrotron X-ray diffraction experiments resolve microstructure and phase transformation in laser processed Ti-6Al-4V10.1080/21663831.2021.1966537 ↗
22. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
23. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
24. Microstructure and texture evolution during solidification processing of Ti–6Al–4V10.1016/S0924-0136(02)00865-8 ↗
25. Microstructure evolution and layer bands of laser melting deposition Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.jallcom.2014.07.161 ↗
26. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
27. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
28. Tensile properties and microstructures of laser-formed Ti-6Al-4V10.1007/s11665-010-9670-9 ↗
29. An overview of additive manufacturing of titanium components by directed energy deposition: microstructure and mechanical properties10.3390/app7090883 ↗
30. Fabrication of large Ti–6Al–4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
31. Quantitative relationship between anisotropic strain to failure and grain morphology in additively manufactured Ti-6Al-4V10.1016/j.msea.2017.09.017 ↗
32. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing
33. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V10.1016/j.msea.2016.07.038 ↗
34. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
35. Additive manufacturing of Ti–6Al–4V parts through laser metal deposition (LMD): Process, microstructure, and mechanical properties10.1016/j.jallcom.2019.04.255 ↗
36. Effect of α texture on the tensile deformation behavior of Ti–6Al–4V alloy produced via electron beam rapid manufacturing10.1016/j.msea.2018.11.012 ↗
37. Effects of the crystallographic and spatial orientation of α lamellae on the anisotropic in-situ tensile behaviors of additive manufactured Ti–6Al–4V10.1016/j.jallcom.2020.156886 ↗
38. Strain localization in Ti-6Al-4V Widmanstätten microstructures produced by additive manufacturing10.1016/j.matchar.2016.10.018 ↗
39. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
40. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
41. The effect of loading direction on strain localisation in wire arc additively manufactured Ti–6Al–4V10.1016/j.msea.2020.139608 ↗
42. Plastic strain localization induced by microstructural gradient in laser cladding repaired structures10.1016/j.tafmec.2020.102520 ↗
43. Characterizing the tensile behavior of additively manufactured Ti-6Al-4V using multiscale digital image correlation10.1016/j.msea.2018.03.091 ↗
44. Digital image correlation analysis of local strain fields on Ti6Al4V manufactured by electron beam melting10.1016/j.msea.2014.09.022 ↗
45. Deformation and failure mechanisms of Ti–6Al–4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
46. Effects of oxygen contamination in the argon shielding gas in laser welding of commercially pure titanium thin sheet10.1007/s10853-005-0447-8 ↗
47. F. Niessen, T. Nyyssönen, A.A. Gazder, R. Hielscher, Parent grain reconstruction from partially or fully transformed microstructures in MTEX, ArXiv210414603 Cond-Mat. (2021). 〈http://arxiv.org/abs/2104.14603〉 (accessed January 10, 2022).
48. Texture analysis with MTEX – free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
49. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium10.1016/S0031-8914(34)80244-3 ↗
50. Ncorr: open-source 2D digital image correlation matlab software10.1007/s11340-015-0009-1 ↗
51. Using transmission Kikuchi diffraction to characterise α variants in an α+β titanium alloy10.1111/jmi.12569 ↗
52. Determination of the structure of α-β interfaces in metastable β-Ti alloys10.1016/j.actamat.2018.03.003 ↗
53. Martensite formation in titanium alloys: crystallographic and compositional effects10.1016/j.jallcom.2021.159636 ↗
54. Lattice correspondance and crystallography of martensites in titanium alloys10.1051/jphyscol:1982441 ↗
55. The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy10.1016/S1359-6454(03)00179-4 ↗
56. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock10.1007/s11837-015-1759-z ↗
57. High cycle fatigue of laser beam deposited Ti-6Al-4V and inconel 718
58. Correlation between microstructures and mechanical properties under tensile and compression tests of heat-treated Ti-6Al–4V ELI alloy produced by additive manufacturing for biomedical applications
59. Boyer · 1994
60. The effect of dissolved nitrogen on the fatigue behavior of Ti-6Al-4V10.1007/s11661-021-06147-2 ↗
61. Effect of interstitial solutes on the strength and ductility of titanium10.1016/0079-6425(81)90001-3 ↗
62. Influence of microtexture on early plastic slip activity in Ti-6Al-4V polycrystals10.1007/s11661-018-4569-4 ↗
63. Microplasticity at room temperature in α/β titanium alloys10.1007/s11661-020-05945-4 ↗
64. On the influence of ageing on the onset of plastic slip in Ti-6Al-4V at room temperature: insight on dwell fatigue behavior10.1016/j.scriptamat.2016.11.042 ↗
65. A three-dimensional crystal plasticity model for duplex Ti–6Al–4V10.1016/j.ijplas.2006.11.006 ↗
66. A size-dependent crystal plasticity finite-element model for creep and load shedding in polycrystalline titanium alloys10.1016/j.actamat.2007.03.017 ↗
67. A 3D analysis of the onset of slip activity in relation to the degree of micro-texture in Ti–6Al–4V10.1016/j.actamat.2019.09.028 ↗
68. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
69. In situ absorption synchrotron measurements, predictive modeling, microstructural analysis, and scanning probe measurements of laser melted Ti-6Al-4V single tracks for additive manufacturing applications10.1016/j.jallcom.2021.163494 ↗
70. Role of geometry on properties of additively manufactured Ti-6Al-4V structures fabricated using laser based directed energy deposition10.1016/j.matdes.2016.05.045 ↗
71. Anisotropic properties of directed energy deposition (DED)-processed Ti–6Al–4V10.1016/j.jmapro.2016.06.020 ↗
72. Directional and oscillating residual stress on the mesoscale in additively manufactured Ti-6Al-4V10.1016/j.actamat.2019.01.050 ↗
73. Study of residual stresses in additively manufactured Ti-6Al-4V by neutron diffraction measurements10.1007/s11661-019-05538-w ↗
74. On the size and orientation effect in additive manufactured Ti-6Al-4V10.1016/j.matdes.2019.108235 ↗