Role of Ferrite and Austenite Phases on the Overall Pitting Behavior of Lean Duplex Stainless Steels in Thiosulfate-Containing Environments

Liang He, Yushu Wang, Preet M. Singh

Publisher page

Abstract

Lean duplex stainless steels UNS S32003 and S82441 were shown to have higher pitting corrosion resistance than UNS S32304 in environments containing chloride and thiosulfate in both potentiodynamic cyclic polarization tests and scratch tests for repassivation. Preferential dissolution of the ferrite phase was observed for UNS S32304 in thiosulfate-containing environments. Individual-ferrite phase and individual-austenite phase were separated from the bulk UNS S32304 through a selective dissolution method. Scratch tests on seperate phases showed that the ferrite phase is more susceptible to localized corrosion than the austenite phase. The ferrite phase is anodic to the austenite phase in hydrochloric acid and the addition of thiosulfate enhanced the galvanic effect between the two phases, which explained the preferential dissolution of the ferrite phase in thiosulfate-containing environments.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Falkland · 2011 · 69510.1002/9780470872864.ch52 ↗
2. Olsson · Desalination · 2007 · 205 · 10410.1016/j.desal.2006.02.051 ↗
3. Choudhary · Corrosion · 2015 · 71 · 114710.5006/1709 ↗
4. Garner · Corrosion · 1985 · 41 · 58710.5006/1.3582988 ↗
5. Laitinen · Corrosion · 1999 · 55 · 85810.5006/1.3284042 ↗
6. Newman · Corrosion · 1982 · 38 · 26110.5006/1.3577348 ↗
7. Newman · Corrosion · 1985 · 41 · 45010.5006/1.3583826 ↗
8. Newman · Corrosion · 1989 · 45 · 28210.5006/1.3577855 ↗
9. Laitinen · Corros. Sci. · 2000 · 42 · 42110.1016/S0010-938X(99)00072-4 ↗
10. Laycock · Corrosion · 1999 · 55 · 59010.5006/1.3280500 ↗
11. Yushu · Corrosion · 2015 · 71 · 93710.5006/1694 ↗
12. Nakhaie · J. Electrochem. Soc. · 2015 · 162 · C12110.1149/2.0041504jes ↗
13. Wang · Corrosion · 2016 · 72 · 62810.5006/1955 ↗
14. Moser · Corros. Sci. · 2012 · 57 · 24110.1016/j.corsci.2011.12.012 ↗
15. He · 2017 · 8
16. He · Metall. Mater. Trans. A · 2019 · 50 · 210310.1007/s11661-019-05189-x ↗
17. Study on the Repassivation Behavior of Steels Using Electrochemical Test Methods10.1520/STP160920170229 ↗
18. Naghizadeh · Corros. Sci. · 2015 · 94 · 17910.1016/j.corsci.2015.01.051 ↗
19. Zhang · Mater. Charact. · 2009 · 60 · 152210.1016/j.matchar.2009.08.009 ↗
20. He · 2017 · 8
21. Zanotto · Corros. Sci. · 2014 · 80 · 20510.1016/j.corsci.2013.11.028 ↗
22. Tsai · Corros. Sci. · 2007 · 49 · 365910.1016/j.corsci.2007.03.035 ↗
23. Lo · Corros. Sci. · 2006 · 48 · 69610.1016/j.corsci.2005.02.004 ↗
24. Bellezze · Corros. Sci. · 2018 · 130 · 1210.1016/j.corsci.2017.10.010 ↗
25. Suzuki · Corrosion · 1973 · 29 · 1810.5006/0010-9312-29.1.18 ↗
26. Newman · Corros. Sci. · 1987 · 27 · 82710.1016/0010-938X(87)90040-0 ↗
27. Newman · Corros. Sci. · 1985 · 25 · 34110.1016/0010-938X(85)90112-X ↗
28. Elbiache · Corros. Sci. · 1992 · 33 · 26110.1016/0010-938X(92)90150-2 ↗
29. Betts · Corros. Sci. · 1993 · 34 · 155110.1016/0010-938X(93)90248-F ↗
30. Bhattacharya · Corrosion · 2008 · 64 · 53210.5006/1.3278489 ↗