journal article·2023-07-01Open access

A Scalable Method for Enhancing the Crystallinity of Zn Powder to Reduce Corrosion and Boost Achievable Capacity

Brian Lenhart, Mike Zuraw, William Mustain

Abstract

Zinc corrosion is an unavoidable phenomenon in alkaline systems. Additives like surfactants and metals at the ppm level are typically included in the zinc-alkaline cell production process to help suppress corrosion. Though these inclusions have helped remediate the issue, the inclusions themselves bring forward new issues such as increased toxicity and cost. Therefore, a method for achieving reduced Zn corrosion that can either complement or replace additives is highly desirable. In this work, a method for the scalable improvement of zinc microparticle crystallinity, without the use of additives, is presented and detailed. The recrystallization process involves oxide film formation, thermal annealing, and oxide film removal. The process converts polycrystalline particles into either a single crystal or one with larger, fewer total grains while conserving particle shape and size. This paper demonstrates reduced corrosion and enhanced achievable capacity for the recrystallized particles as well as improved cyclability. More specifically, the recrystallized particles demonstrate a 19% reduction in corrosion current and a 12% increase in achievable capacity when probed by linear sweep voltammetry and constant current discharge, respectively. When cycled in charge-discharge experiments, the recrystallized particles boast up to a 114% improvement in cyclability.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced battery technologies research · Conducting polymers and applications · Supercapacitor Materials and Fabrication

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Modeling nucleation and growth of zinc oxide during discharge of primary zinc-air batteries10.1016/j.jpowsour.2017.05.073 ↗
2. A review of zinc-based battery from alkaline to acid10.1016/j.mtadv.2021.100149 ↗
3. Corrosion of pure and amalgamated zinc in concentrated alkali hydroxide solutions10.1149/1.2401695 ↗
4. Interfacial parasitic reactions of zinc anodes in zinc ion batteries: Underestimated corrosion and hydrogen evolution reactions and their suppression strategies10.1016/j.jechem.2021.04.016 ↗
5. Tracing the influence of small additions of antimony to zinc on the hydrogen evolution and anodic dissolution processes of zinc as anodes for alkaline batteries application10.1016/j.ijhydene.2021.07.014 ↗
6. Crossroads in the renaissance of rechargeable aqueous zinc batteries10.1016/j.mattod.2020.12.003 ↗
7. Effects of organic corrosion inhibitors on the electrochemical characteristics of zinc in alkaline media10.5006/1.3278462 ↗
8. Electrochemical and surface studies of zinc in alkaline solutions containing organic corrosion inhibitors10.1016/S0378-7753(02)00598-0 ↗
9. On some organic inhibitors of zinc corrosion in alkaline media10.1016/S0010-938X(00)00155-4 ↗
10. Experimental and modeling studies of the hysteresis behavior and dendrite suppression efficacy of an electrolyte additive in zinc electrodeposition10.1149/2.0411913jes ↗
11. Investigation on synergism of composite additives for zinc corrosion inhibition in alkaline solution10.1016/j.matchemphys.2011.02.061 ↗
12. Revealing the effect of polyethylenimine on zinc metal anodes in alkaline electrolyte solution for zinc-air batteries: mechanism studies of dendrite suppression and corrosion inhibition10.1039/D0TA06929A ↗
13. Ramsay · 2011
14. Suppression of dendrite formation and corrosion on zinc anode of secondary aqueous batteries10.1021/acsami.6b16560 ↗
15. Effects of organic additives on zinc electrodeposition from alkaline electrolytes10.1007/s10800-012-0518-x ↗
16. Wang · 1984
17. Electrochemical characterization and mathematical modeling of zinc passivation in alkaline solutions: a review10.1016/j.electacta.2017.03.143 ↗
18. Surface-preferred crystal plane for a stable and reversible zinc anode10.1002/adma.202100187 ↗
19. Impact of anode substrates on electrodeposited zinc over cycling in zinc-anode rechargeable alkaline batteries10.1016/j.electacta.2016.07.041 ↗
20. Surface adsorption of polyethylene glycol to suppress dendrite formation on zinc anodes in rechargeable aqueous batteries10.1002/celc.201800572 ↗
21. Design of highly reversible zinc anodes for aqueous batteries using preferentially oriented electrolytic zinc10.1002/batt.202000112 ↗
22. The secondary alkaline zinc electrode10.1149/1.2085653 ↗
23. Passivation of zinc anodes in alkaline electrolyte: part i. determination of the starting point of passive film formation10.1149/2.0331813jes ↗
24. In-depth structural understanding of zinc oxide addition to alkaline electrolytes to protect aluminum against corrosion and gassing10.1007/s10800-019-01330-1 ↗
25. On the deposition and dissolution of zinc in alkaline solutions10.1149/1.2404188 ↗
26. Enhancing the cycle life of a Zinc–air battery by means of electrolyte additives and zinc surface protection10.3390/batteries4030046 ↗
27. Current density and ZnO precipitation-dissolution distributions in Zn - ZnO porous electrodes and their effect on material redistribution: a two-dimensional mathematical model10.1149/1.2086856 ↗
28. Coupling phenomena between zinc surface morphological variations and ionic mass transfer rate in alkaline solution10.1149/2.083302jes ↗
29. Numerical calculation of ionic mass-transfer rates accompanying anodic zinc dissolution in alkaline solution10.1149/1.3267872 ↗
30. Electrically rechargeable zinc–air batteries: progress, challenges, and perspectives10.1002/adma.201604685 ↗
31. Mathematical modeling of a primary zinc/air battery10.1149/1.2069348 ↗
32. Rechargeable alkaline zinc–manganese oxide batteries for grid storage: Mechanisms, challenges and developments10.1016/j.mser.2020.100593 ↗
33. Retaining the 3D framework of zinc sponge anodes upon deep discharge in Zn-Air cells10.1021/am505266c ↗
34. Electrodeposition of preferentially oriented zinc for flow-assisted alkaline batteries10.1016/j.jpowsour.2014.01.026 ↗
35. The effect of several electrode and electrolyte additives on the corrosion and polarization behavior of the alkaline zinc electrode10.1149/1.2407303 ↗
36. Texture vs morphology in ZnO nano-rods: On the X-ray diffraction characterization of electrochemically grown samples10.1063/1.3669026 ↗
37. Challenges and strategies on Zn electrodeposition for stable Zn-ion batteries10.1016/j.ensm.2021.04.027 ↗
38. Wiring zinc in three dimensions re-writes battery performance - Dendrite-free cycling10.1039/C3EE43754J ↗
39. Ion-sieving carbon nanoshells for deeply rechargeable Zn-based aqueous batteries10.1002/aenm.201802470 ↗
40. Partial deployment of Al in Zn—MnO 2 alkaline battery anodes to improve the capacity and reversibility10.1016/j.jpowsour.2021.230167 ↗
41. Effect of grain size on the electrochemical behavior of pure magnesium anode10.1016/j.jma.2017.09.003 ↗
42. Morphology control of electrodeposited zinc from alkaline zincate solutions for rechargeable zinc air batteries10.1149/1.3507925 ↗
43. Ultrafine- and uniform-grained biodegradable Zn-0.5Mn alloy: Grain refinement mechanism, corrosion behavior, and biocompatibility in vivo10.1016/j.msec.2020.111391 ↗
44. Improved corrosion behavior of nanocrystalline zinc produced by pulse-current electrodeposition10.1016/S0010-938X(03)00142-2 ↗
45. Modified Thornton model for magnetron sputtered zinc oxide: Film structure and etching behaviour10.1016/S0040-6090(03)00949-0 ↗
46. Zn-dust derived ultrafine grained ZnO non-linear ceramic resistors via in situ thermal oxidation of cermet reactant mixture10.1016/j.matdes.2015.12.053 ↗
47. Effect of silica doping on the densification and grain growth in zinc oxide10.1016/j.ceramint.2011.04.017 ↗
48. Improved synthesis of basic zinc acetate, Hexakis(μ-acetato)-μ-oxatetrazinc10.1021/i300010a041 ↗
49. Induction of zinc particles on the morphology and photoluminescent property of globular Zn/ZnO core/shell nanorod heterojunction array architectures10.1080/17458080.2015.1072879 ↗
50. Understanding the dynamics of primary Zn-MnO2 alkaline battery gassing with operando visualization and pressure cells10.1149/2.0321811jes ↗
51. Insight into the corrosion behaviour and degradation mechanism of pure zinc in simulated body fluid10.1016/j.corsci.2020.109071 ↗
52. Grain-boundary character and grain growth in bulk tin and bulk lead-free solder alloys10.1007/s11664-004-0081-2 ↗
53. Suppressing dendritic growth during alkaline zinc electrodeposition using polyethylenimine additive10.1016/j.electacta.2014.12.100 ↗
54. A rotating disc electrode study of zinc electro-deposition from alkaline zincate solutions10.1080/00202967.1995.11871069 ↗
55. Detrimental effects of surface imperfections and unpolished edges on the cycling stability of a zinc foil anode10.1021/acsenergylett.1c00638 ↗
56. Redistributing Zn-ion flux by interlayer ion channels in Mg-Al layered double hydroxide-based artificial solid electrolyte interface for ultra-stable and dendrite-free Zn metal anodes10.1016/j.ensm.2021.06.002 ↗
57. Chemically resistant Cu–Zn/Zn composite anode for long cycling aqueous batteries10.1016/j.ensm.2020.01.032 ↗
58. Dendrite-free zinc anode enabled by zinc-chelating chemistry10.1016/j.ensm.2021.06.026 ↗