Thermal Oxidation Kinetics of Silicon in Pyrogenic H 2 O and 5% HCl / H 2 O Mixtures
Source abstract
Abstract
The kinetics of the thermal oxidation of silicon in and in in using a pyrogenic system have been investigated over the temperature range 900°–1100°C. Oxide thickness‐oxidation time data, rate constants, and activation energies have been obtained for (111) and (100) oriented, , n‐type silicon. Results obtained for oxidation in are very similar to those reported previously for water bubbler systems. The addition of to does not increase the silicon oxidation rate as with dry , but the rate actually decreases apparently because of the reduced vapor pressure. The also appears to reduce impurity contributions from the oxidation system.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Energetic Materials and Combustion · Thermal and Kinetic Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Fairchild Camera and Instrument Corporation, Research and Development Laboratory, Palo Alto, California 94304
References
Reference metadata was not supplied for this record.