Microstructural instability of L-PBF Co-28Cr-6Mo alloy at elevated temperatures
Source abstract
Abstract
Abstract In relation to the production of complex aircraft components, the additive manufacturing (AM) of Co-28Cr-6Mo alloy is highly discussed as it could bring many benefits regarding new designs, components lightening and shortening the design-to-product period. However, such components must undergo strict requirements for mechanical properties and material stability, even at elevated temperatures which might occur during part operation. So far, little is known about the thermal stability of Co-28Cr-6Mo alloy when produced by laser powder bed fusion ( L -PBF), one of the mostly used AM technologies. In the present study, we reveal the instability of this material already at temperatures above 673 K. Material hardening accompanied with a significant loss of plasticity is caused by the breakdown of fine cellular microstructure with intercellular Mo segregation, precipitation of σ-phase and phase transformation of the matrix. Detail characterization by transmission electron microscopy was carried out for the maximum hardness state obtained after annealing the alloy at 1173 K for 5 h. The important findings of this study, representing an operational risk for L -PBF Co-28Cr-6Mo alloy, call for subsequent research into suitable heat treatment that would induce the stability of the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Laser-induced spectroscopy and plasma
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Microstructures and mechanical properties of Co–29Cr–6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗
2. Perspective of additive manufacturing selective laser melting in Co-Cr-Mo alloy in the consolidation of dental prosthesis
3. Microstructural features of biomedical cobalt–chromium–molybdenum (CoCrMo) alloy from powder bed fusion to aging heat treatment10.1016/j.jmst.2019.11.031 ↗
4. Design and characterisation of an additive manufacturing benchmarking artefact following a design-for-metrology approach
5. Structural characterization of biomedical Co–Cr–Mo components produced by direct metal laser sintering10.1016/j.msec.2014.12.009 ↗
6. Fabrication of Co–Cr–Mo endoprosthetic ankle devices by means of Selective Laser Melting (SLM)10.1016/j.matdes.2016.05.083 ↗
7. NIMONIC® alloy 90, data sheet, Special Metals, 2004.
8. The production and properties of large NIMONIC* alloy 901 discs for land-based gas turbines
9. Microstructure and yield strength of SLM-fabricated CM247LC Ni-superalloy10.1016/j.actamat.2017.02.007 ↗
10. L.N. Carter, Selective laser melting of nickel superalloys for high temperature applications. PhD thesis, School of Metallurgy and Materials, University of Birmingham: Birmingham, UK, 2013.
11. The analysis of the mechanical properties of F75 Co–Cr alloy for use in selective laser melting (SLM) manufacturing of removable partial dentures (RPD)
12. Fatigue strength of Co–Cr–Mo alloy clasps prepared by selective laser melting10.1016/j.jmbbm.2016.02.032 ↗
13. Defects-tolerant Co-Cr-Mo dental alloys prepared by selective laser melting10.1016/j.dental.2015.09.003 ↗
14. CoCr alloy processed by Selective Laser Melting (SLM): effect of Laser Energy Density on microstructure, surface morphology, and hardness10.1016/j.jmapro.2020.01.052 ↗
15. Energy density analysis on single tracks formed by selective laser melting with CoCrMo powder material10.1007/s00170-013-4902-4 ↗
16. Beyond the orthogonal: on the influence of build orientation on fatigue crack growth in SLM Ti-6Al-4V10.1016/j.ijfatigue.2018.06.038 ↗
17. Formation of metastable cellular microstructures in selective laser melted alloys10.1016/j.jallcom.2016.12.209 ↗
18. Mechanical and phase transformation behaviour of biomedical Co-Cr-Mo alloy fabricated by direct metal laser sintering10.1016/j.msea.2017.12.087 ↗
19. Effect of phase transformation on ductility of additively manufactured Co–28Cr–6Mo alloy: an in situ synchrotron X-ray diffraction study during mechanical testing10.1016/j.msea.2019.138262 ↗
20. Effect of solution heat treatment on microstructure and mechanical properties of laser powder bed fusion produced cobalt-28chromium-6molybdenum10.1016/j.msea.2019.138511 ↗
21. Morphology and properties of CoCrMo parts fabricated by selective laser melting10.1016/j.msea.2017.12.035 ↗
22. An investigation into the aging behavior of CoCrMo alloys fabricated by selective laser melting10.1016/j.jallcom.2018.04.054 ↗
23. In vitro biocompatibility of CoCrMo dental alloys fabricated by selective laser melting10.1016/j.dental.2014.02.008 ↗
24. Effect of heat-treatment temperature on microstructures and mechanical properties of Co–Cr–Mo alloys fabricated by selective laser melting10.1016/j.msea.2018.04.048 ↗
25. Effect of heat treatment on the anisotropic microstructural and mechanical properties of Co–Cr–Mo alloys produced by selective laser melting10.1016/j.jmbbm.2019.103496 ↗
26. R. Chatterjee, Selective Laser Melting of Co-Cr-Mo Alloys, in: Indian Institute of Technology: Kharagpur, West Bengal, India, 2015.
27. Effect of heat treatment on the microstructure and fatigue strength of CoCrMo alloys fabricated by selective laser melting10.1016/j.matlet.2019.02.085 ↗
28. Additive manufacturing of cobalt-based dental alloys: analysis of microstructure and physicomechanical properties10.1155/2018/8213023 ↗
29. Nickel, cobalt and titanium-based alloys – from aircraft vehicles to medical applications – review10.30544/235 ↗
30. McCabe · 2008
31. Van Noort · 2013
32. Real-time monitoring of laser powder bed fusion process using high-speed X-ray imaging and diffraction10.1038/s41598-017-03761-2 ↗
33. Selective laser melting of Co-29Cr-6Mo alloy with laser power 180–360W: cellular growth, intercellular spacing and the related thermal condition10.1016/j.matchar.2017.11.042 ↗
34. Grain growth during selective laser melting of a Co–Cr–Mo alloy10.1007/s10853-017-0975-z ↗
35. Microstructure of As-cast Co-Cr-Mo Alloy prepared by investment casting10.3938/jkps.72.947 ↗
36. The use of selective laser melting to increase the performance of AlSi9Cu3Fe alloy10.3390/ma11101918 ↗
37. Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures10.1016/j.matchar.2018.01.028 ↗
38. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments10.1016/j.msea.2017.12.043 ↗
39. D. Benedikt, V. Nora, N. Steffen, G. Thomas, G. Mathias, Optimization of the heat treatment of additively manufactured Ni-base superalloy IN718, 27 (2020) 640–648.10.1007/s12613-020-1991-6 ↗
40. Hardened austenite steel with columnar sub-grain structure formed by laser melting10.1016/j.msea.2014.12.018 ↗
41. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
42. Microstructural evolution and mechanical properties of direct metal laser-sintered (DMLS) CoCrMo after heat treatment10.1007/s11661-018-4771-4 ↗
43. The effect of specific energy density on microstructure and corrosion resistance of CoCrMo alloy fabricated by laser metal deposition
44. Isothermal phase transformation in biomedical Co-29Cr-6Mo alloy without addition of carbon or nitrogen10.1007/s11661-010-0273-8 ↗
45. Cobalt-base alloys
46. Formation of hcp martensite during the isothermal aging of an fcc Co-27Cr-5Mo-0.05C orthopedic implant alloy10.1007/s11661-999-0267-6 ↗
47. Effect of solution treatments on the FCC/HCP isothermal martensitic transformation in Co-27Cr-5Mo-0.05C aged at 800 °C10.1016/S1359-6462(98)00489-8 ↗
48. Local strain evolution due to athermal γ→ε martensitic transformation in biomedical CoCrMo alloys10.1016/j.jmbbm.2013.12.019 ↗
49. Thermodynamics of stacking faults10.1007/BF03038365 ↗
50. A general mechanism of martensitic nucleation: part I. General concepts and the FCC → HCP transformation
51. Athermal ε-martensite in a Co–Cr–Mo alloy: grain size effects10.1016/S0167-577X(99)00022-1 ↗
52. Kinetics of the martensitic fcc→ hcp transformation in Co-Cr-Mo alloy powders10.1016/0001-6160(84)90077-4 ↗
53. Development and properties of ε-martensite in Co-Cr-Mo alloys for biomaterials applications
54. Accelerated γ-face-centered cubic to ε-hexagonal close packed massive transformation in a laser powder bed fusion additively manufactured Co-29Cr-5Mo alloy10.1016/j.scriptamat.2020.01.012 ↗