journal article·2023-01

A novel route for predicting the cracking of inoculant-added AA7075 processed via laser powder bed fusion

Jungho Choe, Kyung Tae Kim, Ji Hun Yu, Jeong Min Park, Dong Yeol Yang, Soo ho Jung, Seungki Jo, Hyomoon Joo, Mungu Kang, Soung Yeoul Ahn, Sang Guk Jeong, Eun Seong Kim, Haksung Lee, Hyoung Seop Kim

Publisher page

Abstract

Solidification cracks caused by columnar grains in precipitation-hardenable Al alloys such as Al–Zn–Cu–Mg limits the applicability of laser-based additive manufacturing. Recently, cracking has been effectively reduced by introducing equiaxed grains through inoculant addition to Al alloy powder. However, the mechanisms through which equiaxed grains can prevent cracking have not been explained from the viewpoint of both microstructure and process parameters. Thus, the control over the cracking behavior of Al alloys during the laser powder bed fusion (LPBF) process has remained limited because of a lack of theoretical understanding. In this study, a solidification cracking model was proposed using the parametric LPBF results of ZrH2 particle-added AA7075, where equiaxed grains were formed as a function of energy density. In the proposed model, the cracks in the previously formed layer were healed by liquid backfilling during remelting under appropriate solidification conditions. The synergistic effects of both repeatable melting (layer-by-layer) and equiaxed grain formation on the cracking behavior were revealed. Consequently, the proposed model opens a novel route to cracking prevention in laser-based metal additive manufacturing processes.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. S. Lathabai, Additive manufacturing of aluminium-based alloys and composites, in: R.N. Lumley (Ed.), Fundamentals of Aluminium Metallurgy, Woodhead Publishing, Sawston, 2018, pp. 47–92. https://doi.org/10.1016/B978–0-08–102063-0.00002–3.10.1016/B978-0-08-102063-0.00002-3 ↗
2. Yang · 2017
3. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
4. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
5. Alloys for aeronautic applications: state of the art and perspectives10.3390/met9060662 ↗
6. A comparative investigation on the microstructure and mechanical properties of additively manufactured aluminum alloys10.1016/j.ijfatigue.2021.106165 ↗
7. Fabrication and mechanical properties of Al–Si-based alloys by selective laser melting process10.1080/00325899.2021.1899470 ↗
8. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
9. Role of grain refining in hot cracking and macrosegregation in direct chill cast AA 7075 billets10.1179/174328407X236580 ↗
10. Weldability of 7000 series aluminium alloy materials10.1080/09507116.2011.590665 ↗
11. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
12. Grain refinement mechanisms in additively manufactured nano-functionalized aluminum10.1016/j.actamat.2020.09.043 ↗
13. Influence of the Zr content on the processability of a high strength Al-Zn-Mg-Cu-Zr alloy by laser powder bed fusion10.1016/j.matchar.2021.111650 ↗
14. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
15. Effect of zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
16. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
17. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
18. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
19. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by laser-based powder bed fusion10.1007/s11661-020-06073-9 ↗
20. Selective laser melting of micron-sized niobium functionalized Al7075 alloy: element evaporation and grain refinement10.1016/j.msea.2022.142595 ↗
21. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior10.1016/j.jmst.2020.08.003 ↗
22. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
23. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
24. Laser metal deposition for additive manufacturing of AA5024 and nanoparticulate TiC modified AA5024 alloy composites prepared with balling milling process10.1016/j.optlastec.2020.106438 ↗
25. Demonstrating the roles of solute and nucleant in grain refinement of additively manufactured aluminium alloys
26. Numerical and experimental study on melt treatment for large-volume 7075 alloy by a modified annular electromagnetic stirring10.3390/ma12050820 ↗
27. Trainable Weka segmentation: a machine learning tool for microscopy pixel classification10.1093/bioinformatics/btx180 ↗
28. Formation of fully equiaxed grain microstructure in additively manufactured AlCoCrFeNiTi0.5 high entropy alloy10.1016/j.matdes.2019.108202 ↗
29. Composites of aluminum alloy and magnesium alloy with graphite showing low thermal expansion and high specific thermal conductivity10.1080/14686996.2017.1286222 ↗
30. Role of porosity defects in metal 3D printing: Formation mechanisms, impacts on properties and mitigation strategies10.1016/j.mattod.2022.08.014 ↗
31. Microstructural effects on the tensile and fracture behavior of selective laser melted H13 tool steel under varying conditions10.1016/j.matchar.2019.109817 ↗
32. Pore formation during solidification of aluminum: Reconciliation of experimental observations, modeling assumptions, and classical nucleation theory10.1007/s11661-017-4438-6 ↗
33. Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-Mg-Cu alloy manufactured by selective laser melting10.1016/j.jallcom.2021.163427 ↗
34. Influence of energy density on macro/micro structures and mechanical properties of as-deposited inconel 718 parts fabricated by laser engineered net shaping10.1016/j.jmapro.2019.04.020 ↗
35. Selective laser melting of 304L stainless steel: Role of volumetric energy density on the microstructure, texture and mechanical properties
36. U. Feurer, Influence of alloy composition and solidification conditions on dendrite arm spacing, feeding and hot tearing properties of aluminum alloys, in: H. Nieswaag, J.W. Schut (Eds.), Quality Control of Engineering Alloys and the Role of Metals Science, Proceedings of the International Symposium, Delft, 1977, pp. 131–145.
37. Understanding crack formation mechanisms of Ti–48Al–2Cr–2Nb single tracks during laser powder bed fusion10.1007/s12540-020-00770-1 ↗
38. Experimental evidence of liquid feeding during solidification of a steel10.1016/j.scriptamat.2017.11.003 ↗
39. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
40. J.-M. Drezet, M.S.F. Lima, J.-D. Wagniere, M. Rappaz, W. Kurz, Crack-free aluminium alloy welds using a twin laser process, in: P. Mayr, G. Posch, H. Cerjak (Eds.), Safety and Reliability of Welded Components in Energy and Processing Industry, Proceedings of the International Institute of Welding Conference, Graz, 2008, pp. 87–94.
41. Prediction of solidification cracking in pulsed laser welding of 2024 aluminum alloy10.1016/j.actamat.2014.09.002 ↗
42. A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting
43. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
44. Mechanisms for solidification crack initiation and growth in aluminum welding10.1007/s11661-009-9964-4 ↗
45. Cracking behaviour of high-strength AA2024 aluminium alloy produced by Laser Powder Bed Fusion
46. Microstructure and mechanical properties of Al-Mg-Mn-Er-Zr alloys fabricated by laser powder bed fusion10.1016/j.matdes.2022.111064 ↗
47. Cracking mechanism of Hastelloy X superalloy during directed energy deposition additive manufacturing
48. Laser powder bed fusion of AA7075 alloy: Influence of process parameters on porosity and hot cracking
49. Investigation into the effect of energy density on densification, surface roughness and loss of alloying elements of 7075 aluminium alloy processed by laser powder bed fusion10.1016/j.optlastec.2021.107621 ↗
50. Influence of process parameters on the quality of aluminium alloy EN AW 7075 using selective laser melting (SLM10.1016/j.phpro.2016.08.096 ↗
51. Processing window for laser metal deposition of Al 7075 powder with minimized defects10.1016/j.jmapro.2021.02.031 ↗
52. Effect of process parameters and grain refinement on hot tearing susceptibility of high strength aluminum alloy 2139 in laser powder bed fusion10.1007/s40964-021-00259-2 ↗
53. An analytical model for intergranular liquid feeding and its effect on solidification cracking10.1080/13621718.2022.2051409 ↗
54. Nanoparticles enabled mechanism for hot cracking elimination in aluminum alloys10.1007/s11661-021-06302-9 ↗
55. Heat and fluid flow in additive manufacturing – Part II: Powder bed fusion of stainless steel, and titanium, nickel and aluminum base alloys10.1016/j.commatsci.2018.04.027 ↗
56. Revisiting fundamental welding concepts to improve additive manufacturing: From theory to practice10.1016/j.pmatsci.2019.100590 ↗
57. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
58. Laser powder bed fusion of Zr-modified Al-Cu-Mg alloy: crack-inhibiting, grain refinement, and mechanical properties10.1016/j.msea.2022.142618 ↗
59. An understanding of duplex microstructures encountered during high strength aluminium alloy laser beam melting processing10.1016/j.actamat.2021.117024 ↗
60. Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing
61. Heterogeneous aspects of additive manufactured metallic parts: a review10.1007/s12540-020-00931-2 ↗
62. Phase transition and heterogeneous strengthening mechanism in CoCrFeNiMn high-entropy alloy fabricated by laser-engineered net shaping via annealing at intermediate-temperature10.1016/j.jmst.2021.03.028 ↗