The Effect of Electrolyte Properties on the Mechanism of Crevice Corrosion in Pure Iron
Source abstract
Abstract
The roles of applied potential, solution resistance, pH, and temperature on passive and active metal dissolution and hydrogen evolution inside crevices were evaluated using in situ measurements of potential distribution, pH, and other data, for systems with active/passive transitions in their polarization curves. Their roles can be explained in terms of a requisite IR voltage drop, Δϕ*, for active metal dissolution to occur inside the crevice: IR > Δϕ*. Accordingly, crevice corrosion was suppressed in the systems studied by: ( i ) increased pH (or deacidification) of the crevice solution (the increased Δϕ* and decreased I dominated over the increased R ), ( ii ) increased solution conductivity (decreased R ), ( iii ) decreased solution temperature (the increased Δϕ* and decreased I dominated over the increased R ), and ( iv ) a more noble applied or corrosion potential in the passive region (increased Δϕ*). A decrease in oxidant availability during open‐circuit corrosion reduces the susceptibility by decreasing I .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, The Pennsylvania State University, University Park, Pennsylvania 16802
References
Reference metadata was not supplied for this record.