journal article·2021-11

Heat treatment of laser powder-bed-fused Co–28Cr–6Mo alloy to remove its microstructural instability by massive FCC→HCP transformation

Michaela Roudnická, Jiří Kubásek, Libor Pantělejev, Orsolya Molnárová, Jiří Bigas, Jan Drahokoupil, David Paloušek, Dalibor Vojtěch

Publisher page

Abstract

Abstract Laser powder bed fusion ( L -PBF) of Co–28Cr–6Mo alloy is a powerful tool for many engineering applications but one has to be familiar with its microstructural instability in the as-produced state. In our previous study [Roudnicka et al., Additive Manuf. 44 (2021) 102025], we depicted the phenomenon of this instability when exposing the material to temperatures above 673 K. Microstructural changes bringing about hardening of the material were studied thoroughly. In the present study, we follow up by revealing the effect of this hardening on mechanical properties in tension and show the beneficial effect of heat treatment on removing the observed instability. Hardening associated with increasing the proportion of HCP e-phase and with the precipitation of σ-phase has a detrimental effect on material plasticity and can be negatively affect the fatigue too. We thus applied a two-stage heat treatment comprising solution annealing at 1473 K/2 h and aging at 1173 K/5 h. Not only it induced material stability but also increased the material strength with not such a detrimental decrease in material plasticity as was brought by direct aging at 1173 K/5 h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. The research status and development trend of additive manufacturing technology10.1007/s00170-016-9335-4 ↗
2. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti–6Al–4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
3. Formation of metastable cellular microstructures in selective laser melted alloys10.1016/j.jallcom.2016.12.209 ↗
4. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
5. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
6. Specific response of additively manufactured AlSi9Cu3Fe alloy to precipitation strengthening10.1007/s12540-019-00504-y ↗
7. Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures10.1016/j.matchar.2018.01.028 ↗
8. Differences in the response of additively manufactured titanium alloy to heat treatment-Comparison between SLM and EBM
9. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
10. Elevated temperature microstructure stability of SLM 304 L stainless steel
11. Microstructural instability of L-PBF Co28Cr6Mo alloy at elevated temperatures
12. Nickel, cobalt and titanium-based alloys – from aircraft vehicles to medical applications - REVIEW10.30544/235 ↗
13. Effect of heat-treatment temperature on microstructures and mechanical properties of Co–Cr–Mo alloys fabricated by selective laser melting10.1016/j.msea.2018.04.048 ↗
14. Effect of heat treatment on the anisotropic microstructural and mechanical properties of Co–Cr–Mo alloys produced by selective laser melting10.1016/j.jmbbm.2019.103496 ↗
15. Effect of heat treatment on the microstructure and fatigue strength of CoCrMo alloys fabricated by selective laser melting10.1016/j.matlet.2019.02.085 ↗
16. Microstructural features of biomedical cobalt–chromium–molybdenum (CoCrMo) alloy from powder bed fusion to aging heat treatment10.1016/j.jmst.2019.11.031 ↗
17. An investigation into the aging behavior of CoCrMo alloys fabricated by selective laser melting10.1016/j.jallcom.2018.04.054 ↗
18. Additive manufacturing of cobalt-based dental alloys: analysis of microstructure and physicomechanical properties10.1155/2018/8213023 ↗
19. Mechanical and phase transformation behaviour of biomedical Co–Cr–Mo alloy fabricated by direct metal laser sintering10.1016/j.msea.2017.12.087 ↗
20. Fundamental parameters line profile fitting in laboratory diffractometers10.6028/jres.109.002 ↗
21. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
22. Microstructure of As-cast Co–Cr–Mo alloy prepared by investment casting10.3938/jkps.72.947 ↗
23. M. Klinger, CrysTBox - Crystallographic Toolbox, 2015.
24. Martensitic transformation in a cast Co–Cr–Mo–C alloy10.1007/s11661-007-9370-8 ↗
25. Deformation-induced martensitic transformation in Co–28Cr–6Mo alloy produced by laser powder bed fusion: comparison surface vs. bulk
26. Precipitation during γ-ε phase transformation in biomedical Co–Cr–Mo alloys fabricated by electron beam melting10.3390/met10010071 ↗
27. Isothermal phase transformation in biomedical Co–29Cr–6Mo alloy without addition of carbon or nitrogen10.1007/s11661-010-0273-8 ↗
28. Nucleation kinetics of the α→γM massive transformation in a Ti-47.5 at% Al alloy10.1016/S1359-6454(02)00572-4 ↗
29. Accelerated γ-face-centered cubic to ε-hexagonal close packed massive transformation in a laser powder bed fusion additively manufactured Co–29Cr–5Mo alloy10.1016/j.scriptamat.2020.01.012 ↗
30. Microstructures and mechanical properties of Co–29Cr–6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗
31. An assessment of biomedical CoCrMo alloy fabricated by direct metal laser sintering technique for implant applications10.1016/j.msec.2019.110305 ↗
32. Effect of phase transformation on ductility of additively manufactured Co–28Cr–6Mo alloy: an in situ synchrotron X-ray diffraction study during mechanical testing10.1016/j.msea.2019.138262 ↗
33. Effect of solution treatments on the FCC/HCP isothermal martensitic transformation in Co–27Cr–5Mo–0.05C aged at 800 °C10.1016/S1359-6462(98)00489-8 ↗
34. Deformation mode in biomedical Co–27% Cr–5% Mo alloy consisting of a single hexagonal close-packed structure10.1016/j.scriptamat.2010.08.006 ↗
35. Deformation induced FCC to HCP transformation in a Co–27Cr–5Mo–0.05C alloy10.1016/j.msea.2010.12.024 ↗
36. A model for the microstructure behaviour and strength evolution in lath martensite10.1016/j.actamat.2015.07.018 ↗
37. Additive manufacturing of a martensitic Co–Cr–Mo alloy: towards circumventing the strength–ductility trade-off
38. Microscopic mechanism of plastic deformation in a polycrystalline Co–Cr–Mo alloy with a single hcp phase10.1016/j.actamat.2013.11.005 ↗
39. Microstructure and flow stress of polycrystals and single crystals10.1016/S1359-6454(97)00365-0 ↗
40. C. Moussa, M. Bernacki, R. Besnard, N. Bozzolo, About quantitative EBSD analysis of deformation and recovery substructures in pure Tantalum, IOP Conference Series: Materials Science and Engineering 89 (2015) 012038. 10.1088/1757–899x/89/1/012038.10.1088/1757-899X/89/1/012038 ↗
41. Precipitation hardening in metals10.1179/026708399773002782 ↗
42. Enhanced mechanical properties of As-forged Co–Cr–Mo–N alloys with ultrafine-grained structures10.1007/s11661-012-1288-0 ↗
43. Size effects and Hall–Petch relation in polycrystalline cobalt10.1080/09500839.2015.1020351 ↗
44. Effect of building direction on the mechanical anisotropy of biocompatible Co–Cr–Mo alloy manufactured by selective laser melting process10.1016/j.jallcom.2020.155055 ↗
45. Microstructures and mechanical properties of biomedical Co–29Cr–6Mo–0.14N alloys processed by hot rolling10.1007/s11661-012-1156-y ↗
46. A deformation map for cobalt10.1016/0036-9748(83)90390-3 ↗
47. Anomalous strengthening behavior of Co–Cr–Mo alloy single crystals for biomedical applications10.1016/j.scriptamat.2016.06.016 ↗
48. Formation of hcp martensite during the isothermal aging of an fcc Co–27Cr–5Mo–0.05C orthopedic implant alloy10.1007/s11661-999-0267-6 ↗