Electrical Breakdown: II . During the Anodic Growth of Aluminum Oxide
Source abstract
Abstract
Breakdown characteristics found during the anodic growth of aluminum oxide start with a range of rapid increase in the rate of breakdown . This is followed by a range of saturation, when observations are not disturbed by propagating breakdowns. The mean value of can be subject to some variations in the saturation range. The breakdown characteristics shift to lower voltages with increasing field of anodization. The observations agree with predictions of the succession of avalanche breakdown theory. The reason for variations of in the saturation range is not clear. The coefficient of impact ionization at a field of 8.7 MV/cm was found to be roughly . Compared with tantalum pentoxide the breakdown characteristics of aluminum oxide show a relatively poor reproducibility.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Integrated Circuits and Semiconductor Failure Analysis · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Electrical Engineering, Technion‐Israel Institute of Technology, Haifa, Israel
References
Reference metadata was not supplied for this record.