Effect of annealing and carbon nanotube infill on the mechanical and electrical properties of additively manufactured polyether-ether-ketone nanocomposites via fused filament fabrication
Source abstract
Abstract
The light-weight, high-strength poly-ether-ether-ketone (PEEK) and its composite materials are the ideal candidate for a plethora of engineering applications. However, the inherent high viscosity and melting temperature of PEEK pose great challenges for the extrusion-based 3D printing process, leaving a wide knowledge gap on the properties and functionalities of novel PEEK-based composites. In this work, the PEEK/CNT composite filaments with different CNT content ranging from 1 to 7 wt% are prepared by single-screw extruder and subsequently printed with a custom-made high temperature 3D printer. The effects of CNT content and annealing on the mechanical strength and electrical conductivity of the 3D printed parts are investigated in detail. The tensile test result shows that the presence of CNT significantly enhances the mechanical strength of the composite. With 7 wt% CNT content, the maximum tensile strength and elastic modulus reaches 107.7 MPa and 1908.0 MPa, respectively, which amounts to a rise of 27.4% and 17.0% compared with the neat PEEK sample. The annealing treatment is similarly effective in strengthening the printed composites. The addition of CNT is also found to greatly improve the electrical conductivity to the PEEK, reaching 101 S/m for 7 wt% CNT. With such superior electrical conductivity, the printed PEEK/CNT composite sample exhibits outstanding electromagnetic interference (EMI) shielding performance, reaching 32.4 dB. However, additional annealing treatment decreases the electrical conductivity as wells as EMI shielding performance. Such decrease is mainly attributed to the growth of the crystals during annealing, which expels the CNTs to the grain boundaries and leads to remarkable agglomeration, which disconnects the pervasive conductive networks. The finding in this work can provide insights on the new designs of PEEK composite feedstock materials and cultivate new 3D printing strategies targeted specifically for highly-functional, high-strength novel composites.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Natural Fiber Reinforced Composites · Advanced Sensor and Energy Harvesting Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. A comparison of rapid prototyping technologies10.1016/S0890-6955(97)00137-5 ↗
2. A review on additive manufacturing of polymer-fiber composites10.1016/j.compstruct.2017.08.088 ↗
3. Study on microstructure, mechanical properties and machinability of efficiently additive manufactured AISI 316L stainless steel by high-power direct laser deposition10.1016/j.jmatprotec.2016.09.005 ↗
4. Mechanical impact behavior of polyether–ether–ketone (PEEK10.1016/j.compstruct.2014.12.061 ↗
5. Influence of layer thickness and raster angle on the mechanical properties of 3D-printed PEEK and a comparative mechanical study between PEEK and ABS10.3390/ma8095271 ↗
6. Interfacial bonding strength of short carbon fiber/acrylonitrile-butadiene-styrene composites fabricated by fused deposition modeling10.1016/j.compositesb.2017.11.018 ↗
7. Fatigue performance of fused filament fabrication PLA specimens10.1016/j.matdes.2017.11.072 ↗
8. 3D bioprinting scaffold using alginate/polyvinyl alcohol bioinks10.1016/j.matlet.2016.12.009 ↗
9. Preparation of a new filament based on polyamide-6 for three-dimensional printing10.1002/pen.24515 ↗
10. Thermal and mechanical properties of polyamide 12/graphene nanoplatelets nanocomposites and parts fabricated by fused deposition modeling10.1002/app.45332 ↗
11. Processing poly(ether etherketone) on a 3d printer for thermoplastic modelling
12. Extrusion-based additive manufacturing of PEEK for biomedical applications10.1080/17452759.2015.1097053 ↗
13. Effects of printing parameters of fused deposition modeling on mechanical properties, surface quality, and microstructure of PEEK10.1016/j.jmatprotec.2019.03.016 ↗
14. Effects of nozzle temperature and building orientation on mechanical properties and microstructure of PEEK and PEI printed by 3D-FDM10.1016/j.polymertesting.2019.105948 ↗
15. Influence of thermal processing conditions in 3D printing on the crystallinity and mechanical properties of PEEK material10.1016/j.jmatprotec.2017.04.027 ↗
16. Influence of thermal processing conditions in 3D printing on the crystallinity and mechanical properties of PEEK material10.1016/j.jmatprotec.2017.04.027 ↗
17. Additive manufacturing of continuous fibre reinforced thermoplastic composites using fused deposition modelling: Effect of process parameters on mechanical properties
18. Interlaminar bonding performance of 3D printed continuous fibre reinforced thermoplastic composites using fused deposition modelling10.1016/j.polymertesting.2018.04.038 ↗
19. Mechanical characterization of FDM 3D printing of continuous carbon fiber reinforced PLA composites10.1016/j.compositesb.2019.107147 ↗
20. Effects of carbon nanotube on the thermal, mechanical, and electrical properties of PLA/CNT printed parts in the FDM process10.1016/j.synthmet.2019.05.008 ↗
21. Enhancing the mechanical strength of Multi Jet Fusion–printed polyamide 12 and its glass fiber-reinforced composite via high-temperature annealing
22. Fracture toughness of additively manufactured carbon fiber reinforced composites
23. Thermomechanical characterization of short carbon fiber and short glass fiber-reinforced ABS used in large format additive manufacturing
24. Preparation of short CF/GF reinforced PEEK composite filaments and their comprehensive properties evaluation for FDM-3D printing10.1016/j.compositesb.2020.108175 ↗
25. Flexural properties and fracture behavior of CF/PEEK in orthogonal building orientation by FDM: microstructure and mechanism10.3390/polym11040656 ↗
26. Polymer composites for temperature and current sensors10.1063/1.363682 ↗
27. Advances in the science and technology of carbon nanotubes and their composites: a review10.1016/S0266-3538(01)00094-X ↗
28. Temperature dependent electrical conductivity of CNT–PEEK composites10.1016/j.compscitech.2011.08.018 ↗
29. The influence of a compatibilizer on the thermal and dynamic mechanical properties of PEEK/carbon nanotube composites10.1088/0957-4484/20/31/315707 ↗
30. Enhancement of carbon nanotube particle distribution in PPS/PEEK/carbon nanotube ternary composites with sausage-like structure10.3390/polym8020050 ↗
31. Fused Deposition Modelling of high temperature polymers: Exploring CNT PEEK composites10.1016/j.polymertesting.2017.08.024 ↗
32. Multifunctional performance of carbon nanotubes and graphene nanoplatelets reinforced PEEK composites enabled via FFF additive manufacturing
33. 3D-printed PEEK-Carbon Fiber (CF) composites: Structure and thermal properties10.1016/j.compscitech.2018.05.032 ↗
34. The influence of matrix viscosity on MWCNT dispersion and electrical properties in different thermoplastic nanocomposites10.1016/j.polymer.2011.12.019 ↗
35. Super tough graphene oxide reinforced polyetheretherketone for potential hard tissue repair applications10.1016/j.compscitech.2019.02.028 ↗
36. Dynamic imine chemistry assisted reaction induced hetero-epitaxial crystallization: Novel approach towards aromatic polymer/CNT nanohybrid shish-kebabs and related hybrid crystalline structures10.1016/j.polymer.2013.01.046 ↗
37. Nonisothermal crystallization behavior and mechanical properties of PEEK/SCF/nano-SiO2 composites10.1016/j.matchemphys.2014.06.041 ↗
38. Characterization of thermally annealed PEEK and CFR-PEEK composites: Structure-properties relationships10.1016/j.polymdegradstab.2016.12.005 ↗
39. Improving thermal durability and mechanical properties of poly(ether ether ketone) with single-walled carbon nanotubes10.1016/j.polymer.2019.05.028 ↗
40. Crystal nucleation in poly(ether ether ketone)/carbon nanotube nanocomposites at high and low supercooling of the melt10.1016/j.polymer.2020.122548 ↗
41. Effect of basalt fiber on tribological and mechanical properties of polyether-ether-ketone (PEEK) composites10.1016/j.compstruct.2021.113847 ↗
42. Effect of annealing on the fracture toughness of poly(lactic acid10.1023/B:JMSC.0000012957.02434.1e ↗
43. An experimental study of nozzle temperature and heat treatment (Annealing) effects on mechanical properties of high‐temperature polylactic acid in fused deposition modeling10.1002/pen.25353 ↗
44. Enhancing the interlayer tensile strength of 3D printed short carbon fiber reinforced PETG and PLA composites via annealing
45. Annealing induced electrical conductivity jump of multi-walled carbon nanotube/polypropylene composites and influence of molecular weight of polypropylene10.1002/polb.22106 ↗
46. Thermal annealing induced enhancements of electrical conductivities and mechanism for multiwalled carbon nanotubes filled poly(Ethylene-co-Hexene) composites10.1021/am302597f ↗
47. Enhancing the electrical conductivity of PP/CNT nanocomposites through crystal-induced volume exclusion effect with a slow cooling rate10.1016/j.compositesb.2019.107663 ↗
48. Quick heat dissipation in absorption-dominated microwave shielding properties of flexible PVDF/CNT/Co composite films with anisotropy-shaped Co (Flowers or Chains)10.1021/acsami.8b14733 ↗
49. Synergistic effect of graphene nanoplate and carbonized loofah fiber on the electromagnetic shielding effectiveness of PEEK-based composites10.1016/j.carbon.2018.11.015 ↗
50. Super-compression-resistant multiwalled carbon nanotube/nickel-coated carbonized loofah fiber/polyether ether ketone composite with excellent electromagnetic shielding performance10.1021/acssuschemeng.9b02447 ↗