Glancing angle X‐ray diffraction and Auger electron spectroscopy have been used to investigate interfacial reactions between the Ni(20 nm)/Pt(30 nm)/Au(80 nm) contacts and p‐GaN . The metallization schemes were annealed at temperatures ranging from 500 to 700°C for 30 s in a flowing Ar atmosphere. The anneal of the sample at 500°C resulted in ohmic behavior with a specific contact resistance of . However, the anneal at temperatures ≥600°C led to the degradation of the ohmic property. It is shown that Ga‐(Pt,Ni) phases such as and , and a Pt‐Ni solid solution are formed upon annealing at 500°C, while in addition to the , new phases of and GaAu are formed upon annealing at temperatures 600°C. As for the Pt‐Ni solid solution, the lattice parameter decreases significantly with increasing annealing temperatures. A qualitative explanation is given to describe why the characteristic of the contacts changed from ohmic to rectifying behavior with increasing temperature. © 1999 The Electrochemical Society. All rights reserved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Semiconductor materials and devices · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, Kwangju Institute of Science and Technology, Kwangfu 500-712, Korea
References
Reference metadata was not supplied for this record.