Source abstract
Abstract
Present day high‐purity Czochralski(CZ)‐grown Si crystals are characterized by the bulk carrier recombination life‐time measurements. The bulk lifetime of the p‐type as‐grown Si with resistivity ∼10 Ω‐cm is found to be as high as 500 μs for a CZ‐Si crystal with and as high as ∼1 ms or even higher for a low‐oxygen CZ‐Si crystal with . The as‐grown bulk lifetime is revealed to depend not only on resistivity under the framework of the Shockley‐Read‐Hall (SRH) relation, but also on the oxygen concentration. The dominant recombination center of the as‐grown crystal is found to be an SRH‐type deep‐level center which is considered to be an oxygen‐related defect complex. The complex is quenched easily by a heat‐treatment at a temperature as low as 650°C. Effective density of a recombination center, existing after the 650°C heat‐treatment in the p‐type crystal, correlates well with the amount of oxygen precipitation generated by a subsequent two‐step heat process . Thus the dominant recombination center after the 650°C heat‐treatment is considered to be closely related to the oxygen precipitation nuclei toward the subsequent precipitation formation heat process.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Silicon Nanostructures and Photoluminescence
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
SEH Research and Development Center, Shin‐Etsu Handotai Company, Limited, 2‐13‐1 Isobe, Annaka‐shi, Gunma‐ken 379‐01, Japan
References
Reference metadata was not supplied for this record.