journal article·2024-01Open access

On the size-dependent fatigue behaviour of laser powder bed fusion Ti-6Al-4V

Jieming S. Zhang, Yuanbo T. Tang, Ruining Jin, Andrew Lui, Patrick S. Grant, Enrique Alabort, Alan C.F. Cocks, Roger C. Reed

Abstract

A sample size effect which influences the fatigue behaviour of laser powder bed fusion Ti-6Al-4V is identified and quantified. Two cylindrical samples are considered: ∅ 1.3 mm and ∅ 2.0 mm. The larger specimen demonstrates better fatigue resistance particularly in the high-cycle regime, with the differing surface roughness contributing to this effect. It is also confirmed that processing-induced porosity can compromise the fatigue performance even when the initiation sites are surface defects. The larger contribution of porosity to the fatigue fracture process of the larger specimen results in a higher scatter in the fatigue life. Differences in microstructure do not seem to contribute strongly to the variation in fatigue properties of the two specimens, but we present some evidence that the coarser microstructure of the larger specimen promotes a stronger tolerance to defects and induces more tortuous crack paths which hinders fatigue crack growth.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. Synthetic bone: Design by additive manufacturing10.1016/j.actbio.2019.07.049 ↗
4. Ultralight, ultrastiff mechanical metamaterials10.1126/science.1252291 ↗
5. Damage-tolerant architected materials inspired by crystal microstructure10.1038/s41586-018-0850-3 ↗
6. Fatigue behavior of as-built selective laser melted titanium scaffolds with sheet-based gyroid microarchitecture for bone tissue engineering10.1016/j.actbio.2019.05.046 ↗
7. On the size and orientation effect in additive manufactured Ti-6Al-4V10.1016/j.matdes.2019.108235 ↗
8. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
9. Metallurgical failure analysis of various implant materials used in orthopedic applications10.1007/s11668-996-0007-9 ↗
10. Fatigue properties of AlSi10Mg obtained by additive manufacturing: Defect-based modelling and prediction of fatigue strength10.1016/j.engfracmech.2017.11.002 ↗
11. Additive manufacturing of fatigue resistant materials: Challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
12. A review on additive manufacturing of titanium alloys for aerospace applications: Directed energy deposition and beyond Ti-6Al-4V10.1007/s11837-021-04670-6 ↗
13. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
14. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
15. Architectural bone parameters and the relationship to titanium lattice design for powder bed fusion additive manufacturing
16. Advances in metal additive manufacturing: A review of common processes, industrial applications, and current challenges
17. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
18. Printability of alloys for additive manufacturing10.1038/srep19717 ↗
19. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
20. Size effect in S-N curves: A fractal approach to finite-life fatigue strength10.1016/j.ijfatigue.2008.10.001 ↗
21. Probabilistic modeling of the size effect and scatter in high cycle fatigue using a Monte-Carlo approach: Role of the defect population in cast aluminum alloys
22. Modelling of critical defect distributions for estimating the size effect of selective laser melted 316l stainless steel
23. Fracture and fatigue in additively manufactured metals10.1016/j.actamat.2021.117240 ↗
24. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
25. Effect of build thickness and geometry on quasi-static and fatigue behavior of Ti-6Al-4V produced by electron beam melting
26. Importance of build design parameters to the fatigue strength of Ti6Al4V in electron beam melting additive manufacturing10.3390/ma15165617 ↗
27. Study of size effect on microstructure and mechanical properties of AlSi10Mg samples made by selective laser melting10.3390/ma11122463 ↗
28. The effect of density and feature size on mechanical properties of isostructural metallic foams produced by additive manufacturing10.1016/j.actamat.2014.10.058 ↗
29. ASTM E8/E8M standard test methods for tension testing of metallic materials 1
30. Quantitative X-ray tomography10.1179/1743280413Y.0000000023 ↗
31. A threshold selection method from gray-level histograms10.1109/TSMC.1979.4310076 ↗
32. Experimental investigation of the size effect in high cycle fatigue: Role of the defect population in cast aluminium alloys
33. Fatigue of additive manufactured ti-6al-4v, part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects
34. An experimental and simulation study on build thickness dependent microstructure for electron beam melted Ti-6Al-4V10.1016/j.jallcom.2015.05.178 ↗
35. Reducing porosity in AlSi10Mg parts processed by selective laser melting
36. A novel pole figure inversion method: Specification of the mtex algorithm10.1107/S0021889808030112 ↗
37. Leyens · 2003
38. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing10.1016/j.actamat.2016.03.063 ↗
39. Grain structure and texture of the SLM single track
40. Variant selection and intervariant crystallographic planes distribution in martensite in a Ti-6Al-4V alloy10.1016/j.actamat.2014.06.064 ↗
41. Preparation of weak-textured commercially pure titanium by electron beam melting
42. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: A study from laser power perspective10.1016/j.matdes.2016.12.019 ↗
43. Developing a phenomenological equation to predict yield strength from composition and microstructure in β processed Ti-6Al-4V10.1016/j.msea.2016.02.052 ↗
44. Selective laser melting of crack-free high density M2 high speed steel parts by baseplate preheating10.1115/1.4028513 ↗
45. Critical assessment of the impact of process parameters on vertical roughness and hardness of thin walls of AlSi10Mg processed by laser powder bed fusion
46. Process dependent porosity and the in fl uence of shot peening on porosity morphology regarding selective laser melted AlSi10Mg parts
47. Standardized X-ray tomography testing of additively manufactured parts : A round robin test
48. Pore closure effect of laser shock peening of additively manufactured AlSi10Mg10.1089/3dp.2019.0064 ↗
49. Effects of defects, inclusions and inhomogeneities on fatigue strength10.1016/0142-1123(94)90001-9 ↗
50. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
51. Stress concentrations and microfracturing patterns in a brittle-elastic solid with interacting pores of diverse shapes10.1016/S0020-7683(96)00202-8 ↗
52. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
53. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
54. Additive manufacturing of metallic and polymeric load-bearing biomaterials using laser powder bed fusion: A review10.1016/j.jmst.2021.03.058 ↗
55. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: Processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
56. Numerical modelling of surface roughness effect on the fatigue behavior of Ti-6Al-4V obtained by additive manufacturing10.1016/j.ijfatigue.2019.02.014 ↗
57. Influence of processing on microstructure and mechanical properties of (α + β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
58. Torsional fatigue behavior of wrought and additive manufactured Ti-6Al-4V by powder bed fusion including surface finish effect10.1016/j.ijfatigue.2017.03.002 ↗
59. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti–6Al–4V alloy10.1016/j.actamat.2019.03.003 ↗
60. Critical assessment of the fatigue performance of additively manufactured Ti-6Al-4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
61. Towards predicting differences in fatigue performance of laser powder bed fused Ti-6Al-4V coupons from the same build10.1016/j.ijfatigue.2019.05.004 ↗
62. Inclusion initiated fracture under cyclic torsion very high cycle fatigue at different load ratios10.1016/j.ijfatigue.2019.01.015 ↗
63. The kitagawa-takahashi fatigue diagram to hybrid welded AA7050 joints via synchrotron X-ray tomography10.1016/j.ijfatigue.2019.04.002 ↗
64. Effects of pore position in depth on stress/strain concentration and fatigue crack initiation10.1007/s11661-011-0947-x ↗
65. Fatigue failure of a drive shaft10.1007/s11668-012-9551-7 ↗
66. Fatigue behavior and failure mechanisms of direct laser deposited Ti-6Al-4V10.1016/j.msea.2015.12.026 ↗
67. Interior initiation and early growth of very high cycle fatigue crack in an additively manufactured Ti-alloy
68. Fatigue damage process of additively manufactured 316 L steel using X-ray computed tomography imaging
69. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
70. Polasik · 2014
71. Tensile and fatigue crack growth behavior of commercially pure titanium produced by laser powder bed fusion additive manufacturing
72. Fatigue crack growth mechanisms at the microstructure scale in as-fabricated and heat treated Ti-6Al-4V ELI manufactured by electron beam melting (EBM)10.1016/j.engfracmech.2017.03.024 ↗