journal article·2021-06

Directed energy deposition of Ni-Al-Cr-C composites: Microstructural evolution during solidification and wear

M.S.K.K.Y. Nartu, T.B. Torgerson, S.A. Mantri, R. Banerjee, T.W. Scharf

Publisher page

Abstract

Abstract Laser engineered net shaping (LENS™) allows for the deposition of novel hybrid materials with microstructures composed of solid solution and precipitation strengthened metallic matrices, along with a distribution of reinforcing in situ formed hard ceramic and solid lubricant phases. In this study, four different composites in the Ni-Al-Cr-C system were fabricated via LENS™ as potential candidate materials for high temperature wear resistant components. Microstructural evolution during solidification and sliding wear were studied at room and elevated temperatures. Experimental and solution thermodynamic simulations were used to evaluate the evolution of various compositions of hard chromium carbides and solid lubricant graphite dispersed into a continuous γ/γ′ (L12) matrix. By tailoring the microstructures along the build direction, desired hardness and wear properties were achieved for the different Ni-Al-Cr-C composites. Specifically, compositional modification of chromium and carbon were determined to drastically affect the corresponding phase morphology and properties. The two lowest wear rates measured were for the Ni-14Al-9Cr-29 C (at%) composite at 500 °C and Ni-12Al-3Cr-45 C (at%) composite at room temperature. Mechanistic studies using surface and subsurface scanning and transmission electron microscopies in the wear surfaces revealed this was a result of a combination of increased hardness/load-bearing and formation of tribochemical protective oxide glaze layers.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
2. High temperature materials for aerospace applications: Ni-based superalloys and γ-TiAl alloys10.1016/j.crhy.2018.10.002 ↗
3. The effect of high temperature exposure on dendritic segregation in a conventionally cast Ni based superalloy10.1023/A:1012513615622 ↗
4. Additive manufacturing of nickel-based superalloy Inconel 718 by selective electron beam melting: processing window and microstructure10.1557/jmr.2014.192 ↗
5. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
6. Microstructural architecture, microstructures, and mechanical properties of a nickel-base superalloy fabricated by electron beam melting10.1007/s11661-011-0748-2 ↗
7. An algorithm for inverse modeling of layer-by-layer deposition processes10.1007/s11665-008-9268-7 ↗
8. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
9. Microstructure and micro-texture evolution of additively manufactured β-Ti alloys
10. Recent advances on high-entropy alloys for 3D printing10.1002/adma.201903855 ↗
11. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders
12. In situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
13. In-situ reactive processing of nickel aluminides by laser-engineered net shaping10.1007/s11661-003-0022-3 ↗
14. Intermetallic-matrix composites- a review10.1016/0966-9795(95)00037-2 ↗
15. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
16. Creep behaviour of a Ni-Ni3Al-Cr3C2 eutectic composite10.1016/0001-6160(77)90152-3 ↗
17. Designing a new family of high temperature wear resistant alloys based on Ni3Al IC: experimental results and thermodynamic modelling10.1016/j.intermet.2004.02.027 ↗
18. Characterization of NiCrAlC PTA coatings10.1590/S1516-14392012005000098 ↗
19. Microstructure of cast Ni-Cr-Al-C alloy10.1515/amm-2015-0022 ↗
20. Room temperature mechanical properties and tribology of NICRALC and stellite casting alloys10.1016/j.wear.2011.02.030 ↗
21. Microstructural evolution in laser deposited nickel–titanium–carbon in situ metal matrix composites10.1016/j.jallcom.2010.09.208 ↗
22. Laser deposited in-situ TiC reinforced nickel matrix composites: microstructure and tribological properties
23. Solid/self-lubrication mechanisms of an additively manufactured Ni–Ti–C metal matrix composite
24. Room and elevated temperature sliding wear behavior and mechanisms of additively manufactured novel precipitation strengthened metallic composites10.1016/j.wear.2018.12.046 ↗
25. Structure, nucleation, growth and morphology of secondary carbides in high chromium and Cr-Ni white cast irons10.1007/BF02403640 ↗
26. Microstructure and tribological properties of Cr3C2/Ni3Al composite materials prepared by hot isostatic pressing (HIP)10.1016/j.matdes.2016.11.060 ↗
27. Tribological properties of hard alloys based on chromium carbide10.1023/A:1025763427786 ↗
28. Microstructure and abrasive wear performance of chromium carbide reinforced Ni3Al matrix composite coating10.1016/j.surfcoat.2006.09.106 ↗
29. Microstructure and sliding wear performance of Cr7C3-(Ni,Cr)3(Al,Cr) coating deposited from Cr7C3 in situ formed atomized powder
30. Phase equilibria in the Cr-Ni-C system and their use for developing physicochemical principles for design of hard alloys based on chromium carbide10.1007/BF02676213 ↗
31. The metallurgical structure of as-solidified Ni-Cr-B-Si-C hardfacing alloys10.1007/BF00540502 ↗
32. Control of microstructure and orientation distribution in Ni–Al-based (β/γ′) two phase alloys by thermomechanical processing10.1016/S1359-6454(01)00310-X ↗
33. Kurdjumov · Z. Phys. · 1930 · 64 · 225
34. Enhanced tensile yield strength in laser additively manufactured Al0.3CoCrFeNi high entropy alloy10.1016/j.mtla.2019.100522 ↗
35. Influence of solidification cell structure on the martensitic transformation in additively manufactured steels
36. Characterization of the microstructure evolution in a nickel base superalloy during continuous cooling conditions10.1016/S1359-6454(01)00314-7 ↗
37. Formation of multimodal size distributions of γ′ in a nickel-base superalloy during interrupted continuous cooling10.1016/j.scriptamat.2007.06.014 ↗
38. Phase-field modeling of bimodal particle size distributions during continuous cooling10.1016/S1359-6454(02)00516-5 ↗
39. Influence of cooling rate on the development of multiple generations of γ′ precipitates in a commercial nickel base superalloy10.1016/j.matchar.2011.06.002 ↗
40. The hardness of additively manufactured alloys10.3390/ma11112070 ↗
41. Laser melted TiC reinforced nickel aluminide matrix in situ composites10.1016/j.jallcom.2004.08.066 ↗
42. Growth, structure, and tribological behavior of atomic layer-deposited tungsten disulphide solid lubricant coatings with applications to MEMS10.1016/j.actamat.2006.06.009 ↗
43. Friction and wear mechanisms in MoS2/Sb2O3/Au nanocomposite coatings10.1016/j.actamat.2010.03.040 ↗
44. Materials phenomena revealed by in situ tribometry10.1007/s11837-011-0229-5 ↗
45. Grain refinement: a mechanism for graphene nanoplatelets to reduce friction and wear of Ni3Al matrix self-lubricating composites10.1016/j.wear.2013.12.014 ↗
46. Some frictional features associated with the sliding wear of the nickel-base alloy N80A at temperatures to 250°C10.1016/0043-1648(94)90146-5 ↗
47. The structure and mechanism of formation of the ‘glaze’ oxide layers produced on nickel-based alloys10.1016/0010-938X(73)90030-9 ↗
48. The effect of temperature on gross slip fretting wear of cold-sprayed nickel coatings on Ti6Al4V interfaces10.1016/j.triboint.2008.08.009 ↗
49. Elevated temperature dry sliding wear behavior of nickel-based composite coating on austenitic stainless steel deposited by a novel hollow laser cladding10.1016/j.apsusc.2011.08.072 ↗