Laser directed energy deposition (LDED), based on the powder feeding technology, possesses the capability to fabricate complex structures within hollow structures. The arbitrary Lagrangian-Eulerian (ALE) method was innovatively applied to derive temporal interpolation functions for the free surface contour F (x, y, t) and the temperature distribution T (x, y, t) of the melt pool from a mesoscopic computational fluid dynamics (CFD) thermal model. These interpolation functions were not simply integrated but specifically designed to impart a quantified impetus for the growth of crystalline solidification within the microstructural phase field, effecting real-time adjustments to the computational domain of the phase field model. The multi-area, multi-layer and multi-scale phase field calculation (M3-PFC), which takes into account the bi-directional coupling of Marangoni flow and the phase field, was established to incorporate the transportation of elements within the multi-layer deposition and previously solidified material. Thermodynamics of multi-layer deposition was integrated into M3-PFC, enabling the prediction of multi-layer dendritic evolution using LDED process. Influence of Marangoni flow on microstructure evolution of multi-layer C276 deposited on 316 L-substrate utilizing M3-PFC was investigated during LDED process. It was observed that the nucleation of equiaxed and columnar crystals occurred at the top and bottom-middle of the melt pool. Both columnar and equiaxed crystals were preferentially produced along the opposite direction of Marangoni flow, impeding the apparent dendrite-growth in the counter direction. Partial remelting of the (N + 1)th layer was induced by the thermodynamics generated in the (N + 2)th deposition layer, promoting re-solidification of the liquid phase in the (N + 1)th layer. However, no liquid-solid transformation occurred in the Nth layer subjected to periodic heating. The partially remelted tissue in the (N + 1)th layer was shown in wider columnar crystals generated through the competitive growth, which were transformed into planar crystals and identified as the initial solidification conditions for the nucleation of the (N + 2)th layer. The columnar crystal growth, nucleated at the planar crystals of the (N + 1)th layer, was dominated in the (N + 2)th layer. Micropillar compression tests revealed that the columnar crystal had a compressive strength of 1102.78 MPa, while the equiaxed crystals displayed a higher compressive strength of 1464.34 MPa.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Solidification and crystal growth phenomena · nanoparticles nucleation surface interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. Laser additive manufacturing of bio-inspired metallic structures
3. Solidification microstructure simulation of Ti-6Al-4V in metal additive manufacturing: a review
4. Hybrid additive and subtractive machine tools - research and industrial developments10.1016/j.ijmachtools.2015.11.007 ↗
5. Revealing melt flow instabilities in laser powder bed fusion additive manufacturing of aluminum alloy via in-situ high-speed X-ray imaging10.1016/j.ijmachtools.2022.103861 ↗
6. Thermal behavior and fluid dynamics within molten pool during laser inside additive manufacturing of 316L stainless steel coating on inner surface of steel tube10.1016/j.optlastec.2021.106917 ↗
7. Influence of environmental constraints and carrier gas velocity on powder concentration and temperature distribution during laser inside additive manufacturing process10.1016/j.cirpj.2020.11.010 ↗
8. A discrete dendrite dynamics model for epitaxial columnar grain growth in metal additive manufacturing with application to inconel
9. Simulation of powder bed metal additive manufacturing microstructures with coupled finite difference-Monte Carlo method
10. Deterministic modeling of solidification microstructure formation in directed energy deposition fabricated Ti6Al4V
11. Unravelling heterogeneities in sub-grain cellular structure and micromechanical response of additive manufactured Ti-Nb alloys
12. High-performance integrated additive manufacturing with laser shock peening –induced microstructural evolution and improvement in mechanical properties of Ti6Al4V alloy components10.1016/j.ijmachtools.2019.103475 ↗
13. Characterizing the microstructural effect of build direction during solidification of laser-powder bed fusion of Al-Si alloys in the dilute limit: a phase-field study10.1016/j.actamat.2021.116983 ↗
14. The significance of spatial length scales and solute segregation in strengthening rapid solidification microstructures of 316L stainless steel10.1016/j.actamat.2019.10.044 ↗
15. Multi-scale simulation of grain/sub-grain structure evolution during solidification in laser welding of aluminum alloys10.1016/j.ijheatmasstransfer.2019.119252 ↗
16. Microstructural transition in monotectic alloys: a phase-field study10.1016/j.ijheatmasstransfer.2020.120096 ↗
17. Overgrowth behavior at converging grain boundaries during competitive grain growth: a two-dimensional phase-field study10.1016/j.ijheatmasstransfer.2020.120196 ↗
18. Effect of laser shock on lamellar eutectic growth: a phase-field study10.1016/j.ijheatmasstransfer.2021.122069 ↗
19. Microstructural pattern formation during far-from-equilibrium alloy solidification10.1103/PhysRevLett.130.026203 ↗
20. Modeling of microstructure evolution coupled with molten pool oscillation during electron beam welding of an Al-Cu alloy10.1016/j.ijheatmasstransfer.2022.122735 ↗
21. Electrically actuated shape recovery of NiTi components processed by laser powder bed fusion after regulating the dimensional accuracy and phase transformation behavior
22. Phase-field simulation of microstructure evolution of Ti-6Al-4V in electron beam additive manufacturing process
23. Ultrafine Fe-Fe2Ti eutectics by directed energy deposition: insights into microstructure formation based on experimental techniques and phase field modelling
24. Prediction of microstructure in laser powder bed fusion process10.1016/j.actamat.2016.11.018 ↗
25. Phase-field modeling of grain evolution in additive manufacturing with addition of reinforcing particles
26. Mesoscale multi-physics simulation of rapid solidification of Ti-6Al-4V alloy
27. Multi-physics multi-scale simulation of the solidification process in the molten pool during laser welding of aluminum alloys10.1016/j.ijheatmasstransfer.2020.120316 ↗
28. Impact of fluid flow on the dendrite growth and the formation of new grains in additive manufacturing
29. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
30. A method to manipulate non-steady-state columnar-to-equiaxed transition in powder bed fusion additive manufacturing using an electron beam10.1016/j.actamat.2022.117717 ↗
31. Denudation of metal powder layers in laser powder bed fusion processes10.1016/j.actamat.2016.05.017 ↗
32. Quantitative simulation of selective laser melting of metals enabled by new high-fidelity multiphase, multiphysics computational tool10.1016/j.cma.2022.115422 ↗
33. Controlling interdependent meso-nanosecond dynamics and defect generation in metal 3D printing10.1126/science.aay7830 ↗
34. Intermittent nucleation and periodic growth of grains under thermo-solutal convection during directional solidification of Al-Cu alloy10.1016/j.actamat.2021.116861 ↗
35. Modeling of the effect of powder parameters on laser cladding using coaxial nozzle10.1016/j.surfcoat.2018.12.002 ↗
36. Keyhole fluctuation and pore formation mechanisms during laser powder bed fusion additive manufacturing
37. Investigation of temperature distribution and solidification morphology in multilayered directed energy deposition of Al-0.5Sc-0.5Si alloy10.1016/j.ijheatmasstransfer.2021.122492 ↗
38. Experimental and modelling studies for solidification of undercooled Ni-Fe-Si alloys10.1098/rsta.2018.0208 ↗
39. Phase-field simulation of solidification microstructure in Ni and Cu–Ni alloy using the Wheeler, Boettinger and McFadden model coupled with the CALPHAD data
40. Construction of a pseudo-binary phase diagram for multi-component Ni-base superalloys
41. A phase-field model without artificial curvature effect for the crystal growth simulation10.1016/j.ijheatmasstransfer.2023.123847 ↗
42. Efficient phase field simulation of a binary dendritic growth in a forced flow10.1103/PhysRevE.69.031601 ↗
43. Phase-field formulation for quantitative modeling of alloy solidification10.1103/PhysRevLett.87.115701 ↗
44. Microstructure and properties of Ni-WC gradient composite coating prepared by laser cladding10.1016/j.ceramint.2021.11.338 ↗
45. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing, Science. 374
46. Simultaneously enhanced strength and ductility for 3D-printed stainless steel 316L by selective laser melting10.1038/s41427-018-0018-5 ↗
47. A micropillar compression investigation into the plastic flow properties of additively manufactured alloys10.1016/j.actamat.2022.118290 ↗
48. Microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy10.1016/j.matdes.2020.109007 ↗
49. Effects of post heat treatment on the microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy10.1016/j.matchar.2021.111158 ↗
50. Stabilised mechanical properties in Ni-based Hastelloy C276 alloy by additive manufacturing under different heat inputs incorporated with active interlayer temperature control10.1016/j.msea.2022.144434 ↗
51. Understanding the mechanism of columnar–to-equiaxed transition and grain refinement in additively manufactured steel during laser powder bed fusion
52. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗