journal article·2024-09

Additive manufacturing of a new titanium alloy with tunable microstructure and isotropic properties

Jiaqiang Chang, Yingjie Ma, Sensen Huang, Min Qi, Zirong Zhai, Yingna Wu, Rui Yang, Zhenbo Zhang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. R.R. Boyer, G. Welsch, E.W. Collings, Materials Properties Handbook: Titanium Alloys, ASM International, 1994. 〈https://api.semanticscholar.org/CorpusID:137221408〉.
3. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
4. Laser additive manufacturing of titanium alloys: process, materials and post-processing10.1007/s12598-024-02685-x ↗
5. Recent innovations in laser additive manufacturing of titanium alloys10.1088/2631-7990/ad2545 ↗
6. Functionally graded Ti6Al4V-Mo alloy manufactured with DED-CLAD® process
7. Control of residual oxygen of the process atmosphere during laser-powder bed fusion processing of Ti-6Al-4V
8. Additive manufacturing of the high-strength and low modulus biomedical Ti-10 Nb alloy under reactive atmosphere
9. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
10. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
11. Omega versus alpha precipitation mediated by process parameters in additively manufactured high strength Ti–1Al–8V–5Fe alloy and its impact on mechanical properties
12. Towards uniform and enhanced tensile ductility of additively manufactured Ti−5Al−5Mo−5V−3Cr alloy through designing gradient interlayer deposition time10.1016/j.scriptamat.2022.115066 ↗
13. Controlling the microstructure and properties of wire arc additive manufactured Ti–6Al–4V with trace boron additions10.1016/j.actamat.2015.03.035 ↗
14. Achieving grain refinement and ultrahigh yield strength in laser aided additive manufacturing of Ti−6Al−4V alloy by trace Ni addition10.1080/17452759.2021.1949091 ↗
15. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
16. Grain structure control during metal 3D printing by high-intensity ultrasound10.1038/s41467-019-13874-z ↗
17. Microstructure of interpass rolled wire + arc additive manufacturing Ti-6Al-4V components10.1007/s11661-015-3172-1 ↗
18. In-situ grain structure control in directed energy deposition of Ti6Al4V
19. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
20. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
21. Microstructure and room-temperature tensile property of Ti-5.7Al-4.0Sn-3.5Zr-0.4Mo-0.4Si-0.4Nb-1.0Ta-0.05C with near equiaxed β grain fabricated by laser directed energy deposition technique10.1016/j.jmst.2021.03.012 ↗
22. Underlying factors determining grain morphologies in high-strength titanium alloys processed by additive manufacturing10.1038/s41467-023-38885-9 ↗
23. Beryllium as a grain refiner in titanium alloys10.1016/j.jallcom.2009.03.016 ↗
24. Achieving fully-equiaxed fine β-grains in titanium alloy produced by additive manufacturing10.1080/21663831.2022.2115323 ↗
25. Additive manufacturing of titanium-base alloys with equiaxed microstructures using powder blends
26. Grain-refinement mechanisms in titanium alloys10.1557/JMR.2008.0002 ↗
27. Strong and ductile titanium–oxygen–iron alloys by additive manufacturing10.1038/s41586-023-05952-6 ↗
28. Fe element promotes the transformation from columnar to equiaxed grains and the formation of ultrafine microstructure of Ti-6Al-4V alloy by laser wire deposition
29. Practical considerations for manufacturing high-strength Ti-10V-2Fe-3A1 alloy forgings10.1007/BF03354533 ↗
30. Effects of Cr and Fe addition on microstructure and tensile properties of Ti–6Al–4V prepared by direct energy deposition10.1007/s12540-018-0148-x ↗
31. In-situ elimination of β-flecks in additively manufactured Ti-3.5 wt% Fe alloy10.1016/j.jmrt.2024.01.153 ↗
32. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
33. Eliminating segregation defects during additive manufacturing of high strength β-titanium alloys
34. Towards β-fleck defect free additively manufactured titanium alloys by promoting the columnar to equiaxed transition and grain refinement10.1016/j.actamat.2021.117511 ↗
35. Influencing mechanisms of melt behavior on metal vapor characteristic and columnar grain formation in wire-arc directed energy deposition of titanium alloy
36. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
37. Perspectives on titanium science and technology
38. Gialanella · 2020
39. Controlling reversible martensitic transformation in titanium alloys with high strength and low elastic modulus10.1016/j.scriptamat.2012.06.011 ↗
40. Hierarchical structure and deformation behavior of a novel multicomponent β titanium alloy with ultrahigh strength10.1016/j.jmst.2021.08.031 ↗
41. Microstructure evolution and layer bands of laser melting deposition Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.jallcom.2014.07.161 ↗
42. Crack propagation and fracture toughness of Ti6Al4V alloy produced by selective laser melting
43. Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
44. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
45. Influence of deposition strategies on tensile and fatigue properties in a wire + arc additive manufactured Ti-6Al-4V10.1016/j.ijfatigue.2021.106268 ↗
46. Effect of α texture on the tensile deformation behavior of Ti–6Al–4V alloy produced via electron beam rapid manufacturing10.1016/j.msea.2018.11.012 ↗
47. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
48. Influence of post-deposition heat treatments on the microstructure and tensile properties of Ti-6Al-4V parts manufactured by CMT-WAAM10.3390/met11081161 ↗
49. Designing against phase and property heterogeneities in additively manufactured titanium alloys10.1038/s41467-022-32446-2 ↗
50. Texture and anisotropy of a hot rolled Ti–16Nb alloy10.1016/j.jallcom.2010.04.022 ↗
51. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
52. A high strength and low modulus metastable β Ti-12Mo-6Zr-2Fe alloy fabricated by laser powder bed fusion in-situ alloying
53. Segregation and grain refinement in cast titanium alloys10.1557/jmr.2009.0173 ↗
54. Heterogeneous structure architected by additive manufacturing: facile route towards strong and ductile steel10.1080/21663831.2024.2314145 ↗
55. Heat-affected coarsening of β grain in titanium alloy during laser directed energy deposition10.1016/j.scriptamat.2021.114180 ↗
56. Recent advances in the kinetics of normal/abnormal grain growth: a review10.1007/s43452-021-00185-8 ↗
57. Grain growth in metals10.1016/0001-6160(57)90136-0 ↗
58. Development of an additively manufactured metastable beta titanium alloy with a fully equiaxed grain structure and ultrahigh yield strength
59. Beta fleck and segregation in titanium alloy ingots10.1515/HTMP.2006.25.5-6.337 ↗
60. Crystal growth mechanism and mechanical properties of Ti-6Al-4 V alloy during selective laser melting10.1016/j.matchar.2022.112455 ↗
61. Cantor · 2020