Enabling fast debinding of ceramic vat photopolymerization prints with supercritical carbon dioxide as a solvent

Nonna Nurmi, Erkka J. Frankberg, Milla Rinne, Teemu Sandblom, Piie Konnunaho, Erkki Levänen

Abstract

Thermal debinding of 3D-printed ceramics that include a large fraction of polymeric binders, can take several days to perform, and often includes a long thermal pre-conditioning step. In addition, means to reduce the manufacturing time are limited. This applies for thermal debinding of dense ceramics, such as dental restorations, that have been printed using vat photopolymerization (VPP) based technologies. The thermal debinding of such ceramics can be made faster, more economical, and more ecological by extracting selected slurry components prior to thermal debinding. Thus, creating flow channels for pyrolysis gases originating from the remaining binder polymers to exit the material. Here, supercritical carbon dioxide (scCO2) extraction was used to create such gas flow channels and to study which slurry components can be dissolved from VPP printed polymeric and ceramic/polymeric parts without significant delamination, cracking, or part deformation. The scCO2 extraction resulted in the creation of significant 33 vol.% of nanosized porosity in a pure polymeric as-built print, and 21 vol.% of nanosized porosity in a ceramic/polymeric composite print, where the ceramic powder remains in the part. These gas flow channels may allow faster thermal debinding while avoiding the creation of other defects. In the process, 90 wt.-% of the dissolvable resin fraction was extracted from the ceramic/polymeric prints already in 2 h without significant delamination, while 70 wt.-% of the dissolvable resin fraction was extracted in 2 h from the pure polymeric prints as a reference. This presents a novel, successful demonstration of a chemistry that allows both VPP printing and scCO2 extraction.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Injection Molding Process and Properties · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Stereolithography-fabricated zirconia dental prostheses: concerns based on clinical requirements10.1080/17436753.2019.1709687 ↗
2. Effects of the layer height and exposure energy on the lateral resolution of zirconia parts printed by lithography-based additive manufacturing10.3390/ma13061317 ↗
3. Study on debinding and sintering processes for ceramics fabricated using digital light processing (DLP) 3D printing10.3390/pr10112467 ↗
4. M.N. Rahaman, Ceramic processing, CRC Press/ Taylor & Francis, Boca Raton, FL., 2007.
5. Supercritical extraction with carbon dioxide and ethylene of poly(vinyl butyral) and dioctyl phthalate from multilayer ceramic capacitors10.1016/S0896-8446(02)00023-2 ↗
6. Mechanical properties of 3D-printed prosthetic materials compared with milled and conventional processing: a systematic review and meta-analysis of in vitro studies
7. J.Z. Shen, T. Kosmač, Advanced ceramics for dentistry, Butterworth-Heinemann, Waltham, MA, 2014.
8. Additive manufacturing of ZrO2 ceramic dental bridges by stereolithography10.1108/RPJ-09-2016-0144 ↗
9. H.R. Rezaie, H.B. Rizi, M.M. Rezaei Khamseh, A. Öchsner, Advanced Structured Materials A Review on Dental Materials, in: A Review on Dental Materials, Springer Nature, 2020. https://doi.org/https://doi.org/10.1007/978-3-030-48931-1.10.1007/978-3-030-48931-1 ↗
10. Current state-of-the-art and future perspectives of the three main modern implant-dentistry concerns: aesthetic requirements, mechanical properties, and peri-implantitis prevention10.1002/jbm.a.36661 ↗
11. Influence of boundary masks on dimensions and surface roughness using segmented exposure in ceramic 3D printing10.1016/j.ceramint.2018.11.031 ↗
12. Light curing strategies for lithography-based additive manufacturing of customized ceramics
13. Fabrication of dense zirconia-toughened alumina ceramics through a stereolithography-based additive manufacturing10.1016/j.ceramint.2016.10.027 ↗
14. Influence of irradiation parameters on the polymerization of ceramic reactive suspensions for stereolithography10.1016/j.jeurceramsoc.2017.05.050 ↗
15. Effects of solvent debinding on the microstructure and properties of 3D-printed alumina ceramics10.1021/acsomega.0c03944 ↗
16. Study on defect-free debinding green body of ceramic formed by DLP technology10.1016/j.ceramint.2019.09.237 ↗
17. Mechanisms of binder removal involved in supercritical debinding of injection moulded ceramics
18. Binder removal from ceramic green body in the environment of supercritical carbon dioxide with and without entrainers10.1016/0896-8446(91)90021-W ↗
19. Supercritical carbon dioxide debinding in metal injection molding (MIM) process10.1007/BF02707221 ↗
20. Influence of supercritical debinding and processing parameters on final properties of injection-moulded Inconel 71810.1016/j.powtec.2018.05.047 ↗
21. F. Bordet, T. Chartier, J.-F. Baumard, The Use of Co-Solvents in Supercritical Debinding of Ceramics, Journal of The European Ceramic Society - J Eur Ceram Soc 22 (2002) 1067–1072. https://doi.org/10.1016/S0955-2219(01)00398-3.10.1016/S0955-2219(01)00398-3 ↗
22. In vitro study of hydroxyapatite-based photocurable polymer composites prepared by laser stereolithography and supercritical fluid extraction10.1016/j.actbio.2008.05.024 ↗
23. Laser stereolithography and supercritical fluid processing for custom-designed implant fabrication10.1023/B:JMSM.0000011812.08185.2a ↗
24. 4D printing of shape-memory semi-interpenetrating polymer networks based on aromatic heterochain polymers10.1002/admt.202100790 ↗
25. J.M. DeSimone, W. Tumas, Green Chemistry Using Liquid and Supercritical Carbon Dioxide, Oxford University Press, Incorporated, Oxford, UNITED STATES, 2003.10.1093/oso/9780195154832.001.0001 ↗
26. T. Wu, B. Han, Supercritical Carbon Dioxide (CO2) as Green Solvent, in: B. Han, T. Wu (Eds.), Green Chemistry and Chemical Engineering, Springer New York, New York, NY, 2019: pp. 173–197. https://doi.org/10.1007/978-1-4939-9060-3_391.10.1007/978-1-4939-9060-3_391 ↗
27. Liquid and supercritical carbon dioxide as organic solvents10.1021/jo00200a016 ↗
28. Specific intermolecular interaction of carbon dioxide with polymers10.1021/ja950416q ↗
29. A review on the rheological behavior and formulations of ceramic suspensions for vat photopolymerization10.1016/j.ceramint.2021.01.031 ↗
30. Photopolymerization of ceramic resins by stereolithography process: a review
31. V. Goodship, E. Ogur, Polymer Processing with Supercritical Fluids, iSmithers Rapra Publishing, Shrewsbury, UNITED STATES, 2004.
32. Non-fluorous polymers with very high solubility in supercritical CO2 down to low pressures10.1038/35012040 ↗
33. Morphology and thermomechanical properties in epoxy acrylate interpenetrated networks10.1002/masy.201650012 ↗
34. Microscopic origins for the favorable solvation of carbonate ether copolymers in CO210.1021/ja0510008 ↗
35. Solubility, in supercritical carbon dioxide, of paraffin waxes used as binders for low-pressure injection molding10.1021/ie980552e ↗
36. A.J. Hunt, T.M. Attard, Solubility and Synthesis of Polymers Using Supercritical Carbon Dioxide, in: T.M. Attard, A.J. Hunt (Eds.), Supercritical and Other High-Pressure Solvent Systems - For Extraction, Reaction and Material Processing, The Royal Society of Chemistry, 2018: pp. 340–373. www.rsc.org.10.1039/9781788013543-00340 ↗
37. Solubility of polymers and copolymers in supercritical CO210.1021/jp9615823 ↗
38. Influence of residual monomer on cracking in ceramics fabricated by stereolithography10.1111/j.1744-7402.2010.02578.x ↗
39. M.A. McHugh, V.J. Krukonis, Supercritical Fluid Extraction (2nd Edition), Elsevier, Newton, MA, 1994.
40. Role of supercritical carbon dioxide (scCO2) in fabrication of inorganic-based materials: a green and unique route10.1080/14686996.2021.1955603 ↗
41. Supercritical carbon dioxide as a green solvent for processing polymer melts: processing aspects and applications10.1016/j.progpolymsci.2005.08.002 ↗
42. A comprehensive review of the photopolymerization of ceramic resins used in stereolithography
43. Ceramic stereolithography: additive manufacturing for 3D complex ceramic structures10.4191/kcers.2017.54.6.12 ↗
44. A systematic study of vat-polymerization binders with potential use in the ceramic suspension 3D printing
45. J. Parameswaranpillai, N. Hameed, J. Pionteck, E.M. Woo, Handbook of Epoxy Blends, Springer Nature, 2017. https://doi.org/10.1007/978-3-319-40043-3.10.1007/978-3-319-40043-3 ↗
46. Visible light curable restorative composites for dental applications based on epoxy monomer10.3390/ma7010554 ↗
47. Extraction of binders with supercritical carbon dioxide10.4028/www.scientific.net/KEM.132-136.4 ↗
48. Supercritical debinding of injection molded ceramics10.1111/j.1151-2916.1995.tb08890.x ↗
49. Influence of resin composition on the defect formation in alumina manufactured by stereolithography10.3390/ma10020138 ↗
50. Effect of plasticizer on the fabrication and properties of alumina ceramic by stereolithography-based additive manufacturing10.1016/j.ceramint.2018.07.259 ↗
51. Synergy of solid loading and printability of ceramic paste for optimized properties of alumina via stereolithography-based 3D printing10.1016/j.jmrt.2020.08.038 ↗
52. Pressure distribution and defect formation in green ceramic bodies during supercritical extraction of binder10.1111/j.1551-2916.2008.02896.x ↗
53. Debinding behaviors of injection molded ceramic bodies with nano-sized pore channels during extraction using supercritical carbon dioxide and n-heptane solvent10.1016/j.supflu.2009.09.011 ↗
54. Extraction of binders from green ceramic bodies by supercritical fluid: influence of the porosity10.1016/S0955-2219(01)00474-5 ↗
55. O. Dugauguez, Application of unconventional methods on lnconel 718 MIM components, Université Bourgogne Franche-Comté; Universidad autonóma de Madrid, 2020. https://tel.archives-ouvertes.fr/tel-02550981.
56. Synthesis of an aqueous self-matting acrylic resin with low gloss and high transparency via controlling surface morphology
57. M.G. González, J.C. Cabanelas, J. Baselga, Applications of FTIR on Epoxy Resins - Identification, Monitoring the Curing Process, Phase Separation and Water Uptake, in: Infrared Spectroscopy - Materials Science, Engineering and Technology, InTech, 2012. https://doi.org/10.5772/36323.10.5772/36323 ↗