journal article·2022-12

Laser-melted Al-3.6Mn-2.0Fe-1.8Si-0.9Zr (wt%) alloy with outstanding creep resistance via formation of α-Al(FeMn)Si precipitates

Jovid U. Rakhmonov, Nhon Q. Vo, Joseph R. Croteau, Joshua Dorn, David C. Dunand

Publisher page

Abstract

Microstructural development during solidification and subsequent aging, and the resulting creep resistance, of laser powder-bed fusion (LPBF) Al-3.6Mn-2.0Fe-1.8Si-0.9Zr (wt%) alloy has been investigated. A bimodal grain structure is observed within the melt pool, with the bottom (MPB) exhibiting ultrafine equiaxed grains (∼ 1 µm in diameter) and the top/center (MPT) displaying fine epitaxial grains (∼ 10 µm in diameter). It is demonstrated that primary α-Al(FeMn)Si precipitates act as nuclei for α-Al grains and cause grain refinement at the MPB, thus preventing solidification cracking during processing of this complex alloy via LPBF. The α-Al(FeMn)Si precipitates formed alongside α-Al during solidification extensively decorate grain boundaries and are distributed uniformly within grain interiors. The subsequent aging of the alloy forms densely distributed L12-Al3Zr nanoprecipitates in the α-Al matrix without coarsening the α-Al(FeMn)Si particles. The alloy exhibits outstanding compressive creep resistance in both diffusional and dislocation creep regimes, which is predominantly attributed to the large fraction (∼ 15 vol%) of fine, semi-coherent α-Al(FeMn)Si precipitates that limit the creep flow by restricting both grain-boundary sliding and dislocation motion. With a compressive threshold stress of ∼ 74 MPa for dislocation climb at 300 °C, this alloy greatly outperforms most creep-resistant Al alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Recent advances in the metallurgy of aluminum alloys. Part II: age hardening10.1016/j.crhy.2018.10.012 ↗
2. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing
3. Elevated temperature microstructural stability in cast AlCuMnZr alloys through solute segregation10.1016/j.msea.2019.138279 ↗
4. Coarsening- and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
5. Effects of Mo and Mn microadditions on strengthening and over-aging resistance of nanoprecipitation-strengthened Al-Zr-Sc-Er-Si alloys10.1016/j.actamat.2018.11.031 ↗
6. Improving aging and creep resistance in a dilute Al–Sc alloy by microalloying with Si, Zr and Er10.1016/j.actamat.2013.10.008 ↗
7. Effects of Al(MnFe)Si dispersoids with different sizes and number densities on microstructure and ambient/elevated-temperature mechanical properties of extruded Al-Mg-Si AA6082 alloys with varying Mn content
8. The effect of transition elements on high-temperature mechanical properties of AlSi foundry alloys-a review10.1002/adem.201500468 ↗
9. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
10. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
11. Laser powder bed fusion of a near-eutectic Al–Fe binary alloy: processing and microstructure
12. Solidification microstructure, aging evolution and creep resistance of laser powder-bed fused Al-7Ce-8Mg (wt%)
13. Comparing evolution of precipitates and strength upon aging of cast and laser-remelted Al–8Ce-0.2Sc-0.1Zr (wt%)10.1016/j.msea.2022.142990 ↗
14. Change in microstructural characteristics of laser powder bed fused Al–Fe binary alloy at elevated temperature10.1016/j.jmst.2021.04.038 ↗
15. An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion
16. Influence of melt superheat, Sr modifier, and Al-5Ti-1B grain refiner on microstructural evolution of secondary Al-Si-Cu alloys10.1007/s11661-016-3716-z ↗
17. Influence of the heat treatment on the precipitation of the intermetallic phases in commercial AlMn1FeSi alloy10.1016/j.jmatprotec.2004.07.125 ↗
18. Precipitation of partially coherent α-Al(Mn,Fe)Si dispersoids and their strengthening effect in AA 3003 alloy10.1016/j.actamat.2011.11.003 ↗
19. Dispersoid strengthening in AA3xxx alloys with varying Mn and Si content during annealing at low temperatures10.1016/j.msea.2013.01.004 ↗
20. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
21. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
22. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
23. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
24. Introduction and comparison of new EBSD post-processing methodologies10.1016/j.ultramic.2015.08.001 ↗
25. Re-refinement of α-(AlMnSi)10.1107/S0108270197015989 ↗
26. Quantifying internal strains, stresses, and dislocation density in additively manufactured AlSi10Mg during loading-unloading-reloading deformation10.1016/j.matdes.2020.109339 ↗
27. Thermal mismatch dislocations produced by large particles in a strain-hardening matrix10.1016/0921-5093(91)90557-4 ↗
28. Laser powder bed fusion of high-strength Sc/Zr-modified Al–Mg alloy: phase selection, microstructural/mechanical heterogeneity, and tensile deformation behavior10.1016/j.jmst.2021.03.069 ↗
29. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior10.1016/j.jmst.2020.08.003 ↗
30. Origin of non-uniform plasticity in a high-strength Al-Mn-Sc based alloy produced by laser powder bed fusion10.1016/j.jmst.2021.06.042 ↗
31. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
32. Selective laser melting of a high strength Al Mn Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
33. Microstructural features and mechanical properties of a novel Ti- and Zr-modified Al-Mn alloy processed by laser powder bed fusion10.1016/j.jallcom.2021.163156 ↗
34. Heterogeneous nucleation of α-Al grain on primary α-AlFeMnSi intermetallic investigated using 3D SEM ultramicrotomy and HRTEM10.1007/s11661-014-2346-6 ↗
35. Precipitation behaviors of cubic and tetragonal Zr–rich phase in Al–(Si–)Zr alloys10.1016/j.jallcom.2016.02.236 ↗
36. TEM and HREM study of Al3Zr precipitates in an Al-Mg-Si-Zr alloy10.1111/j.1365-2818.2006.01615.x ↗
37. Modelling of inoculation of metallic melts: application to grain refinement of aluminium by Al–Ti–B10.1016/S1359-6454(00)00094-X ↗
38. J.A. Glerum, J. Mogonye, D.C. Dunand, Creep properties and microstructure evolution at 260–300 °C of AlSi10Mg manufactured via laser powder-bed fusion, 2022.10.1016/j.msea.2022.143075 ↗
39. Effect of Er additions on ambient and high-temperature strength of precipitation-strengthened Al–Zr–Sc–Si alloys10.1016/j.actamat.2012.02.030 ↗
40. Microstructure and mechanical properties of a precipitation-strengthened Al-Zr-Sc-Er-Si alloy with a very small Sc content10.1016/j.actamat.2017.10.040 ↗
41. Ambient- and elevated temperature properties of Sc- and Zr-modified Al–6Ni alloys strengthened by Al3Ni microfibers and Al3(Sc,Zr) nanoprecipitates10.1016/j.msea.2022.142963 ↗
42. The applicability of Norton's creep power law and its modified version to a single-crystal superalloy type CMSX-210.1016/0921-5093(96)10400-7 ↗
43. M.E. Kassner, Fundamentals of Creep in Metals and Alloys (Third Edition), Butterworth-Heinemann, Boston, 2015.10.1016/B978-0-08-099427-7.00001-3 ↗
44. H.J. Frost, M.F. Ashby, Deformation-mechanism Maps: The Plasticity and Creep of Metals and Ceramics, Pergamon Press, New York, 1982.
45. Influence of grain size, solute atoms and second-phase particles on creep behavior of polycrystalline solids10.1016/S0921-5093(01)01121-2 ↗
46. High-temperature creep mechanism in an Al-2 at% Mg alloy determined by stress-relaxation tests10.1016/0036-9748(76)90206-4 ↗
47. H. Sato, H. Oikawa, Effects of solute concentration on creep characteristics of solution hardened Ai-Mg alloys at 600 K, In: Proceedings of the 4th International Conference on Aluminum Alloys, Their Physical and Mechanical Properties, 1995.
48. Warm-temperature tensile ductility in Al-Mg alloys10.1007/s11661-998-0300-1 ↗
49. Five-power-law creep in single phase metals and alloys10.1016/S0079-6425(99)00006-7 ↗
50. Mechanisms of creep deformation in a rapidly solidified Al–Fe–V–Si alloy10.1016/j.msea.2021.140796 ↗
51. High temperature creep deformation of an Al–Fe–V–Si Alloy10.1016/S0921-5093(98)00876-4 ↗
52. Quantitative study on the precipitation behavior of dispersoids in DC-cast AA3003 alloy during heating and homogenization10.1016/S1359-6454(03)00160-5 ↗
53. Strengthening of an Al–Cu–Sn alloy by deformation-resistant precipitate plates10.1016/j.actamat.2008.03.028 ↗
54. On the threshold stress for dislocation creep in particle strengthened alloys10.1016/0001-6160(85)90018-5 ↗
55. Creep of metals containing high volume fractions of unshearable dispersoids—Part II. Experiments in the Al∙Al2O3 system and comparison to models10.1016/S1359-6454(97)00136-5 ↗
56. Deformation behaviour under constant structure of creep-resistant Al-Fe alloys10.1007/BF00721014 ↗
57. Threshold stresses for dislocation climb over hard particles: the effect of an attractive interaction10.1016/0001-6160(86)90247-6 ↗
58. Strengthening mechanisms in AlNiSc alloys containing Al3Ni microfibers and Al3Sc nanoprecipitates10.1016/j.actamat.2018.10.059 ↗
59. Microstructure and creep properties of cast near-eutectic Al–Ce–Ni alloys10.1016/j.msea.2021.142551 ↗
60. Solute-induced strengthening during creep of an aged-hardened Al-Mn-Zr alloy10.1016/j.actamat.2021.117268 ↗
61. Cavitation-resistant intergranular precipitates enhance creep performance of θ′-strengthened Al-Cu based alloys10.1016/j.actamat.2022.117788 ↗
62. Dislocation-θ′ (Al2Cu) interactions during creep deformation of an Al-Cu alloy10.1016/j.scriptamat.2022.114739 ↗
63. High temperature deformation of oxide dispersion strengthened al and Al∙Mg solid solutions10.1016/0001-6160(82)90153-5 ↗
64. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗
65. Influence of grain refiner addition on the precipitation of Fe-rich phases in secondary AlSi7Cu3Mg alloys