Surface pick-up of argon during hot isostatic pressing of material built by laser powder bed fusion
Source abstract
Abstract
Abstract In prior studies, gas atomisation and L-PBF under argon atmosphere caused some pick-up of argon by the material. The gas used during HIP is argon which raises the question if the material can pick-up argon here as well. Hence, the impact of HIP on argon content of the near-surface and bulk in AM-material was investigated in this study. We found that the argon content near the surface increased significantly (of IN718, HX, C276), while the bulk content remained unchanged. Rough surfaces, time in HIP and especially oxidised surfaces prior to HIP all aggravated the argon pick-up. Since the influence of the surface argon pick-up on fatigue performance is not yet known, we recommend that critical components should be machined, blasted, ground or polished after HIP. If that is not possible, components should possess non-oxidised surfaces prior to HIP. By following these guidelines, any risk of a decline in performance of the material can be mitigated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Sophie Dubiez-Le Goff, Pelle Mellin. Artificial Porosity Introduced During L-PBF of IN718, and its Effect on Fatigue Performance Before and After HIP
2. Additive Manufacturing Technologies
3. ASTM F2792-12a · 2012
4. Laser powder bed fusion additive manufacturing of metals; physics, computational, and materials challenges10.1063/1.4937809 ↗
5. 2 - Powder bed fusion processes: An overview
6. Hot isostatic pressing of IN718 components manufactured by selective laser melting
7. Effect of argon and nitrogen atmospheres on the properties of stainless steel 316 L parts produced by laser-powder bed fusion10.1016/j.matdes.2019.107873 ↗
8. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
9. J.P. Kruth, M. Badrossamay, E. Yasa, J. Deckers, L. Thijs, J. van Humbeeck, Part and material properties in selective laser melting of metals. In: Proceedings of the 16th International Symposium on Electromachining, 2010.
10. Investigation of the mechanisms by which hot isostatic pressing improves the fatigue performance of powder bed fused Ti-6Al-4V10.1016/j.ijfatigue.2018.10.015 ↗
11. Effects of defects, surface roughness and hip on fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.prostr.2017.11.055 ↗
12. Analyzing the effects of powder and post-processing on porosity and properties of electron beam melted Ti-6Al-4V10.1080/21663831.2017.1340911 ↗
13. Solubility of argon in laser additive manufactured α-titanium under hot isostatic pressing condition10.1016/j.commatsci.2017.01.040 ↗
14. Fundamental aspects of hot isostatic pressing: an overview10.1007/s11661-000-0078-2 ↗
15. Microstructure and mechanical properties of pure titanium models fabricated by selective laser melting10.1243/0954406041319545 ↗
16. Porosity regrowth during heat treatment of hot isostatically pressed additively manufactured titanium components10.1016/j.scriptamat.2016.05.002 ↗
17. Process gas infiltration in inconel 718 samples during SLM processing
18. National Research Council · 1981
19. Effects of process parameters on porosity in laser powder bed fusion revealed by X-ray tomography
20. Dynamics of pore formation during laser powder bed fusion additive manufacturing10.1038/s41467-019-10009-2 ↗
21. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
22. Topi Kosonen, Katri Kakko, Niko Raitanen. Evaluation of pore re-opening after HIP in LPBF Ti-6Al-4V. Proceedings of the Euro PM2020 Virtual Congress; ‘in press’ 2020.10.1080/00325899.2021.1928997 ↗
23. The structure and properties of a nickel-base superalloy produced by osprey atomization-deposition10.1007/BF02643977 ↗
24. High temperature oxidation effects on surface roughness of Ti–4Al–2V10.1179/1743294412Y.0000000106 ↗
25. Cyclic oxidation behavior of IN 718 superalloy in air at high temperatures10.1007/s11085-010-9230-6 ↗