Enhancing fatigue life of as-printed martensitic M789 steel produced by laser powder bed fusion via in-process surface integrity improvement and phase change induced compressive residual stresses
Source abstract
Abstract
The fatigue strength of metal components produced by Laser Powder Bed Fusion (LPBF) is often impaired by their limited surface quality, and surface finishing post-processing steps are typically required to improve the fatigue behavior. However, the complex geometries of LPBF parts sometimes inhibit conventional surface finishing. Recently, Incremental Dual Laser PBF (IDLPBF) was introduced as a strategy for in-process quality improvement of up-facing inclined surfaces by alternating between building and laser remelting in height steps of 1.5 mm. This improvement is achieved through selective powder removal using laser-induced shock waves and subsequent laser remelting of the uncovered inclined surface. The current study demonstrates a substantial improvement in the fatigue life of as-printed martensitic M789 steel via simultaneous in-process improvement of surface quality, engineering of phase change induced compressive residual surface stresses, and removal of subsurface pores. The investigation encompasses four-point bending fatigue analysis of samples inclined by 5° to 60° treated by IDLPBF in comparison to as-built (AB) and laser remolten (LR) reference samples. IDLPBF samples showed a notable increase in fatigue life by up to 69% compared to AB samples, despite the presence of high tensile residual surface stresses (420 MPa). The improved fatigue life was primarily attributed to significantly reduced surface roughness and corresponding stress concentration factor by 40% and 50%, respectively. The LR reference samples showed further increased fatigue life due to the presence of compressive residual surface stresses (- 280 MPa), caused by a locally induced martensitic transformation. By leveraging this phenomenon, a modified IDLPBF strategy was employed to induce desirable compressive residual surface stresses (-109 MPa), which significantly enhanced the fatigue life compared to AB samples by up to 600% and, moreover, demonstrated a performance similar to LR samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (81)
Show source-provided references
1. Metal additive manufacturing cycle in aerospace industry: a comprehensive review
2. Additive manufacturing for the automotive industry
3. Additive manufacturing processes in medical applications10.3390/ma14010191 ↗
4. Defects as a root cause of fatigue failure of metallic components. I: Basic aspects10.1016/j.engfailanal.2019.01.055 ↗
5. Defects as a root cause of fatigue failure of metallic components. II: Non-metallic inclusions10.1016/j.engfailanal.2019.01.054 ↗
6. Defects as a root cause of fatigue failure of metallic components. III: Cavities, dents, corrosion pits, scratches10.1016/j.engfailanal.2019.01.034 ↗
7. Effects of defects on mechanical properties in metal additive manufacturing: a review focusing on X-ray tomography insights10.1016/j.matdes.2019.108385 ↗
8. Combined effect of surface anomalies and volumetric defects on fatigue assessment of AlSi7Mg fabricated via laser powder bed fusion
9. Additive manufacturing of metallic components – Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
10. Process defects and in situ monitoring methods in metal powder bed fusion: a review10.1088/1361-6501/aa5c4f ↗
11. Effects of process parameters on porosity in laser powder bed fusion revealed by X-ray tomography
12. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
13. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
14. Hot isostatic pressing in metal additive manufacturing: X-ray tomography reveals details of pore closure
15. A review on the state-of-the-art of surface finishing processes and related ISO/ASTM standards for metal additive manufactured components10.1080/17452759.2020.1830346 ↗
16. Fatigue life prediction of a L-PBF component in Ti-6Al-4V using sample data, FE-based simulations and machine learning10.1016/j.ijfatigue.2022.107276 ↗
17. Analysis of the effect of surface roughness on fatigue performance of powder bed fusion additive manufactured metals10.1016/j.tafmec.2020.102638 ↗
18. Killer notches: The effect of as-built surface roughness on fatigue failure in AlSi10Mg produced by laser powder bed fusion
19. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
20. Texture of inclined up-facing surfaces in laser powder bed fusion of metals
21. Surface texture measurement for additive manufacturing
22. Surface post-treatments for metal additive manufacturing: Progress, challenges, and opportunities
23. Effect of Surface and Subsurface Defects on Fatigue Behavior of AlSi10Mg Alloy Processed by Laser Powder Bed Fusion (L-PBF)10.3390/met9101063 ↗
24. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
25. Laser powder bed fused 304 L steel shot-peened with various ceramic shot sizes: Surface/subsurface characteristics, tensile behavior, and fatigue behavior10.1016/j.ijplas.2023.103784 ↗
26. Laser polishing: a review of a constantly growing technology in the surface finishing of components made by additive manufacturing10.1007/s00170-022-08840-x ↗
27. Laser processing of freeform surfaces: a new approach based on an efficient workpiece partitioning strategy10.1016/j.ijmachtools.2020.103593 ↗
28. Practical implementation of laser polishing on additively manufactured metallic components10.2351/7.0000222 ↗
29. Review on mechanism and process of surface polishing using lasers10.1007/s11465-019-0535-0 ↗
30. Laser polishing of additively manufactured metal parts: a review10.1080/02670844.2022.2072080 ↗
31. Effect of laser remelting on deposition quality, residual stress, microstructure, and mechanical property of selective laser melting processed Ti-5Al-2.5Sn alloy10.1016/j.matchar.2019.02.010 ↗
32. Pore elimination mechanisms during 3D printing of metals10.1038/s41467-019-10973-9 ↗
33. Healing of keyhole porosity by means of defocused laser beam remelting: Operando observation by X-ray imaging and acoustic emission-based detection
34. Influences of laser remelting on mechanical performances of AISI4140 steel10.1177/02670836231212614 ↗
35. Effect of higher laser power remelting on porosity and mechanical performance of part built by laser powder bed fusion10.1007/s00170-023-11067-z ↗
36. Low-cycle fatigue performance of remelted laser powder bed fusion (L-PBF) biomedical Ti25Ta10.1016/j.msea.2020.140228 ↗
37. Influence of a remelt scan strategy on the microstructure and fatigue behaviour of additively manufactured biomedical Ti65Ta efficiently assessed using small scale specimens10.1016/j.ijfatigue.2022.106944 ↗
38. Role of laser remelting and heat treatment in mechanical and tribological properties of selective laser melted Ti6Al4V alloy10.1016/j.jallcom.2021.163207 ↗
39. Laser polishing for improving fatigue performance of additive manufactured Ti-6Al-4V parts10.1016/j.optlastec.2020.106639 ↗
40. Material characterization, thermal analysis, and mechanical performance of a laser-polished Ti Alloy prepared by selective laser melting
41. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
42. Laser polishing of Ti6Al4V fabricated by selective laser melting
43. Surface treatment of powder-bed fusion additive manufactured metals for improved fatigue life10.1007/s11665-018-3732-9 ↗
44. Pore healing effect of laser polishing and its influence on fatigue properties of 316 L stainless steel parts fabricated by laser powder bed fusion10.1016/j.optlastec.2022.108535 ↗
45. Effects of different surface modifications on the fatigue life of selective laser melted 15–5 PH stainless steel10.1016/j.msea.2019.138109 ↗
46. Novel strategy for quality improvement of up-facing inclined surfaces of LPBF parts by combining laser-induced shock waves and in situ laser remelting
47. Improving fatigue performance of metal parts with up-facing inclined surfaces produced by laser powder bed fusion and in-situ laser remelting
48. Enhanced fatigue life of additively manufactured high-strength TiB2-reinforced Al-Cu-Mg-Ag composite through in-process surface modification during hybrid laser processing10.1080/17452759.2023.2276247 ↗
49. Improved surface quality and fatigue life of high-strength, hybrid particle reinforced (Ti+B4C)/Al-Cu-Mg metal matrix composite processed by dual-laser powder bed fusion10.1016/j.prostr.2024.01.003 ↗
50. Investigation of an incremental dual Laser Powder Bed Fusion strategy for improving the quality of up-facing inclined surfaces10.1016/j.procir.2022.08.104 ↗
51. Novel strategy for automated quality enhancement of up-facing inclined surfaces by incremental dual laser powder bed fusion
52. Böhler, www.bohler-edelstahl.com/en/products/m789-ampo, (2023).
53. Application of laser-based powder bed fusion for direct metal tooling10.3390/met11030458 ↗
54. Advances in maraging steels for additive manufacturing10.1007/s00501-019-0835-z ↗
55. 3DSystems, www.3dsystems.com/materials/certified-m789-a, (2023).
56. Improving the quality of up-facing inclined surfaces in laser powder bed fusion of metals using a dual laser setup10.1016/j.procir.2020.09.050 ↗
57. Hetnarski · 2014
58. ISO 16610-21, 2011. Geometrical product specifications (GPS) – Filtration – Part 21: Linear profile filters: Gaussian filters.
59. ISO 21920-3, 2021. Geometrical product specifications (GPS). Surface texture: Profile – Part 3: Specific operators.
60. ISO 21920-2, 2021. Geometrical product specifications (GPS). Surface texture: Profile – Part 2: Terms, definitions and surface.
61. Noyan · 1987
62. A method for obtaining and analyzing sensitivity data10.1080/01621459.1948.10483254 ↗
63. Study on the microstructure, mechanical property and residual stress of SLM Inconel-718 alloy manufactured by differing island scanning strategy10.1016/j.optlastec.2015.07.009 ↗
64. Effect of scanning strategies on residual stress and mechanical properties of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
65. Stress and deformation evaluations of scanning strategy effect in selective laser melting
66. Residual Stresses at Laser Surface Remelting and Additive Manufacturing10.1016/j.phpro.2011.03.032 ↗
67. Directional and oscillating residual stress on the mesoscale in additively manufactured Ti-6Al-4V10.1016/j.actamat.2019.01.050 ↗
68. The role of defect structure and residual stress on fatigue failure mechanisms of Ti-6Al-4V manufactured via laser powder bed fusion: Effect of process parameters and geometrical factors10.1016/j.jmapro.2023.07.014 ↗
69. Analysis of dynamic recrystallization through austenite grain reconstruction of additively manufactured martensitic M789 steel10.1016/j.msea.2024.146345 ↗
70. The effect of heat treatments on mechanical properties of M789 steel fabricated by laser powder bed fusion10.1016/j.jallcom.2021.161033 ↗
71. Laser powder bed fusion of M789 maraging steel on Cr–Mo N709 steel: microstructure, texture, and mechanical properties10.1016/j.msea.2022.142827 ↗
72. Precipitation behaviour at the interface of an additively manufactured M789–N709 hybrid alloy10.1007/s40195-023-01558-z ↗
73. The effect of laser focus shift on microstructural variation of Inconel 718 produced by selective laser melting10.1016/j.matdes.2018.04.019 ↗
74. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
75. New aspects about the search for the most relevant parameters optimizing SLM materials
76. Dynamics of pore formation during laser powder bed fusion additive manufacturing10.1038/s41467-019-10009-2 ↗
77. Effect of low transformation temperature weld filler metal on welding residual stress10.1179/136217110X12714217309614 ↗
78. Characterization of microstructure and residual stress in a 3D H13 tool steel component produced by additive manufacturing10.1557/jmr.2014.190 ↗
79. R. Mertens, S. Dadbakhsh, J.Van Humbeeck, J.P. Kruth, Application of base plate preheating during selective laser melting, in: Procedia CIRP, Elsevier B.V., 2018: pp. 5–11. https://doi.org/10.1016/j.procir.2018.08.002.10.1016/j.procir.2018.08.002 ↗
80. Kinetics of Martensitic transformation in partially bainitic 300 M steel10.1016/0921-5093(90)90273-6 ↗
81. Oerlikon,https://www.oerlikon.com/en/, (2024).