Microstructure tailoring of a wire-arc DED processed Ti6242 alloy for high damage tolerance performance
Source abstract
Abstract
This paper examines the effects of interpass hammer peening and post-process β annealing on the tensile properties, high-cycle fatigue, and fatigue crack growth behaviour of the titanium alloy Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Ti6242), processed via wire-arc directed energy deposition (w-DED, also known as WAAM). A major challenge in additive manufacturing of titanium alloys is the development of a coarse columnar grain structure under standard build conditions, leading to significant anisotropy and variability in mechanical properties. This study demonstrates that interpass peening effectively refines the grain structure by inducing recrystallization, resulting in isotropic properties and increased strength without compromising fatigue crack growth resistance. Additionally, post-deposition annealing above the β-transus temperature (β annealing) significantly reduces the fatigue crack growth rate by an order of magnitude through microstructural refinement. The formation of coarse single-variant lamellar colonies promotes crack path branching and deviation, enhancing fatigue crack growth performance. Combining in-process grain refinement via peening with post-process β annealing further increases the threshold stress intensity factor by 2.5 times. These improvements provide substantial benefits for damage-tolerant design principles.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Welsch · 1994
2. High Temperature Alloys
3. Energy and emissions saving potential of additive manufacturing: the case of lightweight aircraft components10.1016/j.jclepro.2015.04.109 ↗
4. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
5. Wire + Arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
6. Comparison of microstructure refinement in wire-arc additively manufactured Ti–6Al–2Sn–4Zr–2Mo–0.1Si and Ti–6Al–4V built with inter-pass deformation10.1007/s11661-022-06811-1 ↗
7. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1007/s11661-012-1444-6 ↗
8. Influence of deposition strategies on tensile and fatigue properties in a wire + arc additive manufactured Ti-6Al-4V10.1016/j.ijfatigue.2021.106268 ↗
9. Controlling the microstructure and properties of wire arc additive manufactured Ti-6Al-4V with trace boron additions10.1016/j.actamat.2015.03.035 ↗
10. Trace carbon addition to refine microstructure and enhance properties of additive-manufactured Ti-6Al-4V10.1007/s11837-018-2994-x ↗
11. High strength Ti alloy fabricated by directed energy deposition with in-situ Cu alloying10.1016/j.jmatprotec.2022.117759 ↗
12. Isomorphic grain inoculation in Ti-6Al-4V during additive manufacturing
13. The potential for grain refinement of Wire-Arc Additive Manufactured (WAAM) Ti-6Al-4V by ZrN and TiN inoculation
14. Achieving a columnar-to-equiaxed transition through dendrite twinning in high deposition rate additively manufactured titanium Alloys10.1007/s11661-024-07388-7 ↗
15. Refinement of Ti-6Al-4V prior-β grain structure in the as-deposited condition via process control during wire-direct energy deposition
16. The effectiveness of combining rolling deformation with wire–arc additive manufacture on β-grain refinement and texture modification in Ti–6Al–4V10.1016/j.matchar.2016.02.001 ↗
17. Mechanical properties enhancement of additive manufactured Ti-6Al-4V by machine hammer peening
18. Improved microstructure and increased mechanical properties of additive manufacture produced TI-6AL-4V by interpass cold rolling
19. Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
20. Selective laser melting of a Near-α Ti6242S alloy for high-performance automotive parts10.1002/adem.202001194 ↗
21. Effect of annealing temperature on microstructure and high-temperature tensile behaviour of Ti-6242S alloy produced by Laser Powder Bed Fusion10.1080/26889277.2021.1997341 ↗
22. Effects of Postprocess Hot Isostatic Pressing Treatments on the Mechanical Performance of EBM Fabricated TI-6Al-2Sn-4Zr-2Mo10.3390/ma13112604 ↗
23. Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)10.1016/j.msea.2020.139533 ↗
24. Tailoring the microstructure and mechanical property of laser powder bed fusion fabricated Ti–6Al–2Sn–4Zr–2Mo via heat treatment10.1016/j.jallcom.2021.162648 ↗
25. Effect of microstructure on the fatigue properties of Ti–6Al–4V titanium alloys10.1016/j.matdes.2012.10.059 ↗
26. Relationship between microstructures, facet morphologies at the high-cycle fatigue (HCF) crack initiation site, and HCF strength in Ti-6242S10.1016/j.msea.2018.04.043 ↗
27. Fatigue of the Near-Alpha Ti-Alloy Ti624210.1007/s11340-009-9238-5 ↗
28. High-temperature mechanical performance of directed energy deposited Ti6242S alloy10.1016/j.msea.2022.143526 ↗
29. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: Bimodal vs. lamellar structures10.1007/s11661-002-0160-z ↗
30. Crystallography of fatigue crack initiation and growth in fully lamellar Ti-6Al-4V10.1007/s11661-009-0064-2 ↗
31. Effect of α phase on fatigue crack growth of Ti-6242 alloy10.1016/S1006-706X(17)30121-8 ↗
32. Effect of microstructure on the fatigue crack growth behaviour of a near-α Ti alloy10.1016/j.ijfatigue.2014.12.013 ↗
33. Relationship between microstructures, facet morphologies at the high-cycle fatigue (HCF) crack initiation site, and HCF strength in Ti-6242S10.1016/j.msea.2018.04.043 ↗
34. Influence of Deposition Strategies on Residual Stress in Wire + Arc Additive Manufactured Titanium Ti-6Al-4V
35. ASTM E112-13, Standard Test Methods for Determining Average Grain Size, in: 2021.
36. Development of Microstructure and Crystallographic Texture during Stationary Shoulder Friction Stir Welding of Ti-6Al-4V10.1007/s11661-011-0606-2 ↗
37. ASTM E647-15e1, Standard Test Method for Measurement of Fatigue Crack Growth Rates, in: ASTM International, West Conshohocken, PA, 2015.
38. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
39. Grain morphology evolution and texture characterization of wire and arc additive manufactured Ti-6Al-4V10.1016/j.jallcom.2018.07.235 ↗
40. Microstructural characterisation and mechanical properties of Ti-5Al-5V-5Mo-3Cr built by wire and arc additive manufacture10.1080/14786435.2022.2113470 ↗
41. The effect of processing parameters on rapid-heating β recrystallization in inter-pass deformed Ti-6Al-4V wire-arc additive manufacturing10.1016/j.matchar.2020.110298 ↗
42. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
43. Prior β grain evolution and phase transformation of selective laser melted Ti6Al4V alloy during heat treatment10.1016/j.jallcom.2022.165235 ↗
44. Early Stages of Microstructure and Texture Evolution during Beta Annealing of Ti-6Al-4V10.1007/s11661-017-4444-8 ↗
45. The effect of loading direction on strain localisation in wire arc additively manufactured Ti–6Al–4V10.1016/j.msea.2020.139608 ↗
46. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
47. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
48. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
49. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
50. Donachie · 2000
51. Strong morphological and crystallographic texture and resulting yield strength anisotropy in selective laser melted tantalum10.1016/j.actamat.2013.04.036 ↗
52. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
53. Role of microstructure heterogeneity on deformation behaviour in additive manufactured Ti-6Al-4V
54. Mechanical performance and microstructural characterisation of titanium alloy-alloy composites built by wire-arc additive manufacture10.1016/j.msea.2019.138289 ↗
55. A Stress-Strain Function for the Fatigue of Metals
56. The role of microstructure and local crystallographic orientation near porosity defects on the high cycle fatigue life of an additive manufactured Ti-6Al-4V10.1016/j.matchar.2020.110576 ↗
57. The role of microstructure and local crystallographic orientation near porosity defects on the high cycle fatigue life of an additive manufactured Ti-6Al-4V10.1016/j.matchar.2020.110576 ↗
58. Anisotropy of fatigue crack growth in wire arc additive manufactured Ti-6Al-4V10.1016/j.msea.2017.10.064 ↗
59. Effects of microstructure on fatigue crack propagation behavior in a bi-modal TC11 titanium alloy fabricated via laser additive manufacturing10.1016/j.jmst.2018.10.031 ↗
60. A Critical Analysis of Crack Propagation Laws10.1115/1.3656900 ↗
61. An investigation on fatigue and dwell-fatigue crack growth in Ti–6Al–2Sn–4Zr–2Mo–0.1Si10.1016/S0167-6636(03)00035-8 ↗
62. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗