journal article·2024-09

Influence of interface on microstructure and mechanical properties of laser-direct energy deposited Ti60 alloy

Jinhan Chen, Zhiqiang Li, Tinglian Zhang, Jin Min, Zhonggang Sun, Qi Liu, Huang Yuan, Wei Chen

Publisher page

Abstract

In this study, the laser-direct energy deposition (L-DED) was employed to fabricate Ti60 structures on the wrought Ti60 substrate. Detailed microstructure characterization and mechanical behavior investigation of the deposited material and substrate material were carried out. The parameter of the improved indentation inversion algorithm was optimized to obtain local elastoplastic properties of the interface between deposition and substrate. Quantitative analyses show that the interface exhibits improved mechanical properties compared to the wrought substrate. The theoretical strengthening models confirms that by introducing overall α texture and acicular α/α' in deposited zone and heat-affected zone, additional grain boundary strengthening is achieved by reducing the effective grain size, while simultaneously achieving additional dislocation strengthening when compared to the substrate zone. For the sample which has both deposited material and substrate, the yield and fracture stresses are determined by the strength of the wrought substrate. The over-matching between the deposited zone with higher strength and the substrate zone does not compromise the overall structural strength.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Cantor · 2001
2. High-temperature Titanium Alloys10.14429/dsj.55.1979 ↗
3. High Temperature Titanium Alloys: status and Perspective
4. Lütjering · 2007
5. Additive manufacturing: Laser metal deposition (LMD) and Selective laser melting (SLM) in turbo-engine applications10.1002/latj.201090029 ↗
6. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
7. Microstructure and mechanical properties of laser solid formed Ti60 alloy
8. Reclamation of titanium alloy based aerospace parts using laser based metal deposition methodology10.1016/j.matpr.2021.01.354 ↗
9. Repair and restoration of engineering components by laser directed energy deposition10.1016/j.matpr.2022.09.022 ↗
10. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
11. Heat-affected coarsening of β grain in titanium alloy during laser directed energy deposition10.1016/j.scriptamat.2021.114180 ↗
12. Critical review of the state of the art in multi-material fabrication via directed energy deposition10.1016/j.cossms.2021.100924 ↗
13. J.J. Lewandowski, M. Seifi, Metal Additive Manufacturing: A Review of Mechanical Properties, in: D.R. Clarke (Ed.), Annual Review of Materials Research, Vol 462016, pp. 151-186.10.1146/annurev-matsci-070115-032024 ↗
14. Microstructural and mechanical characterization of Ti6Al4V refurbished parts obtained by laser metal deposition10.1016/j.msea.2015.07.029 ↗
15. Analysis of microstructure and mechanical properties of additive repaired Ti–6Al–4V by Direct Energy Deposition10.1016/j.msea.2020.140604 ↗
16. TC17 titanium alloy laser melting deposition repair process and properties10.1016/j.optlastec.2016.02.013 ↗
17. Microstructures and mechanical properties of laser forming repair of TA19 titanium alloy
18. Researches of microstructure and mechanical properties on TC18 titanium alloy wrought billet repaired by laser additive manufacturing10.3788/AL20133305.0477 ↗
19. Study on microstructure and mechanical properties of laser solid repaired Ti60 alloy
20. Experimental Study on Laser Cladding and Shape-repair of Ti alloys
21. Research on laser deposition repair technology of titanium alloy blades
22. Influence of scanning path on residual stress and distortion of laser repairing titanium alloy
23. Research status and development trends of deformation control in laser cladding forming process
24. Progress in additive manufacturing, additive repair and fatigue evaluation of aviation titanium alloy blades10.1080/21663831.2023.2275599 ↗
25. Computational modeling of the forward and reverse problems in instrumented sharp indentation10.1016/S1359-6454(01)00295-6 ↗
26. Characterization of the recasting-affected zone in the nickel-based superalloy upon single-pulse laser treatment10.1016/j.msea.2021.141897 ↗
27. Microstructure and room-temperature tensile property of Ti-5.7Al-4.0Sn-3.5Zr-0.4Mo-0.4Si-0.4Nb-1.0Ta-0.05C with near equiaxed β grain fabricated by laser directed energy deposition technique10.1016/j.jmst.2021.03.012 ↗
28. Quantification of Alpha Lath in Ti-6Al-4V using OpenCV10.1016/j.matchar.2022.111802 ↗
29. Development of methods for the quantification of microstructural features in α+β-processed α/β titanium alloys10.1016/j.msea.2008.12.038 ↗
30. Effect of grain size on fracture behavior of pure magnesium sheet: an in-situ study combined with grain-scale DIC analysis10.1016/j.msea.2021.142396 ↗
31. Additive manufacturing: making imagination the major limitation10.1007/s11837-014-0886-2 ↗
32. Solidification behavior and grain morphology of laser additive manufacturing titanium alloys10.1016/j.jallcom.2018.11.055 ↗
33. Effect of energy density on the microstructure and texture evolution of Ti-6Al-4V manufactured by laser powder bed fusion10.1016/j.matchar.2020.110238 ↗
34. Microstructural modelling of above β-transus heat treatment of additively manufactured Ti-6Al-4V using cellular automata
35. Understanding the microstructure and mechanical properties of Ti-6Al-4V and Inconel 718 alloys manufactured by Laser Engineered Net Shaping
36. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
37. Effects of deposition strategies on macro/microstructure and mechanical properties of wire and arc additive manufactured Ti 6Al 4V10.1016/j.msea.2019.03.001 ↗
38. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
39. Tensile fracture of an adhesive joint: the role of crack length and of material mismatch10.1016/j.jmps.2019.06.004 ↗
40. The IBESS Approach for the Determination of the Fatigue Life and Strength of Weldments by Fracture Mechanics Analysis
41. Microstructural control during direct laser deposition of a β-titanium alloy10.1016/j.matdes.2015.05.031 ↗
42. In-situ grain structure control in directed energy deposition of Ti6Al4V
43. Microstructure and tensile properties of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.msea.2013.08.032 ↗
44. An overview of residual stresses in metal powder bed fusion
45. Electron backscattered diffraction to estimate residual stress levels of a superalloy produced by laser powder bed fusion and subsequent heat treatments10.3390/ma13204643 ↗
46. Microstructural characterization and fatigue performance of the recast material induced by laser manufacturing of a nickel-based superalloy10.1016/j.jmatprotec.2021.117087 ↗
47. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
48. Microstructure and mechanical properties of high temperature titanium alloy Ti60 at 600℃
49. Cyclic plasticity modeling and fatigue life assessment of the recasting material of a nickel-based superalloy induced by laser manufacturing10.1016/j.ijfatigue.2021.106154 ↗
50. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
51. Unique opportunities for microstructure engineering via trace B4C addition to Ti-6Al-4V through laser powder bed fusion process: as-built and heat-treated scenarios
52. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
53. Grain size and orientation distributions: application to yielding of α-titanium10.1016/j.actamat.2008.12.037 ↗
54. Oxygen effects on crystal plasticity of Titanium: a multiscale calibration and validation framework10.1016/j.actamat.2019.06.040 ↗
55. Modeling of discontinuous dynamic recrystallization of a near-α titanium alloy IMI834 during isothermal hot compression by combining a cellular automaton model with a crystal plasticity finite element method10.1016/j.commatsci.2013.08.004 ↗
56. Crystal plasticity modeling of the dynamic recrystallization of two-phase titanium alloys during isothermal processing10.1016/j.ijplas.2013.05.001 ↗
57. Micromechanical properties of single crystals and polycrystals of pure α-titanium: anisotropy of microhardness, size effect, effect of the temperature (77–300 K)
58. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
59. Mechanism-based strain gradient plasticity— I. Theory10.1016/S0022-5096(98)00103-3 ↗
60. Selective growth of low stored energy grains during δ Sub-solvus annealing in the Inconel 718 nickel-based superalloy10.1007/s11661-015-3035-9 ↗
61. Simultaneous strength and ductility enhancement of wire-arc directed energy deposited Al–Cu alloy by interlayer laser shock peening10.1016/j.msea.2023.145699 ↗
62. Effect of thermal exposure on microstructure and tensile properties of laser deposited Ti60A alloy10.1016/j.msea.2012.11.050 ↗
63. Chemical composition, microstructure, tensile and creep behavior of Ti60 alloy fabricated via electron beam directed energy deposition10.3390/ma15093109 ↗
64. Effect of aging on fatigue crack growth behavior of a high temperature titanium alloy10.2320/matertrans.45.1577 ↗