No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Additive Manufacturing Materials and Processes · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
2. Development and applications of aluminum alloys for aerospace industry10.1016/j.jmrt.2023.09.274 ↗
3. Costs, benefits, and adoption of additive manufacturing: a supply chain perspective10.1007/s00170-015-7973-6 ↗
4. A vision for sustainable additive manufacturing10.1038/s41893-024-01313-x ↗
5. Scientific, technological and economic issues in metal printing and their solutions10.1038/s41563-019-0408-2 ↗
6. Microstructure and mechanical properties of 2195 Al-Li alloy via friction stir additive manufacturing with different stirring paths10.1016/j.jallcom.2024.176666 ↗
7. Influence of argon, helium, and their mixtures on the powder bed fusion of an Al–Cu–Li–Ti alloy using a laser beam: evaporation, microstructure, and mechanical properties
8. Achieving fully equiaxed grains with minor Sc addition of a novel Al-Li alloy fabricated by laser direct energy deposition10.1016/j.matlet.2024.136780 ↗
9. Wire arc additive manufacturing (WAAM) for aluminum-lithium alloys: a review10.3390/ma16041375 ↗
10. Progress in metal additive manufacturing using innovative solid-state friction stir-based techniques10.1016/j.jallcom.2024.177395 ↗
11. Local microstructure evolution and mechanical performance of friction stir additive manufactured 2195 Al-Li alloy10.1016/j.matchar.2022.111818 ↗
12. Problems and issues in laser beam welding of aluminum–lithium alloys10.1016/j.jmapro.2013.10.005 ↗
13. A review of laser additive manufacturing (LAM) aluminum alloys: methods, microstructures and mechanical properties10.1016/j.optlastec.2024.110722 ↗
14. Microstructural evolution and mechanical properties of 2195 Al-Li alloy processed by rapid solidification and thermo-mechanical processing10.1016/j.jallcom.2023.169794 ↗
15. Heat sources in wire arc additive manufacturing and their impact on macro-microstructural characteristics and mechanical properties – an overview
16. Challenges and developments in wire arc additive manufacturing of steel: a review10.1016/j.rineng.2025.104657 ↗
17. Improving mechanical properties of wire arc additively manufactured AA2196 Al–Li alloy by controlling solidification defects
18. Porosity in wire-arc directed energy deposition of aluminum alloys: formation mechanisms, influencing factors and inhibition strategies
19. Effects of Li content on microstructure evolution and mechanical properties of squeeze-cast Al-5Cu-xLi alloy assisted with ultrasonic treatment10.1016/j.jallcom.2023.171083 ↗
20. Grushko · 2016
21. Effect and mechanism of Li content on the corrosion resistance of Al-Li alloy10.1016/j.corsci.2025.112768 ↗
22. Additive manufacturability of nickel-based superalloys: composition-process induced vapourization
23. In-process spectroscopic detection of chromium loss during Directed Energy Deposition of alloy 71810.1016/j.matdes.2019.108317 ↗
24. Fabrication of high-strength Mg-Gd-Zn-Zr alloy via selective laser melting10.1016/j.matchar.2020.110377 ↗
25. Analysis of element loss, densification, and defects in laser-based powder-bed fusion of magnesium alloy WE4310.1016/j.jma.2022.02.011 ↗
26. Loss of elemental Mg during wire + arc additive manufacturing of Al-Mg alloy and its effect on mechanical properties10.1016/j.jmapro.2019.10.033 ↗
27. Effect of compositional changes on microstructure in additively manufactured aluminum alloy 213910.1016/j.matchar.2018.04.002 ↗
28. A novel bypass-gas metal arc directed energy deposition for in-situ synthesis Al–Cu–Li alloy: exploring the microstructure and mechanical properties evolution from as-deposited state to T6 state10.1080/17452759.2025.2472394 ↗
29. Effect of precipitates on mechanical properties of AA219510.1016/j.jallcom.2016.01.229 ↗
30. Microstructures and cryogenic mechanical properties of spray deposited 2195 Al–Cu–Li alloy with different heat treatments10.1016/j.msea.2024.146173 ↗
31. Study on microstructure evolution and aging precipitation behavior of a novel Al-Li alloy fabricated by laser rapid melting10.1016/j.jallcom.2022.164630 ↗
32. Precipitation behavior of an Al–Cu–Li–X alloy and competing relationships among precipitates at different aging temperatures10.1016/j.msea.2021.141125 ↗
33. The effects of process parameters on melt-pool oscillatory behaviour in gas tungsten arc welding10.1088/1361-6463/abf808 ↗
34. Distribution of the heat and current fluxes in gas tungsten arcs10.1007/BF02667521 ↗
35. Heat and fluid flow in pulsed current GTA weld pool10.1016/S0017-9310(98)00052-0 ↗
36. Metal vaporization from weld pools10.1007/BF02657376 ↗
37. Effect of characteristic substrate parameters on the deposition geometry of CMT additive manufactured Al-6.3%Cu alloy10.1016/j.applthermaleng.2019.114302 ↗
38. Modelling of wire-arc additive manufacturing – a review
39. Control of grain structure, phases, and defects in additive manufacturing of high-performance metallic components10.1016/j.pmatsci.2023.101153 ↗
40. Effect of precipitates on mechanical properties of AA219510.1016/j.jallcom.2016.01.229 ↗
41. Precipitation behavior of an Al–Cu–Li–X alloy and competing relationships among precipitates at different aging temperatures10.1016/j.msea.2021.141125 ↗
42. A novel high-strength Al–Li alloy printed by laser powder bed fusion: microstructural evolution and strengthening mechanism10.1016/j.jmrt.2024.05.062 ↗
43. Dislocation-induced precipitation and its strengthening of Al–Cu–Li–Mg alloys with high Mg10.1007/s40195-020-01166-1 ↗
44. Pore formation and evolution in wire + arc additively manufactured 2319 Al alloy
45. Statistical analysis of spatial distribution of pores in metal additive manufacturing
46. Melting and casting of aluminum–lithium alloys
47. Hot cracking evolution and formation mechanism in 2195 Al-Li alloy printed by laser powder bed fusion
48. Achieving high strength-ductility of Al-Zn-Mg-Cu alloys via hot-wire arc additive manufacturing enabled by strengthening precipitates
49. Additive manufacturing of Ti-6Al-4V with laser-wire DED and local shielding gas protection10.1016/j.procir.2024.08.111 ↗
50. Porosity evolution mechanisms, influencing factors, and ultrasonic-assisted regulation in joining high Mg-content aluminum alloys10.1016/j.jmatprotec.2024.118706 ↗
51. Review on field assisted metal additive manufacturing10.1016/j.ijmachtools.2023.104032 ↗
52. Hot-wire arc additive manufacturing of aluminum alloy with reduced porosity and high deposition rate10.1016/j.matdes.2020.109370 ↗
53. Improved properties of wire arc directed energy deposited thin-walled Al-6Mg-0.3Sc component via laser shock peening10.1080/17452759.2024.2370956 ↗
54. Wire-arc directed energy deposited high-performance AZ31 magnesium alloy via a novel interlayer hammering treatment10.1016/j.msea.2023.145864 ↗
55. Strain-dependent heterogeneity of microstructure and mechanical properties of 2195 Al–Li alloy during power spinning and heat treatment10.1016/j.msea.2024.146689 ↗
56. Dynamic recrystallization and crystal phase evolution and its influence on static recrystallization and three-dimensional mechanical properties of the multi-directionally forged 2195 Al-Li alloy10.1016/j.msea.2024.147707 ↗
57. Effect of heat treatment on the microstructure and mechanical properties of cryogenic rolling 2195 Al–Cu–Li alloy10.1016/j.msea.2021.141682 ↗
58. Microstructure and mechanical properties of wire + arc additively manufactured 2050 Al–Li alloy wall deposits10.1186/s10033-019-0405-z ↗
59. Quantify strengthening and weakening factors in molybdenum fabricated by laser powder bed fusion (LPBF) with a revisit of its oxygen sensitivity10.1016/j.msea.2025.147856 ↗
60. Wire-arc directed energy deposition of aluminum alloy 7075 with dispersed nanoparticles10.1115/1.4056257 ↗