The Mechanism of Si Incorporation and the Digital Control of Si Content during the Metallorganic Atomic Layer Deposition of Ti-Si-N Thin Films
Source abstract
Abstract
Titanium‐silicon‐nitride thin films were grown by metallorganic atomic layer deposition (MOALD) using tetrakis(dimethylamido)titanium (TDMAT), ammonia, and silane at 180°C. When the reactants are injected into the reactor in the sequence ofTDMAT pulse, pulse, and pulse, the Si content in the Ti‐Si‐N films is saturated at 18 atom %. By changing the supplying sequence in the order of TDMAT, , and , the Si content is increased to 21 atom %. The Si content in the films is almost insensitive to the partial pressure over a wide range of 0.27 and 13.3 Pa, because it is self‐limited by the quantity of molecules absorbed on the film surface. By utilizing these inherent characteristics of MOALD, digital control of Si content in Ti‐Si‐N thin film is possible by controlling the number of pulses during film deposition. The MOALD Ti‐Si‐N films have almost 100% step coverage on a 0.3 μm diam hole with an aspect ratio of 10:1. MOALD is considered to be a promising deposition method for less than 10 nm thick Ti‐Si‐N films as a Cu diffusion barrier film. © 2000 The Electrochemical Society. All rights reserved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.