Ball-milled elemental Co, Ni, Al, and W powders were used to fabricate a Co-0.20Ni-0.11Al-0.08W (mole fraction) alloy via laser powder bed fusion (L-PBF). In the as-fused state, microstructural features present within the FCC-γ Co-Ni-Al-W matrix – partially-melted W powders, W-deficient regions, and cracks – are investigated with respect to the laser scanning speed. Tungsten particles appear to block or deflect internal cracks, thus improving cracking resistance due to thermal cycling during laser fusion. However, W-deficient regions, which are also enriched with Ni and Al, can act as crack nucleation sites due to the brittleness of the β-NiAl and eutectic microconstituents. A homogenous FCC-γ Co-0.20Ni-0.11Al-0.08 W (mole fraction) solid solution is obtained after a solutionizing treatment at 1200 °C, as W-rich particles fully dissolve, and W-deficient regions homogenize, into the matrix. A γ/γ′-two-phase microstructure forms upon subsequent aging at 900 °C, whose creep resistance is measured at 850 °C: below 300 MPa, deformation is dominated by diffusional creep (consistent with a relatively fine grain size of 50–100 µm) while above 300 MPa, it is controlled by dislocation creep. Using elemental powder blends is a viable method to create microstructurally-sound, creep-resistant Co-based γ/γ′ superalloys via L-PBF.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. L12-strengthened Cobalt-base superalloys10.1146/annurev-matsci-070214-021043 ↗
2. Deformation behavior and creep properties of Co-Al-W-based superalloys: A review10.1016/j.pnsc.2021.09.009 ↗
3. Low-density, high-temperature Co base superalloys10.1146/annurev-matsci-080619-014459 ↗
4. Lee · 1971
5. Cobalt-base high-temperature alloys10.1126/science.1121738 ↗
6. The importance of sign and magnitude of γ/γ’ lattice misfit in superalloys - with special reference to the new γ’-hardened cobalt-base superalloys10.1016/j.actamat.2014.08.005 ↗
7. Experimental investigation and thermodynamic modeling of the Co-rich region in the Co-Al-Ni-W quaternary system10.1007/s11669-014-0327-5 ↗
8. Coarsening behaviour and interfacial structure of γ′ precipitates in Co-Al-W based superalloys10.1016/j.actamat.2016.08.023 ↗
9. Alloying effects in polycrystalline γ’ strengthened Co-Al-W base alloys10.1016/j.intermet.2013.10.022 ↗
10. Application of computational thermodynamics to the design of a Co-Ni-Based γ′-strengthened superalloy10.1007/s11661-017-4040-y ↗
11. Evolution of Y2O3 dispersoids during laser powder bed fusion of oxide dispersion strengthened Ni-Cr-Al-Ti γ/γ’ superalloy
12. Fatigue strength of additive manufactured Mar-M-509 superalloy10.1016/j.msea.2022.142913 ↗
13. Directed energy deposition of γ/γ’ Co-Al-W superalloys
14. In-situ alloying in laser-based additive manufacturing processes: a critical review10.1016/j.jallcom.2021.159567 ↗
15. Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy
16. Effect of Y2O3 dispersoids on microstructure and creep properties of Hastelloy X processed by laser powder-bed fusion
17. Effect of minor alloying elements on crack-formation characteristics of Hastelloy-X manufactured by selective laser melting
18. In‐situ alloyed medium entropy alloy fabricated by laser powder bed fusion: microstructure and cryogenic performance10.1002/adem.202200900 ↗
19. In-situ alloyed CoCrFeMnNi high entropy alloy: Microstructural development in laser powder bed fusion10.1016/j.jmst.2021.11.083 ↗
20. Evaluation of in-situ alloyed Inconel 625 from elemental powders by laser directed energy deposition10.1016/j.msea.2021.142296 ↗
21. Formation mechanism and thermal stability of γ’ and γ" compact co-precipitated nanostructure in directed energy deposited Ni-based slloy10.1016/j.matchar.2022.112450 ↗
22. Hierarchical microstructure and enhanced mechanical properties of SLM-fabricated GH5188 Co-superalloy10.1016/j.msea.2021.142276 ↗
23. Effects of build orientation and heat treatment on the evolution of microstructure and mechanical properties of alloy Mar-M-509 fabricated via laser powder bed fusion10.1016/j.ijplas.2019.06.002 ↗
24. A defect-resistant Co–Ni superalloy for 3D printing10.1038/s41467-020-18775-0 ↗
25. Chemically driven growth of tungsten grains during sintering in liquid nickel10.1016/0001-6160(79)90185-8 ↗
26. Processing and microstructural characterization of liquid phase sintered tungsten-nickel-cobalt heavy alloys10.1016/j.ijrmhm.2014.12.009 ↗
27. Thermodynamic re-assessment of the Al-Co-W system10.1016/j.calphad.2017.09.007 ↗
28. Development of a diffusion mobility database for Co-based superalloys
29. Grain structure control of additively manufactured metallic materials10.3390/ma10111260 ↗
30. High temperature tensile properties of a series of nickel-base superalloys on a γ/γ′ tie line10.1016/S0921-5093(96)10504-9 ↗
31. Creep strength of Ni-base single-crystal superalloys on the γ/γ’ Tie-Line10.7449/2004/Superalloys_2004_155_162 ↗
32. Quaternary alloying effects and the prospects for a new generation of Co-base superalloys
33. Phase equilibria and microstructure on γ′ phase in Co-Ni-Al-W system10.2320/matertrans.MER2008073 ↗
34. Phase equilibria in the Al-Co-Ni alloy system10.1007/s11669-017-0586-z ↗
35. Additive manufacturing of high-strength crack-free Ni-based Hastelloy X superalloy
36. A microstructure-based creep model for additively manufactured nickel-based superalloys10.1016/j.actamat.2021.117528 ↗
37. Micro-cracking, microstructure and mechanical properties of Hastelloy-X alloy printed by laser powder bed fusion: as-built, annealed and hot-isostatic pressed
38. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
39. Compressive properties of zone-directionally solidified β-NiAl and its off-eutectic alloys with chromium and tungsten10.1016/S0921-5093(01)01919-0 ↗
40. Mechanical properties of extruded dual-phase NiAl Alloys10.1007/BF01154496 ↗
41. On the toughening of intermetallics with ductile fibers: Role of interfaces10.1016/0956-7151(91)90010-X ↗
42. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
43. Laser powder bed fabrication of nickel-base superalloys: Influence of parameters; characterisation, quantification and mitigation of cracking10.1002/9781118516430.ch64 ↗
44. Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing10.1016/j.matdes.2018.10.042 ↗
45. The Al-Co (Aluminum-Cobalt) system10.1007/BF02877635 ↗
46. Effect of Cr content on interdiffusion and Kirkendall pore formation during homogenization of pack-aluminized Ni and Ni-Cr wires10.1016/j.intermet.2018.07.007 ↗
47. Microstructure development during pack aluminization of nickel and nickel-chromium wires10.1016/j.intermet.2014.02.009 ↗
48. A novel crack healing technique in a low carbon steel by cyclic phase transformation heat treatment: The process and mechanism10.1016/j.msea.2019.138712 ↗
49. Morphology evolution and mechanisms of crack healing in a low-carbon steel during isothermal heat treatment10.1007/s11661-021-06284-8 ↗
50. Effect of deformation modes and heat treatment on microstructure and impact property restoration of internal crack healing in SA 508 steel10.1016/j.msea.2020.139073 ↗
51. Microstructure and mechanical properties of internal crack healing in a low carbon steel10.1016/j.msea.2016.03.045 ↗
52. Strain/Oxidation Interactions in Steels and Model Alloys10.1002/maco.19720231003 ↗
53. Creep in mechanically alloyed NiAl10.1016/0921-5093(94)03289-0 ↗
54. Fatigue crack closure: From LCF to small scale yielding10.1016/j.ijfatigue.2012.02.016 ↗
55. Microstructural evolution and high-temperature strength of a γ(f.c.c.)/γ’(L12) Co–Al–W–Ti–B superalloy10.1016/j.actamat.2019.05.058 ↗
56. Creep properties of different γ’-strengthened Co-base superalloys10.1016/j.msea.2012.04.083 ↗
57. Exploring the correlation between microscopic mechanisms and macroscopic behaviour in creep of a directionally solidified tungsten-free γ/γ′ CoNi-base superalloy10.1016/j.actamat.2022.117738 ↗
58. Peter · 2015
59. Controlling crack formation and porosity in laser powder bed fusion: Alloy design and process optimisation
60. Pure molybdenum manufactured by laser powder bed fusion: thermal and mechanical characterization at room and high temperature
61. Printability assessment with porosity and solidification cracking susceptibilities for a high strength aluminum alloy during laser powder bed fusion
62. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
63. Solving the problem of solidification cracking during additive manufacturing of CrMnFeCoNi high-entropy alloys through addition of Cr3C2 particles to enhance microstructure and properties
64. The fracture resistance of directionally solidified dual-phase NiAl reinforced with refractory metals10.1016/0956-7151(93)90079-8 ↗
65. A survey of toughness in ductile phase composites10.1016/0956-716X(92)90654-W ↗
66. The mechanics of crack growth in layered materials10.1016/0956-7151(93)90171-N ↗
67. Yielding and fracture in tungsten and tungsten-rhenium alloys10.1016/0022-5088(69)90047-2 ↗