journal article·2021-10

Experimental investigation on shear strength of laser powder bed fusion AlSi10Mg under quasi-static and dynamic loads

Ben Amir, Eytan Kochavi, Shimon Gruntman, Yuval Gale, Shmuel Samuha, Oren Sadot

Publisher page

Abstract

Abstract This study deals with additive manufacturing (AM) products. Employing AM technology, complex-shaped, and lightweight parts can be fabricated using the aluminum alloy, AlSi10Mg. Typically, AM of this alloy is performed by laser powder bed fusion (LPBF). The mechanical properties of LPBF products are crucial for many engineering applications. Therefore, there have been efforts to measure the dynamic and quasi-static properties of such products. However, both the dynamic and quasi-static shear behaviors of this alloy are yet to be investigated. The present study is focused on experimentally investigating the shear behavior of LPBF AlSi10Mg. ‏Quasi-static shear tests were performed according to the ASTM B565 protocol, whereas dynamic shear tests were conducted using a standard split Hopkinson pressure bar equipped with an innovative sample holder that generates pure shear in a sample. The results of the performed tests showed that as the shear load rate increased, the shear strength considerably increased. In addition, in the quasi-static regime, the shear strength was practically independent of the product build direction. In contrast, under the dynamic shear conditions, samples built horizontally failed at a shear strength approximately 10% lower than that of those manufactured vertically. To investigate the build orientation effect on the shear behavior, this study conducted extensive microstructural characterization along with fracture analysis. Crack nucleation and propagation were analyzed in view of the effects of the unique microstructural characteristics of the LPBF AlSi10Mg, including the morphologies of the melt pool boundaries. The results obtained in this study suggested that for engineering applications in which dynamic loads are expected, the build orientation of AlSi10Mg parts produced using LPBF technology must be considered.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. High power selective laser melting (HP SLM) of aluminum parts10.1016/j.phpro.2011.03.035 ↗
3. Contribution of microstructural parameters to strengthening in an ultrafine-grained Al–7% Si alloy processed by severe deformation10.1016/j.actamat.2006.09.037 ↗
4. Effect of solution heat treatment and additives on the microstructure of Al-Si (A413.1) automotive alloys10.1023/A:1027333602276 ↗
5. Influence of selective laser melting machine source on the dynamic properties of AlSi10Mg Alloy10.3390/ma12071143 ↗
6. Split Hopkinson pressure bar tests for investigating dynamic properties of additively manufactured AlSi10Mg alloy by selective laser melting
7. On the precipitation hardening of selective laser melted AlSi10Mg10.1007/s11661-015-2980-7 ↗
8. The AlSi10Mg samples produced by selective laser melting: single track, densification, microstructure and mechanical behavior10.1016/j.apsusc.2017.02.215 ↗
9. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
10. Microstructure and mechanical properties of AlSi10Mg parts produced by the laser beam additive manufacturing (AM) technology10.1007/s13632-014-0168-y ↗
11. Selective laser melting of AlSi10Mg: influence of post-processing on the microstructural and tensile properties development10.1016/j.matdes.2016.05.066 ↗
12. Selective laser melting of aluminum die-cast alloy—correlations between process parameters, solidification conditions, and resulting mechanical properties10.2351/1.4906389 ↗
13. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
14. Texture, anisotropy in microstructure and mechanical properties of IN738LC alloy processed by selective laser melting (SLM)10.1016/j.msea.2014.10.003 ↗
15. Influence of process parameters on surface roughness of aluminum parts produced by DMLS10.1007/s00170-012-4688-9 ↗
16. Processing AlSi10Mg by selective laser melting: parameter optimisation and material characterisation10.1179/1743284714Y.0000000702 ↗
17. Selective laser melting of AlSi10Mg alloy: process optimisation and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
18. Porosity formation mechanisms and fatigue response in Al-Si-Mg alloys made by selective laser melting10.1016/j.msea.2017.11.078 ↗
19. The effect of selective laser melting process parameters on the microstructure and mechanical properties of Al6061 and AlSi10Mg alloys
20. Effect of selective laser melting process parameters on the quality of Al alloy parts: powder characterization, density, surface roughness, and dimensional accuracy10.3390/ma11122343 ↗
21. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting
22. Influence of sub-cell structure on the mechanical properties of AlSi10Mg manufactured by laser powder bed fusion
23. [dataset] SLM Solutions, Material data sheet Al-Alloy AISi10Mg, SLM Solutions Group AG, 2019. 〈https://www.slm-solutions.com/fileadmin/Content/Powder/MDS/MDS_Al-Alloy_AlSi10Mg_0221.pdf〉.
24. [dataset] EOS GmbH - Electro Optical Systems, Material data sheet: EOS aluminium AlSi10Mg,[Online], 2014. 〈https://www.eos.info/material-m〉, 〈https://www.eos.info/03_system-related-assets/material-related-contents/metal-materials-and-examples/metal-material-datasheet/aluminium/material_datasheet_eos_aluminium-alsi10mg_en_web.pdf〉.
25. [dataset] Concept Laser, Cl 30Al / Cl 31Al, 2015. 〈https://www.ge.com/additive/sites/default/files/2018–12/CLMAT_30_31AL_DS_EN_US_2_v1.pdf〉.
26. Strength of welded aluminum columns10.1061/JSDEAG.0000553 ↗
27. 2003
28. 2012
29. Kaufman · 2000 · 14
30. Application of modern aluminum alloys to aircraft10.1016/0376-0421(95)00004-6 ↗
31. Additive manufactured A357.0 samples using the laser powder bed fusion technique: shear and tensile performance10.3390/met8090670 ↗
32. Dynamic response of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.msea.2017.02.004 ↗
33. High strain rate behaviour at high temperature of AlSi12 parts produced by selective laser melting
34. On dynamic mechanical behavior of additively manufactured AlSi10Mg_200C10.1016/j.matlet.2017.10.001 ↗
35. Effect of build orientation on the quasi-static and dynamic response of SLM AlSi10Mg10.1016/j.msea.2020.139445 ↗
36. Dynamic shear deformation and failure of Ti-6Al-4V and Ti-5Al-5Mo-5V–1Cr-1Fe alloys
37. Novel technique for static and dynamic shear testing of Ti6Al4V sheet10.1007/s11340-011-9541-9 ↗
38. Dynamic shear characteristics of titanium alloy Ti-6Al-4V at large strain rates by the split Hopkinson pressure bar test10.1016/j.ijimpeng.2017.06.007 ↗
39. Modification of the shear-compression specimen for large strain testing10.1007/s11340-015-0057-6 ↗
40. A shear compression disk specimen with controlled stress triaxiality under dynamic loading10.1007/s11340-012-9630-4 ↗
41. A critical analysis of plane shear tests under quasi-static and impact loading10.1016/j.ijimpeng.2014.06.012 ↗
42. Dynamic punch testing of 2024-T351 aluminum
43. Mechanical properties of SLM-printed aluminium alloys: a review10.3390/ma13194301 ↗
44. ASTM, B565 – 04, 2015.
45. The study of adiabatic shear band instability in a pearlitic 4340 steel using a dynamic punch test10.1007/BF02648867 ↗
46. LS-DYNA R11, LIvermore Software Technology Corporation (LSTC), Livermore, California.
47. W.H. Johnson, G.R.; Cook, A constitutive model and data for metals subjected to large strains, high strain rates and high, in: Proceedings of the Seventh Int. Symp. Ballist., vol. retrieved, no. May, 541–547, 1983.
48. Fracture characteristics of three metals subjected to various strains, strain rates, temperatures and pressures10.1016/0013-7944(85)90052-9 ↗
49. R.R. Nirmal, B.S. V. Patnaik, R. Jayaganthan, Numerical Simulation on Deformation Behaviour of Additively Manufactured AlSi10Mg Alloy, 2, (10), 445–450, 2020.
50. Numerical and experimental investigation of Johnson–Cook material models for aluminum (Al 6061-T6) alloy using orthogonal machining approach10.1177/1687814018797794 ↗
51. Dynamic shear strength of SiC whisker reinforced aluminum alloy composites
52. Properties and Selection: Nonferrous Alloys andSpecial-Purpose Materials, ASM International, 1990.
53. Archimedes’ principle revisited10.4236/jamp.2017.54073 ↗
54. Influences of platform heating and post-processing stress relief treatment on the mechanical properties and microstructure of selective-laser-melted AlSi10Mg alloys10.1016/j.msea.2021.141612 ↗
55. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: comparison between virgin and recycled powders
56. Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by selective laser melting10.1016/j.msea.2016.11.070 ↗
57. K. Qin, L.M. Yang, S. Hu, Interpretation of strain rate effect of metals, in: Proceedings of the Conference of the Society for Experimental Mechanics Series, 1, 2014, 21–27.10.1007/978-3-319-00771-7_3 ↗
58. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
59. Direction and location dependency of selective laser melted AlSi10Mg specimens10.1016/j.jmatprotec.2016.11.029 ↗
60. Microstructure and mechanical properties of Al-12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
61. Effect of molten pool boundaries on the mechanical properties of selective laser melting parts10.1016/j.jmatprotec.2014.06.002 ↗
62. Delamination Toughening of ultrafine grain structure steels processed through tempforming at elevated temperatures10.2355/isijinternational.50.152 ↗
63. Mechanisms influencing the cryogenic fracture-toughness behavior of aluminum-lithium alloys10.1016/0956-7151(90)90098-2 ↗
64. Delamination cracking in advanced aluminum–lithium alloys – experimental and computational studies10.1016/j.engfracmech.2009.06.010 ↗
65. High temperature fracture characteristics of a nanostructured ferritic alloy (NFA)10.1016/j.jnucmat.2010.09.031 ↗
66. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting10.1016/j.actamat.2016.06.009 ↗