This study investigates the properties of fluorosilicate glass film prepared by temperature‐difference‐based liquid‐phase deposition. Experimental results indicate that the deposition temperature can significantly affect the deposition rate and film properties. As the deposition temperature increases from 15 to 35°C, the deposition rate increases exponentially from 30 to 687 Å/h. Meanwhile, the F and OH contents increase from 2.56 to 3.49% and from 0.16 to 0.5%, respectively. The dielectric constants and stresses for the films deposited at 15, 25, and 35°C, are 3.56/63 MPa, 3.46/43 MPa, and 3.66/73 MPa, respectively. The current densities at 20 MV/cm for the films deposited at 15, 25, and 35°C are , , and , respectively. For the film deposited at 25°C, the dielectric constant and the stress are minimal because of the high F content, low OH content, and low bond strain. The properties are also compared with those of fluorosilicate glass prepared by plasma‐enhanced chemical vapor deposition. In addition to exhibiting a lower dielectric constant and much better resistance to moisture, the film prepared by temperature‐difference‐based liquid‐phase deposition also shows a comparable or better insulating property, revealing a reliable intermetal dielectric with a low dielectric constant. © 2000 The Electrochemical Society. All rights reserved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Copper Interconnects and Reliability · Advanced ceramic materials synthesis · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.