The ageing response of direct laser deposited metastable β-Ti alloy, Ti–5Al–5Mo–5V–3Cr
Source abstract
Abstract
Abstract The formation of solely β-phase titanium after direct laser deposition (DLD) of metastable β-Ti alloy does not provide the desired properties. Hence, we present a study into the ageing response of DLD built Ti-5553 β-Ti alloy to obtain the bimodal (β + α) microstructure providing improved properties. The results obtained from the heat treatments showed that a unique microstructure with refined intragranular and discontinuous grain boundary α-phase can be obtained by directly ageing (using fast heating rate) the as-built samples at the ageing condition (600 °C + 0.5 h). This microstructure produced a good balance in mechanical properties (UTS = 1345 ± 5 MPa and δ = 11.6 ± 0.5%). The interparticle spacing between the α-phase ( d ) showed a correlation with microhardness ( H v = 340 + 158 / √ d ) and yield stress ( σ 0.2 = 870 + 15086 / √ d ) values for all the aged samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Influence of duplex ageing on secondary α precipitates and mechanical properties of the near β -Ti alloy Ti-5553110.1016/j.matchar.2018.06.025 ↗
2. The dependence of isothermal ω precipitation on the quenching rate in a metastable β-Ti alloy10.1038/srep14632 ↗
3. A. Settefrati, M. Dehmas, G. Geandier, B. Denand, E. Aeby-Gautier, B. Appolaire, G. Khelifati, J. Delfosse, Precipitation sequences in beta metastable phase of Ti-5553 alloy during ageing, Proc. 12th World Conf. Titan., 2011, pp. 468–472.
4. Effect of solution treatment and aging on microstructure and tensile properties of high strength β titanium alloy, Ti–5Al–5V–5Mo–3Cr10.1016/j.matdes.2014.04.015 ↗
5. Development of α precipitates in metastable Ti-5Al-5Mo-5V–3Cr and similar alloys10.1016/j.matchar.2016.09.005 ↗
6. Development of a pre-heat treatment for obtaining discontinuous grain boundary α in laser melting deposited Ti-5Al-5Mo-5V–1Cr-1Fe alloy10.1016/j.msea.2014.03.028 ↗
7. Role of ω phase in the formation of extremely refined intragranular α precipitates in metastable β-titanium alloys10.1016/j.actamat.2015.11.020 ↗
8. Novel mixed-mode phase transition involving a composition-dependent displacive component10.1103/PhysRevLett.106.245701 ↗
9. Influence of cooling rate on the precipitation kinetics of nanoscale isothermal ω-phase in metastable β-Ti alloy, Ti–5Al–5Mo–5V–3Cr10.1016/j.jallcom.2020.157822 ↗
10. Additive manufacturing and postprocessing of Ti-6Al-4V for superior mechanical properties10.1557/mrs.2016.215 ↗
11. An overview of direct laser deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control
12. Microstructure and mechanical properties of the near-beta titanium alloy Ti-5553 processed by selective laser melting10.1016/j.matdes.2016.04.103 ↗
13. Processing of Ti-5553 with improved mechanical properties via an in-situ heat treatment combining selective laser melting and substrate plate heating10.1016/j.matdes.2017.05.010 ↗
14. Evolution of microstructure and mechanical properties of selective laser melted Ti-5Al-5V–5Mo-3Cr after heat treatments10.1080/13621718.2019.1594589 ↗
15. Influence of continuous grain boundary α on ductility of laser melting deposited titanium alloys10.1016/j.msea.2016.03.034 ↗
16. A critical evaluation of the microstructural gradient along the build direction in electron beam melted Ti-6Al-4V alloy10.1016/j.msea.2018.12.016 ↗
17. Precipitation processes in the beta-titanium alloy Ti-5Al-5Mo-5V–3Cr10.1016/j.jallcom.2015.05.251 ↗
18. Nanoprecipitation in a beta-titanium alloy10.1016/j.jallcom.2014.10.038 ↗
19. Evolution of secondary α phase during aging treatment in novel near Ti-6Mo-5V–3Al-2Fe alloy10.3390/ma11112283 ↗
20. Microstructures and mechanical properties of Ti-5553 alloy processed by high-pressure torsion10.1088/1757-899X/63/1/012069 ↗
21. Hardness-strength relationships in fine and ultra-fine grained metals processed through constrained groove pressing10.1016/j.msea.2015.03.122 ↗
22. Microstructural evolution and mechanical properties of Ti–5Al–5Mo–5V–3Cr alloy by heat treatment with continuous temperature gradient10.1016/S1003-6326(18)64660-6 ↗
23. Porter · 1992
24. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
25. Hardened austenite steel with columnar sub-grain structure formed by laser melting10.1016/j.msea.2014.12.018 ↗
26. Residual stress analysis of additive manufacturing of metallic parts using ultrasonic waves: State of the art review
27. Effect of heat treatment on dislocation states and work hardening behaviors of SiCw/6061Al composite10.1016/S0167-577X(02)00568-2 ↗
28. Hardness characteristic and shear band formation in metastable β-titanium alloys10.1016/j.matchar.2014.07.027 ↗
29. Relationship between microstructure and tensile properties on a near-β titanium alloy after multidirectional forging and heat treatment10.1007/s12598-018-1159-y ↗
30. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength10.1016/j.scriptamat.2018.05.040 ↗
31. Relationship between fatigue limit and Vickers hardness in steels10.1016/j.msea.2011.01.040 ↗
32. Analysis of hardness – tensile strength relationships for electroformed nanocrystalline materials10.1016/j.msea.2008.02.015 ↗