journal article·2023-07

Influence of layer thickness on the printability of nickel alloy 718:A systematic process optimization framework

David Shoukr, Peter Morcos, Tayler Sundermann, Thomas Dobrowolski, Chad Yates, Jayesh R. Jain, Raymundo Arróyave, Ibrahim Karaman, Alaa Elwany

Publisher page

Abstract

Laser-powder bed fusion (L-PBF) is a metal additive manufacturing (AM) process involving layer-by-layer metal parts fabrication. It has been successfully used in the literature to manufacture nickel alloy 718 parts. However, the process parameter selection has generally been based on either intensive experimental methods or expensive computational simulations. As such, these methods test a limited region of the parameter space. Thus, hindering the evaluation of possible parameter combinations that can prove superior to those in the tested space. Moreover, most of the previous studies combine the process parameters into single metrics, e.g., linear energy density (LED) or volumetric energy density (VED). Both metrics have been shown in the literature to provide an incomplete understanding of the produced parts and inconsistent mechanical properties and microstructures. This paper uses a systematic framework developed by the authors that covers the entire scanning speed-laser power (v-P) parameter space, estimates the maximum hatch spacing at each v-P combination, and detects the good printability region. This framework defines the good printability region as the region that is free of the main possible porosity defects, namely, lack of fusion, keyholing, and balling. Furthermore, to cover the effect of the fourth process parameter (layer thickness), the framework is applied to 60 and 90 μ m layer thicknesses. This extension of the framework is performed to test the possibility of increasing the volumetric build rate (VBR) by increasing the layer thickness. Finally, the printability is validated using density and porosity measurements, while performance is evaluated using tensile tests. Using the framework, parts with 99.99% densification were fabricated successfully for both layer thicknesses. Moreover, tensile strength values of 1059.1 and 1063.5 MPa and volumetric build rates of 7.10 and 6.92 mm 3 /s were achieved for the as-printed parts for the 60 and 90 μ m layer thicknesses, respectively. However, these VBR values are constrained by the conservative hatch spacing criterion used in the framework. Further optimization of the hatch spacing can provide higher VBR values for the 90 μ m layer thickness.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Manufacturing Process and Optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Processing parameters in laser powder bed fusion metal additive manufacturing10.1016/j.matdes.2020.108762 ↗
4. Effects of processing parameters on consolidation and microstructure of W-Cu components by DMLS10.1016/j.jallcom.2008.05.065 ↗
5. Optimizing quality of additively manufactured Inconel 718 using powder bed laser melting process
6. Selective laser melting additive manufacturing of Inconel 718 superalloy parts: Densification, microstructure and properties10.1016/j.jallcom.2013.09.171 ↗
7. Porosity evolution and its thermodynamic mechanism of randomly packed powder-bed during selective laser melting of Inconel 718 alloy10.1016/j.ijmachtools.2017.01.005 ↗
8. Effect of energy input on microstructural evolution of direct laser fabricated IN718 alloy10.1016/j.matchar.2015.06.027 ↗
9. Is the energy density a reliable parameter for materials synthesis by selective laser melting?10.1080/21663831.2017.1299808 ↗
10. An ultra-high strength martensitic steel fabricated using selective laser melting additive manufacturing: Densification, microstructure, and mechanical properties10.1016/j.actamat.2019.12.037 ↗
11. Effects of laser sintering processing parameters on the microstructure and densification of Iron powder10.1016/S0921-5093(03)00341-1 ↗
12. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
13. Effects of selective laser melting additive manufacturing parameters of Inconel 718 on porosity, microstructure and mechanical properties10.1016/j.msea.2018.08.037 ↗
14. Impact of heat treatment on mechanical behaviour of Inconel 718 processed with tailored microstructure by selective laser melting10.1016/j.matdes.2017.05.065 ↗
15. Functionally graded Inconel 718 processed by additive manufacturing: Crystallographic texture, anisotropy of microstructure and mechanical properties10.1016/j.matdes.2016.10.075 ↗
16. API Standard 6ACRA
17. An efficient framework for printability assessment in laser powder bed fusion metal additive manufacturing
18. Effect of energy density on laser powder bed fusion built single tracks and thin wall structures with 100 μm preplaced powder layer thickness10.1016/j.optlastec.2019.106016 ↗
19. The role of powder layer thickness on the quality of SLM printed parts10.1016/j.acme.2018.01.015 ↗
20. Experimental studies on laser additive manufacturing of inconel-625 structures using powder bed fusion at 100 μm layer thickness10.1007/s11665-020-05215-9 ↗
21. Effect of laser speed, layer thickness, and part position on the mechanical properties of maraging 300 parts manufactured by selective laser melting10.1016/j.msea.2019.138425 ↗
22. Research on high layer thickness fabricated of 316L by selective laser melting10.3390/ma10091055 ↗
23. Effect of layer thickness in selective laser melting on microstructure of Al/5 wt.%Fe2O3 powder consolidated parts10.1155/2014/106129 ↗
24. Effects of layer thickness in laser-powder bed fusion of 420 stainless steel10.1108/RPJ-10-2019-0279 ↗
25. Performance of high layer thickness in selective laser melting of Ti6Al4V10.3390/ma9120975 ↗
26. Powder bed fusion of Nickel-based superalloys: A review10.1016/j.ijmachtools.2021.103729 ↗
27. The effect of layer thickness at selective laser melting10.1016/j.proeng.2017.01.179 ↗
28. Improving productivity in the laser powder bed fusion of Inconel 718 by increasing layer thickness: Effects on mechanical behavior
29. Selective laser melting of the Inconel 718 Nickel superalloy
30. Heat treatment of alloy 718 made by additive manufacturing for oil and gas applications10.1007/s11837-018-03321-7 ↗
31. Alloy 718 for oilfield applications10.1007/s11837-012-0238-z ↗
32. Inconel alloy 718 datasheet
33. 2020
34. 2017
35. Metal Powder Industries Federation (MPIF) Standards · 2022
36. Recent advances in inductively coupled plasma optical emission spectrometry10.1039/C7JA00103G ↗
37. Inductively coupled plasma mass spectrometry10.1021/ac8006945 ↗
38. ASTM International · 2020
39. ASTM B212 · 1999
40. Temperature fields produced by traveling distributed heat sources
41. Additive manufacturing of metallic components–process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
42. Multivariate calibration and experimental validation of a 3D finite element thermal model for laser powder bed fusion metal additive manufacturing10.1007/s40192-018-0113-z ↗
43. Uncertainty propagation analysis of computational models in laser powder bed fusion additive manufacturing using polynomial chaos expansions10.1115/1.4041179 ↗
44. Thermophysical properties of solid and liquid Inconel 718 alloy10.1068/htwu340 ↗
45. Experimental study of direct laser deposition of Ti-6Al-4V and Inconel 718 by using pulsed parameters
46. Bayesian calibration of computer models10.1111/1467-9868.00294 ↗
47. ASTM International · 2015
48. Rasband · 2011
49. Stress concentration factors for ASTM E8/E8M-15a plate-type specimens for tension testing10.1520/JTE20160385 ↗
50. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
51. A highly accurate methodology for the prediction and correlation of mechanical properties based on the slimness ratio of additively manufactured tensile test specimens10.1007/s10853-020-04654-y ↗
52. The microstructure and mechanical properties of deposited-IN718 by selective laser melting10.1016/j.jallcom.2011.10.107 ↗
53. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
54. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
55. Effect of heat treatment on microstructure evolution of Inconel 718 alloy fabricated by selective laser melting10.1016/j.jallcom.2018.06.112 ↗