Selective laser melting of elemental powder blends for fabrication of homogeneous bulk material of near-eutectic Ni‒Sn composition
Source abstract
Abstract
Abstract Cubic specimens of near-eutectic Ni‒Sn composition were built by selective laser melting of elemental powder blends and annealed. Microstructure of the specimens before and after annealing was investigated. Cracks and pores were present in all specimens due to thermal stresses and insufficient melting. Despite such defects, specimens built at low laser power and low laser scanning speed showed improved bulk chemical homogeneity compared to those built at high power and high speeds. Microscopic studies showed that a dendritic structure was formed in specimens of hypoeutectic Ni83Sn17 composition, whereas a banded structure was formed in specimens of eutectic Ni81.3Sn18.7 and hypereutectic Ni80Sn20 composition. After annealing, these structures were converted into a similar anomalous eutectic-like structure. While the formation of the banded structure was attributed to a high liquid undercooling during selective laser melting, the annealing effect was explained by assuming supersaturation of solute atoms in phase constituents. It is concluded that selective laser melting of elemental powder blends followed by post annealing is a promising way of producing a two-phase bulk material of near-eutectic composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
2. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
3. Structure of undercooled Ni–Sn eutectic10.1007/BF02900268 ↗
4. High undercooling and rapid solidification of Ni–32.5% Sn eutectic alloy10.1016/0956-7151(91)90212-J ↗
5. Microtexture and macrotexture formation in the containerless solidification of undercooled Ni–18.7 at.% Sn eutectic melts10.1016/j.actamat.2004.10.029 ↗
6. Eutectic growth in bulk undercooled melts10.1016/j.actamat.2005.01.042 ↗
7. Structural evidence for the transition from coupled to decoupled growth in the solidification of undercooled Ni–Sn eutectic melt10.1007/s11661-007-9198-2 ↗
8. New evidence for dual origin of anomalous eutectic structures in undercooled Ni–Sn alloys: in-situ observations and EBSD characterization10.1016/j.actamat.2011.03.016 ↗
9. Modeling of free eutectic growth and competitive solidification in undercooled near-eutectic alloys based on in-situ measurements10.1007/s10853-014-8585-5 ↗
10. In situ observation of remelting induced anomalous eutectic structure formation in an undercooled Ni–18.7 at. % Sn eutectic alloy10.1016/j.scriptamat.2019.10.019 ↗
11. Microstructure evolution in laser surface remelting of Ni–33wt.% Sn alloy10.1016/j.jallcom.2013.05.119 ↗
12. Three-dimensional reconstruction of anomalous eutectic in laser remelted Ni–30 wt.% Sn alloy10.1088/1468-6996/16/6/065007 ↗
13. Regular eutectic and anomalous eutectic growth behavior in laser remelting of Ni–30wt% Sn alloys10.1016/j.actamat.2016.12.061 ↗
14. Rapid solidification of Al–Cu eutectic alloy by laser remelting10.1016/0001-6160(89)90203-4 ↗
15. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
16. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
17. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
18. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
19. Laser cladding with mixed powder feed
20. Alloy system analysis by laser cladding
21. In situ elaboration of a binary Ti‒26Nb alloy by selective laser melting of elemental titanium and niobium mixed powders10.1016/j.msec.2016.02.033 ↗
22. Investigations on the influence of composition in the development of Ni‒Ti shape memory alloy using laser based additive manufacturing10.1016/j.optlastec.2014.12.014 ↗
23. Microstructure and transformation behavior of in-situ shape memory alloys by selective laser melting Ti–Ni mixed powder10.1016/j.jmst.2013.05.006 ↗
24. Laser deposition of compositionally graded titanium-vanadium and titanium-molybdenum alloys10.1016/S0921-5093(02)00909-7 ↗
25. Wear behavior and microstructure of hypereutectic Al‒Si alloys prepared by selective laser melting10.1016/j.apsusc.2016.03.221 ↗
26. Fatigue-resistant high-performance elastocaloric materials made by additive manufacturing10.1126/science.aax7616 ↗
27. Direct laser deposition of alloys from elemental powder blends10.1016/S1359-6462(01)01107-1 ↗
28. Microstructure and mechanical properties of laser solid formed Ti–6Al–4V from blended elemental powders10.1016/S1875-5372(10)60028-8 ↗