journal article·2022-08

Effect of oxide dispersoids on precipitation-strengthened Al-1.7Zr (wt %) alloys produced by laser powder-bed fusion

Jennifer A. Glerum, Anthony De Luca, Marvin L. Schuster, Christoph Kenel, Christian Leinenbach, David C. Dunand

Publisher page

Abstract

Binary Al-1.7 wt % Zr (Al-0.5 at % Zr) alloys, with and without 1 wt % (0.7 vol %) Al2O3 nanoparticle additions (80–100 nm), are fabricated by laser powder-bed fusion (L-PBF) from blends of Al, Zr, and Al2O3 powders. Elemental Zr, which is ~80 % dissolved in the melt pool, forms primary L12-Al3Zr precipitates upon solidification and is also retained in a supersaturated solid solution in the Al matrix. The primary L12-Al3Zr phase takes three forms: (i) discrete, micron-sized precipitates that nucleate fine Al matrix grains, (ii) elongated “strings” of submicron precipitates forming in highly enriched Zr regions, and (iii) < 100 nm precipitates within fine Al-grains. The Al2O3 nanodispersoid additions are either lost to slag or entrapped within Al-grains as oxide dispersoids, resulting in an oxide concentration of 0.46 wt % for the modified ODS alloy. Al2O3 nanoscale dispersoids (0.28 wt %) are also observed in the unmodified alloy, and are assumed to originate from (i) native oxides from the surface of the Al powder particles, and/or (ii) reaction with trace amounts of oxygen in the processing environment. The hardness upon aging at 400 °C reaches a peak value of ~750–850 MPa after 1.5 h, consistent with precipitation of secondary L12-Al3Zr nanoprecipitates. Upon overaging, hardness slowly decreases to 500 MPa (the as-processed value) after 1,500 h at 400 °C, with no difference observed between the Al-Zr and Al-Zr-Al2O3 alloys. Strengthening mechanisms combines Hall-Petch strengthening from micron-sized grains, Zr solid-solution strengthening, and secondary L12-Al3Zr precipitate strengthening, with slow precipitate coarsening and effective grain pinning by Al3Zr precipitates and oxide dispersoids located at grain boundaries. Creep resistance is comparable for both alloys, which show threshold stresses of ~15 and 6 MPa, at 300 and 400 °C respectively. Oxygen content analysis is recommended for all Al-based alloys fabricated via L-PBF due to the potential for non-reproducible nanoscale oxide inclusions (from native oxide on Al powders and from reaction with residual oxygen), which may affect the mechanical properties of the alloys, but are difficult to observe via SEM or TEM analysis.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Microstructure characterization of SLM-processed Al-Mg-Sc-Zr alloy in the heat treated and HIPed condition
2. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
3. SLM-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
4. Influence of SLM scan-speed on microstructure, precipitation of Al 3 Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
5. Microstructure and mechanical properties of as-processed scandium-modified aluminium using selective laser melting10.1016/j.cirp.2016.04.057 ↗
6. Mechanical anisotropy investigated in the complex SLM-processed Sc- and Zr-modified Al-Mg alloy microstructure
7. Comparison of microstructure and mechanical properties of scalmalloy((r)) produced by selective laser melting and laser metal deposition
8. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
9. Coarsening- and creep resistance of precipitation-strengthened Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
10. Effect of laser rescanning on the grain microstructure of a selective laser melted Al-Mg-Zr alloy10.1016/j.matchar.2018.03.033 ↗
11. Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
12. Operando X-ray diffraction study of thermal and phase evolution during laser powder bed fusion of Al-Sc-Zr elemental powder blends
13. In-situ full-field mapping of melt flow dynamics in laser metal additive manufacturing
14. Effect of Al alloys on selective laser melting behaviour and microstructure of in situ formed particle reinforced composites10.1016/j.jallcom.2012.06.097 ↗
15. Synthesis and characterisation of advanced ball-milled Al-Al 2 O 3 nanocomposites for selective laser melting10.1016/j.powtec.2016.04.015 ↗
16. Microstructure evolution and mechanical properties of Al-Al2O3 composites fabricated by selective laser melting10.1016/j.powtec.2016.12.079 ↗
17. Alumina loss mechanism of Al2O3-AlSi10 Mg composites during selective laser melting10.1016/j.jallcom.2019.01.116 ↗
18. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
19. Microstructure and room and high temperature mechanical properties of ultrafine structured Al-5 wt%Y2O3 and Al-5 wt%La2O3 nanocomposites fabricated by mechanical alloying and hot pressing10.1016/j.msea.2019.01.091 ↗
20. Selective laser melting of nano-TiB 2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
21. A heat treatable TiB2/Al-3.5Cu-1.5Mg-1Si composite fabricated by selective laser melting: Microstructure, heat treatment and mechanical properties10.1016/j.compositesb.2018.04.026 ↗
22. Microstructure, solidification behavior and mechanical properties of Al-Si-Mg-Ti/TiC fabricated by selective laser melting
23. Selective laser melting of nano-TiN modified AlSi10Mg composite powder with low laser reflectivity10.1016/j.matlet.2018.10.126 ↗
24. Melt spreading behavior, microstructure evolution and wear resistance of selective laser melting additive manufactured AlN/AlSi10Mg nanocomposite10.1016/j.surfcoat.2018.05.072 ↗
25. Synthesis of a (ZrAl3+AlN)/Al composite and the influence of particles content and element Cu on the microstructure and mechanical properties10.1016/j.jallcom.2019.03.416 ↗
26. Creep properties and microstructure evolution at 260-300oC of AlSi10Mg manufactured via laser powder-bed fusion10.1016/j.msea.2022.143075 ↗
27. Coarsening kinetics at 600 degrees C of Al2O3 dispersoids in a mechanically alloyed aluminium alloy10.1016/S1359-6462(02)00153-7 ↗
28. Creep of metals containing high volume fractions of unshearable dispersoids—Part II. Experiments in the Al·Al2O3 system and comparison to models10.1016/S1359-6454(97)00136-5 ↗
29. Strengthening mechanisms in aluminum containing coherent Al3Sc precipitates and incoherent Al2O3 dispersoids10.1016/j.actamat.2006.10.004 ↗
30. Monkman-grant analysis of creep fracture in dispersion-strengthened and particulate-reinforced aluminum10.1007/s11661-999-0076-y ↗
31. Enhanced densification of cavitated dispersion-strengthened aluminum by thermal cycling10.1007/s11661-000-0209-9 ↗
32. Effects of W and Si microadditions on microstructure and the strength of dilute, precipitation-strengthened Al–Zr–Er alloys10.1016/j.msea.2020.140159 ↗
33. Precipitation evolution in Al–Zr and Al–Zr–Ti alloys during isothermal aging at 375–425°C10.1016/j.actamat.2007.09.004 ↗
34. Coarsening resistance at 400°C of precipitation-strengthened Al–Zr–Sc–Er alloys10.1016/j.actamat.2011.07.057 ↗
35. Effect of vanadium micro-alloying on the microstructural evolution and creep behavior of Al-Er-Sc-Zr-Si alloys10.1016/j.actamat.2016.11.033 ↗
36. Diffusion of zirconium in aluminum
37. Effects of hot isostatic pressing and internal porosity on the performance of selective laser melted AlSi10Mg alloys10.1016/j.msea.2019.138713 ↗
38. Effect of different heat-treatment routes on the impact properties of an additively manufactured AlSi10Mg alloy10.1016/j.msea.2020.140671 ↗
39. Factors that affect the properties of additively-manufactured AlSi10Mg: Porosity versus microstructure
40. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
41. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
42. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
43. Microstructures and tensile properties of a selective laser melted Al–Zn–Mg–Cu (Al7075) alloy by Si and Zr microalloying10.1016/j.msea.2020.139492 ↗
44. The Al-Zr (aluminum-zirconium) system10.1007/BF02667556 ↗
45. Al-Zr (Aluminum-Zirconium)10.1361/105497102770331497 ↗
46. The mechanism of discontinuous precipitation of the metastable Al 3 Zr phase from an Al-Zr solid solution10.1016/0001-6160(77)90133-X ↗
47. On the formation of fan-shaped precipitates during the decomposition of a highly supersaturated Al-Zr solid solution10.1016/0036-9748(71)90142-6 ↗
48. Precipitation and recrystallization in an Al-0.5 wt percent Zr-alloy
49. Precipitation behavior of L12 Al3Zr phase in Al-Mg-Zr alloy10.1016/j.matchar.2018.02.030 ↗
50. Solidification of peritectic alloys10.1179/imr.1996.41.4.129 ↗
51. Peritectic formation in the Ni-Al system10.1016/0022-0248(94)90477-4 ↗
52. Two-phase growth in peritectic Fe–Ni alloys10.1016/S1359-6454(00)00034-3 ↗
53. Peritectic reaction and its influences on the microstructures evolution during directional solidification of Fe–Ni alloys10.1016/j.jallcom.2007.07.009 ↗
54. Direct nucleation and growth of peritectic phase induced by substantial undercooling condition10.1016/j.matlet.2013.06.084 ↗
55. The peritectoid formation of ordered Zr3Al10.1016/0001-6160(76)90081-X ↗
56. Non-equilibrium solidification of hyperperitetic Al-Zr Alloys10.1016/0001-6160(77)90132-8 ↗
57. Wetting of aluminium oxide by molten aluminium and other metals10.1007/BF00555046 ↗
58. Tabor · 1951
59. Effect of aging treatment on the microstructure and mechanical properties of Al-3.02Mg-0.2Sc-0.1Zr alloy printed by selective laser melting10.1016/j.matdes.2019.107668 ↗
60. Precipitation hardening in dilute Al–Zr alloys10.1016/j.jmrt.2017.05.006 ↗
61. Microstructure and mechanical properties of a precipitation-strengthened Al-Zr-Sc-Er-Si alloy with a very small Sc content10.1016/j.actamat.2017.10.040 ↗
62. Ambient- and elevated-temperature strengthening by Al3Zr-Nanoprecipitates and Al3Ni-Microfibers in a cast Al-2.9Ni-0.11Zr-0.02Si-0.005Er (at%) alloy10.1016/j.msea.2019.05.018 ↗
63. Creep resistance of cast and aged Al–0.1Zr and Al–0.1Zr–0.1Ti (at%) alloys at 300–400°C10.1016/j.scriptamat.2008.02.059 ↗
64. Precipitation evolution in Al–Zr and Al–Zr–Ti alloys during aging at 450–600°C10.1016/j.actamat.2007.11.011 ↗
65. Modeling the creep threshold stress due to climb of a dislocation in the stress field of a misfitting precipitate10.1016/j.actamat.2011.04.044 ↗
66. Mechanical properties of Al(Sc,Zr) alloys at ambient and elevated temperatures10.1016/S1359-6454(03)00320-3 ↗
67. Frost · 1982
68. The kinetics of dislocation climb over hard particles--II. effects of an attractive particle-dislocation interaction10.1016/0001-6160(88)90159-9 ↗
69. Nucleation and precipitation strengthening in dilute Al-Ti and Al-Zr alloys10.1007/s11661-007-9283-6 ↗
70. Strengthening mechanisms in Al Ni Sc alloys containing Al3Ni microfibers and Al3Sc nanoprecipitates10.1016/j.actamat.2018.10.059 ↗
71. A new approach to synthesise high strength nano-oxide dispersion strengthened alloys10.1016/j.jallcom.2019.03.221 ↗
72. In-situ alloyed, oxide-dispersion-strengthened CoCrFeMnNi high entropy alloy fabricated via laser powder bed fusion10.1016/j.matdes.2020.108966 ↗
73. Characterization of nano-scale oxides in austenitic stainless steel processed by powder bed fusion10.1016/j.scriptamat.2018.06.011 ↗
74. Numerical modeling of oxide particle evolution during additive manufacturing