journal article·1930-01-01

The Production of Electrolytic Iron Printing Plates

C. T. Thomas, W. Blum

Publisher page

Abstract

Thick printing plates are being made by depositing iron from baths that contain about 3 N FeCl 3 , 2 to 4 N CaCl 2 , and 0.01 N HCl. A cathode current density of about 7 amp./sq. dm. (65 amp./sq. ft.), is used and a temperature of about 90° C. (194° F.). The anodes are suspended in porous alundum diaphragms. The deposited iron has a tensile strength of about 4,000 kg./sq. cm. (56,000 lb./sq. in.) and an elongation of about 20 per cent. The finished plates are plated with chromium to increase the resistance to abrasion.