journal article·2024-01Open access

Nanoscale engineering of low-misfit TiB2/Al3(Sc,Zr)/α-Al multi-interface to improve strength-ductility synergy for direct energy deposited aluminum alloy

Yang Li, Yihao Wang, Lei Hu, Tingting Chen, Gang Ji, Han Chen, Hongze Wang, Haowei Wang, Zhe Chen

Abstract

The nature of the interface between ceramic particle (CP) and metal matrix is critical to obtain solidification microstructures with optimal mechanical properties of CPreinforced Al alloys in additive manufacturing. Generally, when the lattice misfit between the CP (e.g., TiB2) and the α-Al matrix is higher than 4 %, the interfacial coherency reduces, lowering the effectiveness of CPs. Here, we demonstrate that an L12 threedimensional compound (3DC), which possesses lattice misfit with α-Al lower than 1 %, can be introduced in between TiB2 and α-Al via properly regulating the solidification cooling rate. In the 5TiB2/Al-4.5Mg-0.7Sc-0.2Zr (wt.%) as a model system, the lattice coherence of the TiB2/α-Al interface is tailored by introducing a 10-30 nm thick Al3(Sc,Zr) 3DC interphase when the cooling rate is increased to ~1000 o C/s. But, further increasing the cooling rate to ~6800 o C/s, only Al3(Sc,Zr) two-dimensional compound (2DC) with an apparent lattice strain forms at the interface. Taking advantage of the cooling rate (10 2 -10 3 o C/s) provided by laser direct energy deposition (L-DED), the low-misfit "TiB2/Al3(Sc,Zr) 3DC/α-Al" multi-structural interfaces are acquired, enabling the 3.56TiB2/Al-4.36Mg-0.72Sc-0.22Zr alloy as fabricated with L-DED to achieve improved strength-ductility synergy (yield strength 257 MPa, elongation 13.8%) due to the isotropically fine Al grain structure and the homogenous TiB2 particle dispersion. The outcome of this study provides fundamental knowledge on designing "ceramic/coherent primary interphase/metal matrix" multi-structural interfaces to improve the mechanical properties of engineering metallic materials manufactured by rapid solidification techniques, such as DED additive manufacturing (AM).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (86)

Show source-provided references
1. A review of Laser Powder Bed Fusion Additive Manufacturing of aluminium alloys: microstructure and properties
2. Demonstrating the roles of solute and nucleant in grain refinement of additively manufactured aluminium alloys
3. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
4. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
5. Towards understanding grain nucleation under Additive Manufacturing solidification conditions10.1016/j.actamat.2020.05.012 ↗
6. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
7. The role of in-situ nano-TiB2 particles in improving the printability of noncastable 2024Al alloy10.1080/21663831.2022.2080514 ↗
8. Additive manufacturing enabled synergetic strengthening of bimodal reinforcing particles for aluminum matrix composites
9. Atomic-scale investigation of the interface precipitation in a TiB2 nanoparticles reinforced Al–Zn–Mg–Cu matrix composite10.1016/j.actamat.2019.11.068 ↗
10. Achieving simultaneously improved tensile strength and ductility of a nano-TiB2/AlSi10Mg composite produced by cold spray additive manufacturing10.1016/j.compositesb.2020.108404 ↗
11. Simultaneously increasing strength and ductility of nanoparticles reinforced Al composites via accumulative orthogonal extrusion process10.1080/21663831.2018.1471421 ↗
12. High performance Al/TiB2 composites fabricated by nanoparticle reinforcement and cutting-edge super vacuum assisted die casting process10.1016/j.compositesb.2019.107453 ↗
13. On the strength of discontinuous silicon carbide reinforced aluminum composites10.1016/0036-9748(86)90210-3 ↗
14. Grain refining mechanism in the Al/Al–Ti–B system10.1016/j.actamat.2014.10.055 ↗
15. A new insight into heterogeneous nucleation mechanism of Al by non-stoichiometric TiCx10.1016/j.actamat.2022.117977 ↗
16. Grain refinement of Mg-alloys by native MgO particles: an overview10.1016/j.jma.2022.10.006 ↗
17. Understanding alloying behaviors of Sc, Ni and Zn additions on Al/TiB2 interfaces based on interfacial characteristics and solute properties
18. Interfacial energy between Al melt and TiB2 particles and efficiency of TiB2 particles to nucleate α-Al10.1016/j.scriptamat.2018.09.042 ↗
19. Interface alloying design to improve the dispersion of TiB2 nanoparticles in Al composites: a first-principles study10.1021/acs.jpcc.1c00371 ↗
20. Mechanism of Sc poisoning of Al-5Ti-1B grain refiner10.1016/j.scriptamat.2020.01.031 ↗
21. Effect of solutes on grain refinement
22. Interfacial superstructures and chemical bonding transitions at metal-ceramic interfaces
23. Insight into Si poisoning on grain refinement of Al-Si/Al-5Ti-B system10.1016/j.actamat.2020.01.039 ↗
24. Mechanism for Zr poisoning of Al-Ti-B based grain refiners10.1016/j.actamat.2018.10.056 ↗
25. Break through the strength-ductility trade-off dilemma in aluminum matrix composites via precipitation-assisted interface tailoring10.1016/j.actamat.2022.118470 ↗
26. Complete columnar-to-equiaxed transition and significant grain refinement in an aluminium alloy by adding Nb particles through laser powder bed fusion
27. Development of a high strength Zr/Sc/Hf-modified Al-Mn-Mg alloy using laser powder bed fusion: design of a heterogeneous microstructure incorporating synergistic multiple strengthening mechanisms
28. Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys
29. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
30. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
31. Understanding grain refinement of Sc addition in a Zr containing Al-Zn-Mg-Cu aluminum alloy from experiments and first-principles10.1016/j.intermet.2020.106823 ↗
32. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
33. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior10.1016/j.jmst.2020.08.003 ↗
34. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
35. Grain refinement mechanisms in additively manufactured nano-functionalized aluminum10.1016/j.actamat.2020.09.043 ↗
36. Solidification orientation relationships between Al3Ti and TiB210.1016/j.actamat.2019.12.013 ↗
37. An understanding of duplex microstructures encountered during high strength aluminium alloy laser beam melting processing10.1016/j.actamat.2021.117024 ↗
38. Dendritic and seaweed growth of proeutectic scandium tri-aluminide in hypereutectic Al-Sc undercooled melt10.1016/j.actamat.2020.08.078 ↗
39. Effect of cooling rate on morphology of primary particles in Al-Sc-Zr master alloy10.1016/S1003-6326(14)63366-5 ↗
40. Significantly improved particle strengthening of Al–Sc alloy by high Sc composition design and rapid solidification10.1016/j.msea.2020.140304 ↗
41. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
42. Selective laser melting of a novel Sc and Zr modified Al-6.2Mg alloy: processing, microstructure, and properties10.1016/j.powtec.2017.06.050 ↗
43. Comparison of microstructure and mechanical properties of Scalmalloy® produced by selective laser melting and laser metal deposition10.3390/ma11010017 ↗
44. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
45. Effects of step size and cut-off limit of residual liquid amount on solidification simulation of Al–Mg–Zn system with Scheil model10.1016/j.intermet.2008.12.006 ↗
46. PANDAT software with PanEngine, PanOptimizer and Panprecipitation for multi-component phase diagram calculation and materials property simulation10.1016/j.calphad.2008.08.004 ↗
47. Understanding cellular structure formation in rapidly solidified Al–Ni alloys by constructing solidification microstructure selection maps
48. Novel composite powders with uniform TiB2 nano-particle distribution for 3D printing10.3390/app7030250 ↗
49. A physical modeling and predictive simulation of the laser cladding process
50. Multicomponent multiphase modeling of dissimilar laser cladding process with high-speed steel on medium carbon steel10.1016/j.ijheatmasstransfer.2019.118990 ↗
51. Microstructures and Mechanical Properties of Al-Mg-Sc-Zr Alloy Additively Manufactured by Laser Direct Energy Deposition
52. Investigation of misfit dislocations in α-Fe2O3/α-Al2O3 interface by geometric phase analysis and dislocation density tensor analysis10.1016/j.matchar.2015.06.012 ↗
53. The optimum grain size for strength-ductility combination in metals10.1016/j.ijplas.2023.103574 ↗
54. Achieving uniform plasticity in a high strength Al-Mn-Sc based alloy through laser-directed energy deposition
55. Fabrication of Al-11.2 Si components by direct laser metal deposition for automotive applications10.5781/JWJ.2017.35.4.10 ↗
56. Microstructure refinement for superior ductility of Al–Si alloy by electron beam melting
57. Directed energy deposition of Al 5xxx alloy using Laser Engineered Net Shaping (LENS®)10.1016/j.matdes.2020.108763 ↗
58. Deformation microstructures and strengthening mechanisms for the wire+arc additively manufactured Al-Mg-4.5Mn alloy with inter-layer rolling10.1016/j.msea.2017.11.113 ↗
59. The heterogeneous band microstructure and mechanical performance in a wire+arc additively manufactured 2219 Al alloy
60. Hot deformation induced microstructural evolution in local-heterogeneous wire+ arc additive manufactured 2219 Al alloy10.1016/j.jallcom.2021.158949 ↗
61. Mechanical properties and precipitation behavior of the heat-treated wire+arc additively manufactured 2219 aluminum alloy10.1016/j.matchar.2020.110735 ↗
62. Properties of wire+arc additively manufactured 2024 aluminum alloy with different solution treatment temperature10.1016/j.matlet.2018.07.144 ↗
63. Directed energy deposition of AlSi10Mg: single track nonscalability and bulk properties10.1016/j.matdes.2020.108847 ↗
64. Mechanical properties of AlSi10Mg alloy fabricated by laser melting deposition and improvements via heat treatment10.1016/j.ijleo.2018.10.112 ↗
65. Laser metal deposition of nickel coated Al 7050 alloy10.1016/j.jallcom.2017.05.171 ↗
66. Wire-arc additive manufacturing of a novel high-performance Al-Zn-Mg-Cu alloy: processing, characterization and feasibility demonstration
67. Microstructure and Mechanical Properties of TiC-Reinforced Al–Mg–Sc–Zr Composites Additively Manufactured by Laser Direct Energy Deposition
68. Directed energy deposition additive manufacturing of a Sc/Zr-modified Al–Mg alloy: effect of thermal history on microstructural evolution and mechanical properties10.1016/j.msea.2020.140606 ↗
69. Microstructure and mechanical properties of a combination interface between direct energy deposition and selective laser melted Al-Mg-Sc-Zr alloy10.3390/met11050801 ↗
70. Kurz · 1992
71. Morphological stability of a solid particle growing from a binary alloy melt10.1016/0022-0248(80)90197-9 ↗
72. An analytical model for solute segregation at liquid metal/solid substrate interface10.1007/s11661-014-2525-5 ↗
73. Improved prediction of the grain size of aluminum alloys that includes the effect of cooling rate10.1016/j.msea.2007.11.009 ↗
74. Perepezko · 1988
75. Modelling of inoculation of metallic melts: application to grain refinement of aluminium by Al–Ti–B10.1016/S1359-6454(00)00094-X ↗
76. The interdependence theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
77. Processing and properties of magnesium containing a dense uniform dispersion of nanoparticles10.1038/nature16445 ↗
78. Interaction between nucleant particles and a solid-liquid interface in Al-4.5Cu alloy10.1016/j.actamat.2021.116956 ↗
79. Theoretical study and pathways for nanoparticle capture during solidification of metal melt10.1088/0953-8984/24/25/255304 ↗
80. Effect of clustering on particle pushing and solidification behaviour in TiB2 reinforced aluminium PMMCs10.1016/j.compositesa.2004.10.027 ↗
81. Controlling particle/metal interactions in metal matrix composites during solidification: the role of melt viscosity and cooling rate10.1007/s11661-019-05307-9 ↗
82. On the behaviour of foreign particles at an advancing solid-liquid interface10.1016/0022-0248(89)90097-3 ↗
83. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface10.1007/BF02801184 ↗
84. Microhardness measurements and the Hall-Petch relationship in an Al–Mg alloy with submicrometer grain size10.1016/1359-6454(96)00105-X ↗
85. The Hall–Petch relation in aluminium and its dependence on the grain boundary structure10.1080/01418618608242849 ↗
86. Quantitative study of particle size distribution in an in-situ grown Al–TiB2 composite by synchrotron X-ray diffraction and electron microscopy10.1016/j.matchar.2015.03.003 ↗