journal article·2024-07

Influence of friction and back stresses evolution on cyclic softening of laser powder bed fusion Ti-6Al-4V ELI alloy

Akhilesh Goyal, Anish Ranjan, Bhallamudi Ravi, Shyamprasad Karagadde

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Effect of heat treatment temperature and turning residual stresses on the plain and notch fatigue strength of Ti-6Al-4V additively manufactured via laser powder bed fusion
2. Investigation of fatigue behavior of laser powder bed fusion Ti-6Al-4V: Roles of heat treatment and microstructure
3. T. L. F. Behavior, F. Mechanism, and T. Methods, “The Low-Cycle Fatigue Behavior, Failure Mechanism and,” 2021.
4. Influence of oxygen content on the forging response of equiaxed (α+β) preform of Ti-6Al-4V: commercial vs. ELI grade10.1016/S0924-0136(00)00832-3 ↗
5. R. Boyer, G. Welsch, and E.W. Collings, Materials properties handbook: titanium alloys. 1994.
6. Patient-specific Ti-6Al-4V lattice implants for critical-sized load-bearing bone defects reconstruction10.1016/j.matdes.2023.111605 ↗
7. Effect of build thickness and geometry on quasi-static and fatigue behavior of Ti-6Al-4V produced by Electron Beam Melting
8. Influence of surface finishing and heat treatments on the corrosion resistance of LPBF-produced Ti-6Al-4V alloy for biomedical applications
9. Melt pool temperature and cooling rates in laser powder bed fusion
10. Separation of the impact of residual stress and microstructure on the fatigue performance of LPBF Ti-6Al-4V at elevated temperature
11. An overview of residual stresses in metal powder bed fusion
12. Towards isotropic behaviour in Ti–6Al–4V fabricated with laser powder bed fusion and super transus hot isostatic pressing
13. F. Technique, R. Metals, T. Alloys, Q.C. Program, and T. Alloys, “Standard Specification for Wrought Titanium-6Aluminum-4Vanadium ELI (Extra Low Interstitial) Alloy for Surgical Implant Applications ( UNS R56401),” vol. 13, no. Reapproved, pp. 1–5, 2009, doi: 10.1520/F0136-13R21E01.2.
14. ASTM, “ASTM F3001-14: Standard Specification for Additive Manufacturing Titanium-6 Aluminum-4 Vanadium ELI (Extra Low Interstitial) with Powder Bed Fusion,” ASTM Interational, vol. i, no. Reapproved, pp. 1–8, 2012, doi: 10.1520/F3001-14R21.10.1520/F3001-14R21 ↗
15. ASTM International, “F2924-14: Standard Specification for Additive Manufacturing Titanium-6 Aluminum-4 Vanadium with Powder Bed Fusion,” ASTM Int., vol. i, no. Reapproved, pp. 1–9, 2021, doi: 10.1520/F2924-14R21.2.
16. Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V10.1016/j.jallcom.2018.02.111 ↗
17. Effect of heat treatment on the anisotropic mechanical properties of AlSi10Mg fabricated by selective laser melting
18. Effects of heat treatment on microstructure and mechanical properties of selective laser melted Ti-6Al-4V lattice materials
19. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: a comparative study
20. In-situ selective laser heat treatment for microstructural control of additively manufactured Ti-6Al-4V
21. Fatigue crack growth parameters of Laser Powder Bed Fusion produced Ti-6Al-4V
22. Microstructure evolution and cyclic deformation behavior of Ti-6Al-4 V alloy via electron beam melting during low cycle fatigue
23. Strain controlled fatigue behaviour of a wire + arc additive manufactured Ti-6Al-4V
24. Coupling effects of microstructure and defects on the fatigue properties of laser powder bed fusion Ti-6Al-4V
25. Standardized loads acting in hip implants10.1371/journal.pone.0155612 ↗
26. Hip joint contact forces during stumbling10.1007/s00423-003-0434-y ↗
27. Low cycle fatigue properties of Ti-6Al-4V alloy fabricated by high-power laser directed energy deposition: experimental and prediction10.1016/j.ijfatigue.2019.05.035 ↗
28. P. Zhang, A.N. He, F. Liu, K. Zhang, and J. Jiang, “Evaluation of Low Cycle Fatigue Performance of,” Metals (Basel)., vol. 9, no. 1041, pp. 1–16, 2019.10.3390/met9101041 ↗
29. Cyclic plasticity and damage mechanisms of Ti-6Al-4V processed by electron beam melting
30. Cyclic softening behavior of Ti–6Al–4V alloy at macro and micro-scale10.1016/j.matlet.2016.08.119 ↗
31. A study of the back stress and the friction stress behaviors of Ti-6Al-4V alloy during low cycle fatigue at room temperature10.1016/j.msea.2017.06.051 ↗
32. Comparison of the microstructures and mechanical properties of Ti-6Al-4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗
33. Comparative study of fatigue properties of Ti-6Al-4V specimens built by electron beam melting (EBM) and selective laser melting (SLM)10.1016/j.matchar.2018.03.028 ↗
34. Fatigue Behaviour of Additively Manufactured Ti-6Al-4V10.1016/j.proeng.2015.12.632 ↗
35. Torsional fatigue behavior of wrought and additive manufactured Ti-6Al-4V by powder bed fusion including surface finish effect10.1016/j.ijfatigue.2017.03.002 ↗
36. Heat treatment of Inconel 718 produced by selective laser melting: microstructure and mechanical properties10.1016/j.msea.2019.02.046 ↗
37. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
38. Investigation on ANisotropic Mechanical Behavior of Ti-6Al-4V alloy via schmid factor and kernel average misorientation distribution10.3390/met13010089 ↗
39. Stress-strain curves and modified material constitutive model for Ti-6Al-4V over thewide ranges of strain rate and temperature
40. Cyclic deformation behaviour of an α/β titanium alloy - I. Micromechanisms of plasticity under various loading paths10.1016/S1359-6454(96)00406-5 ↗
41. Unusual stress-induced martensite transformation in Ti-6Al-4V alloy enabled by solution treatment in the lower α+β regime10.1016/j.jallcom.2023.170330 ↗
42. Grain size effect on deformation mechanisms and mechanical properties of titanium
43. Comparative assessment of strain-controlled fatigue performance of SS 316L at room and low temperatures
44. A. Drews, “Standard Test Method for,” in Manual on Hydrocarbon Analysis, 6th Edition, vol. i, 100 Barr Harbor Drive, PO Box C700, West Consho hocken, PA 19428-2959: ASTM International, 2008, pp. 545-545–3.10.1520/MNL10913M ↗
45. Suresh S. - Fatigue of Materials-Cambridge University Press (1998).pdf.”.10.1017/CBO9780511806575 ↗
46. New method for evaluation of the Manson-Coffin-Basquin and Ramberg-Osgood equations with respect to compatibility10.1016/j.ijfatigue.2008.01.012 ↗
47. The low-cycle fatigue behavior, failure mechanism and prediction of SLM Ti-6Al-4V alloy with different heat treatment methods
48. The physics of fatigue crack initiation10.1016/j.ijfatigue.2012.10.009 ↗
49. Fatigue crack growth behavior of laser powder bed fusion additive manufactured Ti-6Al-4V: roles of post heat treatment and build orientation
50. High cycle fatigue and fatigue crack propagation behaviors of β-annealed Ti-6Al-4V alloy10.1186/s40712-016-0069-8 ↗
51. Cyclic deformation response and micromechanisms of Ti alloy Ti-5Al-5V–5Mo-3Cr-0.5Fe10.1016/j.msea.2011.08.045 ↗
52. Effect of strain amplitude on low cycle fatigue and microstructure evolution in Ti-6Al-4V: A TKD and TEM characterization
53. Dislocations and plastic flow in crystals10.1119/1.1933704 ↗
54. Dislocation behavior in fatigue IV. Quantitative interpretation of friction stress and back stress derived from hysteresis loops10.1016/0025-5416(79)90062-4 ↗
55. Cyclic softening of the Ti-10V–2Fe-3Al titanium alloy10.1016/S0921-5093(96)10531-1 ↗
56. Effect of the primary alpha fraction on the dwell fatigue behaviour of Ti-6Al-4V alloy
57. Low cycle fatigue behavior of an α + β titanium alloy: Ti624610.1016/0921-5093(93)90423-C ↗
58. Low cycle fatigue behavior of Ti alloy IMI 834 at room temperature10.1016/S0921-5093(01)01468-X ↗