Effect of layer-wise femtosecond laser shock peening on cracking growth in laser powder bed fused AA 7075
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Additively manufactured fine-grained ultrahigh-strength bulk aluminum alloys with nanostructured strengthening defects
2. Densification and crack suppression in selective laser melting of pure molybdenum10.1016/j.matdes.2017.04.094 ↗
3. Cracking in laser additively manufactured W: Initiation mechanism and a suppression approach by alloying10.1016/j.matdes.2018.12.010 ↗
4. Review of recent trends and developments in aluminium 7075 alloys and metal matrix composites (MMCs) for aircraft applications10.1016/j.rineng.2023.101372 ↗
5. Deformation-based additive manufacturing of 7075 aluminum with wrought-like mechanical properties10.1016/j.matdes.2020.109288 ↗
6. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
7. Superior mechanical properties of a selective-laser-melted AlZnMgCuScZr alloy enabled by a tunable hierarchical microstructure and dual-nanoprecipitation10.1016/j.mattod.2021.11.019 ↗
8. Laser powder bed fusion of AA7075 alloy: Influence of process parameters on porosity and hot cracking
9. Experimental and numerical investigations of the hot cracking susceptibility during the powder bed fusion of AA 7075 using a laser beam
10. A new hot-tearing criterion10.1007/s11661-999-0334-z ↗
11. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
12. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: Cracking elimination by co-incorporation of Si and TiB2
13. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
14. Residual stress analysis of additive manufacturing of metallic parts using ultrasonic waves: State of the art review10.1016/j.jmrt.2020.05.092 ↗
15. Cracking in laser additively manufactured W: Initiation mechanism and a suppression approach by alloying10.1016/j.matdes.2018.12.010 ↗
16. A novel route for predicting the cracking of inoculant-added AA7075 processed via laser powder bed fusion
17. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
18. Review on field assisted metal additive manufacturing10.1016/j.ijmachtools.2023.104032 ↗
19. 3D Laser Shock Peening – A new method for the 3D control of residual stresses in Selective Laser Melting10.1016/j.matdes.2017.05.083 ↗
20. Healing cracks in selective laser melting by 3D laser shock peening
21. In situ X-ray tomography of fracture behaviour in low-porosity L-PBF AlSi10Mg alloy with laser shock peening10.1080/17452759.2023.2273955 ↗
22. Strengthened and hydrophobic surface of titanium alloy by femtosecond laser shock peening without a protective or sacrificial layer10.1016/j.optlastec.2023.109787 ↗
23. Femtosecond Laser Peening of Friction Stir Welded 7075-T73 Aluminum Alloys10.1016/j.jmatprotec.2018.06.022 ↗
24. Investigations on femtosecond laser-induced surface modification and periodic micropatterning with anti-friction properties on Ti6Al4V titanium alloy10.1016/j.cja.2021.01.003 ↗
25. Femtosecond Laser Shock Peening Residual Stress and Fatigue Life of Additive Manufactured AlSi10Mg10.1007/s11837-023-05820-8 ↗
26. Superior wear resistance in cast aluminum alloy via femtosecond laser induced periodic surface structures and surface hardening layer10.1016/j.apsusc.2023.157866 ↗
27. Enhanced Wear Properties of an Inspired Fish-Scale Film Structure in Terms of Microstructured Self-Lubrication Induced Effects by High-Speed Laser Surface Remelting Processing
28. Microstructure and residual stress modulation of 7075 aluminum alloy for improving fatigue performance by laser shock peening
29. Temperature dependence tensile behaviors of additively manufactured GH4099 Ni-based superalloy10.1016/j.msea.2024.146464 ↗
30. Linear chirping effects on heating of silicon surface after interaction with femtosecond laser pulses10.1016/j.ijleo.2019.163480 ↗
31. Double-pulse femtosecond laser peening of aluminum alloy AA5038: Effect of inter-pulse delay on transient optical plume emission and final surface micro-hardness10.1063/1.4968594 ↗
32. Residual stresses induced by laser-shocks
33. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
34. Measurement of Shock Wave Rise Times in Metal Thin Films10.1103/PhysRevLett.85.3205 ↗
35. A mechanism for dislocation generation in shock-wave deformation10.1016/0036-9748(78)90219-3 ↗