An additively manufactured heat-resistant Al-12Si alloy via introducing stable eutectic engineering
Source abstract
Abstract
The poor microstructural stability of crack-free Al alloys synthesized via additive manufacturing typically possesses poor heat resistance. In this work, a novel heat-resistant Al-12Si-1.5Ni-2.0Fe (wt.%) alloy was fabricated by additive manufacturing, in which tensile strength reaches 271 MPa and 98.1 MPa at 300 ºC and 400 ºC, respectively. Calculation and electron microscopy characterizations show that Fe/Ni segregation with high partition coefficients and low diffusion rates delivers a high thermal stability, thus providing a strong pinning force to inhibit the broken-up of Si eutectics and a solid barrier for dislocation motion at elevated temperatures. In addition to providing weight reduction by substituting Steel, Ti, and Ni-based alloys at 200-450 °C, the adoption of low-cost and stable eutectic engineering reduces the economic barriers to additive manufacturing applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (86)
Show source-provided references
1. Synergy of multiple precipitate/matrix interface structures for a heat resistant high-strength Al alloy10.1038/s41467-023-38730-z ↗
2. Heat-resistant super-dispersed oxide strengthened aluminium alloys10.1038/s41563-024-01884-2 ↗
3. Revealing the mechanism of grain refinement and anti Si-poisoning induced by (Nb, Ti)B2 with a sandwich-like structure10.1016/j.actamat.2021.117265 ↗
4. Extreme shear-deformation-induced modification of defect structures and hierarchical microstructure in an Al–Si alloy10.1038/s43246-020-00087-x ↗
5. On the origin of a remarkable increase in the strength and stability of an Al rich Al-Ni eutectic alloy by Zr addition10.1016/j.actamat.2019.03.025 ↗
6. Additive manufacturing of an ultrastrong, deformable Al alloy with nanoscale intermetallics10.1038/s41467-024-48693-4 ↗
7. From crack-prone to crack-free: Eliminating cracks in additively manufacturing of high-strength10.1016/j.jmst.2024.04.009 ↗
8. Anisotropic material properties of pure copper with fine-grained microstructure fabricated by laser powder bed fusion process
9. High-precision laser powder bed fusion processing of pure copper
10. Development of conformal shell lattices via laser powder bed fusion and unraveling their mechanical responses via modeling and experiments
11. Design of elastically isotropic shell lattices from anisotropic constitutive materials for additive manufacturing
12. Elastically-isotropic open-cell minimal surface shell lattices with superior stiffness via variable thickness design
13. An additively manufactured near-eutectic Al-Ce-Ni-Mn-Zr alloy with high creep resistance10.1016/j.actamat.2024.119787 ↗
14. Laser powder bed fusion of nano-titania modified 2219 aluminium alloy with superior mechanical properties at both room and elevated temperatures: The significant impact of solute
15. A high-strength heat-resistant Al−5.7Ni eutectic alloy with spherical Al3Ni nano-particles by selective laser melting10.1016/j.scriptamat.2021.114034 ↗
16. Achieving exceptional high-temperature resistant Al matrix composites via two-dimensional BN pinning grain rotation10.1016/j.compositesb.2023.110570 ↗
17. A novel Al-Cu composite with ultra-high strength at 350 ºC via dual-phase particle reinforced submicron-structure10.1002/advs.202207208 ↗
18. Tailoring the mechanical properties and thermal stability of additive manufactured micro-alloyed Al-Cu alloy via multi-stage heat treatment10.1016/j.matdes.2023.112287 ↗
19. Enhanced high-temperature mechanical properties of laser-arc hybrid additive manufacturing of Al-Zn-Mg-Cu alloy via microstructure control10.1016/j.jmst.2023.05.071 ↗
20. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
21. Process and mechanical properties: applicability of a scandium modified al-alloy for laser additive manufacturing10.1016/j.phpro.2011.03.047 ↗
22. An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion
23. Development of a rapid solidification model for additive manufacturing process and application to Al-Si alloy10.1016/j.actamat.2023.119638 ↗
24. High-strength Al–5Mg2Si–2Mg–2Fe alloy with extremely high Fe content for green industrial application through additive manufacturing10.1080/17452759.2023.2235587 ↗
25. Synergy of tensile strength and high cycle fatigue properties in a novel additively manufactured Al-Ni-Ti-Zr alloy with a heterogeneous microstructure
26. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
27. Microstructural evolution and strengthening mechanisms of a high-strength Al-Mg-Si alloy processed by laser powder bed fusion and ageing treatment10.1016/j.matchar.2024.113754 ↗
28. Change in microstructural characteristics of laser powder bed fused Al–Fe binary alloy at elevated temperature10.1016/j.jmst.2021.04.038 ↗
29. Laser powder bed fusion of Al–10 wt% Ce alloys: microstructure and tensile property10.1007/s10853-020-05037-z ↗
30. Research progress on microstructure tuning of heat-resistant cast aluminum alloys10.1016/j.mtnano.2019.100035 ↗
31. Effect of Ag addition on the precipitation evolution and interfacial segregation for Al–Mg–Si alloy10.1016/j.actamat.2019.09.015 ↗
32. Precipitating thermally reinforcement phase in aluminum alloys for enhanced strength at 400 °C10.1016/j.jmst.2023.06.038 ↗
33. Stabilizing nanoprecipitates in Al-Cu alloys for creep resistance at 300°C10.1080/21663831.2018.1546773 ↗
34. A new AlSi7Mg-xSc alloy with high strength and high strain Manufactured by Selective Laser Melting10.1016/j.jmrt.2024.04.123 ↗
35. Superior thermal stability and strength of additively manufactured CoCrFeMnNi high-entropy alloy via NbC decorated sub-micro dislocation cells10.1016/j.scriptamat.2023.115401 ↗
36. Effect of heat treatment on microstructure, mechanical and thermal properties of selective laser melted AlSi7Mg alloy10.1016/j.jallcom.2023.169278 ↗
37. Microstructures and mechanical properties of A356 (AlSi7Mg0.3) aluminum alloy fabricated by selective laser melting10.1016/j.matdes.2015.10.065 ↗
38. The effect of heat treatment on the room and high temperature mechanical properties of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.jmrt.2023.02.086 ↗
39. Effect of heat treatment on the anisotropy in mechanical properties of selective laser melted AlSi10Mg10.1016/j.msea.2022.144130 ↗
40. Microstructural analysis of the influences of platform preheating and post-build heat treatment on mechanical properties of laser powder bed fusion manufactured AlSi10Mg alloy10.1016/j.msea.2023.145486 ↗
41. Study of heat treatment parameters for additively manufactured AlSi10Mg in comparison with corresponding cast alloy10.1016/j.msea.2018.10.026 ↗
42. Microstructure and mechanical properties of Al-12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
43. Enhancement in strength and thermal stability of selective laser melted Al–12Si by introducing titanium nanoparticles10.1016/j.msea.2022.143833 ↗
44. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting10.1016/j.actamat.2016.06.009 ↗
45. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
46. Microstructures and mechanical properties of aluminum-transition metal binary alloys (Al-Fe, Al-Mn, and Al-Cr) processed by laser powder bed fusion10.1016/j.jallcom.2021.159680 ↗
47. Microstructure, tensile properties and thermal stability of AlMgSiScZr alloy printed by laser powder bed fusion10.1016/j.jmst.2020.08.033 ↗
48. Elevated temperature ductility dip in an additively manufactured Al-Cu-Ce alloy10.1016/j.actamat.2021.117285 ↗
49. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
50. Review on the correlation between microstructure and mechanical performance for laser powder bed fusion AlSi10Mg
51. Developing a novel high-strength Al–Mg–Zn–Si alloy for laser powder bed fusion10.1016/j.msea.2022.143636 ↗
52. Strengthening mechanisms in solid solution aluminum alloys10.1007/s11661-006-0142-7 ↗
53. Thermodynamic modelling of growth-restriction effects in aluminium alloys10.1016/j.actamat.2004.11.024 ↗
54. Demonstrating the roles of solute and nucleant in grain refinement of additively manufactured aluminium alloys
55. Insight into the mechanisms of columnar to equiaxed grain transition during metallic additive manufacturing
56. Mechanical and thermal properties of in situ AlN/Al-12Si composite fabricated by laser powder bed fusion10.1016/j.matchar.2024.113825 ↗
57. Pinning effect of second-phase particles on grain growth in polycrystalline films studied by 3-D phase field simulations10.1016/j.actamat.2006.11.018 ↗
58. A high Fe-containing AlSi12 alloy fabricated by laser powder bed fusion10.1016/j.jmrt.2022.04.008 ↗
59. Compositional regulation in additive manufacturing of precipitation-hardening (CoCrNi)94Ti3Al3 medium-entropy superalloy: cellular structure stabilization and strength enhancement10.1016/j.compositesb.2024.111570 ↗
60. Robust additive manufacturable Ni superalloys designed by the integrated optimization of local elemental segregation and cracking susceptibility criteria10.1016/j.actamat.2024.119658 ↗
61. Toward the superior high-temperature strength of Al-5Fe alloy for powder bed fusion-laser beam: stabilizing Al6Fe nanoprecipitate by Sc and Zr elements10.1016/j.msea.2024.146351 ↗
62. Coarsening behavior of Al3Sc interface precipitates and related impact on mechanical properties of AlFeNi-Sc alloy at 400 °C10.1016/j.msea.2023.145189 ↗
63. Die-cast multicomponent near-eutectic and hypoeutectic Al–Si–Ni–Fe–Mn alloys: microstructures and mechanical properties10.1016/j.msea.2023.144977 ↗
64. Segregation engineering of grain boundaries of a metastable Fe-Mn-Co-Cr-Si high entropy alloy with laser-powder bed fusion additive manufacturing
65. Role of dislocation elastic field on impurity segregation in Fe-based alloys10.1038/s41598-020-80140-4 ↗
66. Solute trapping and non-equilibrium microstructure during rapid solidification of additive manufacturing10.1038/s41467-023-43563-x ↗
67. Mechanical property and cellular structure of an additive manufactured FeCoNiCrMo0.2 high-entropy alloy at high-velocity deformation10.1016/j.jmst.2022.08.013 ↗
68. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
69. Effect of heat treatment on the microstructure and mechanical properties of an Al-5Mg2Si-2Mg alloy processed by laser powder bed fusion10.1016/j.jallcom.2022.165944 ↗
70. Blocking of Ostwald ripening allowing long-term stabilization
71. Solute repositioning to tune the multiple microalloying effects in an Al–Cu alloy with minor Sc, Fe and Si addition
72. Solute-vacancy clustering in aluminum10.1016/j.actamat.2020.06.062 ↗
73. Roles of different Ni-Si interactions in methane combustion under oscillating temperature conditions10.1016/j.jcis.2024.04.184 ↗
74. Mechanisms for stabilizing θ′(Al2Cu) precipitates at elevated temperatures investigated with phase field modeling10.1016/j.mtla.2019.100335 ↗
75. Enhancement in strength and thermal stability of selective laser melted Al-12Si by introducing titanium nanoparticles10.1016/j.msea.2022.143833 ↗
76. Selective laser melting of a novel Al-Si-Fe-Mn-Ni alloy with superior mechanical properties at both room and elevated temperatures: influence of processing parameters and heat treatment10.1016/j.matchar.2024.114098 ↗
77. Role of hierarchical microstructure of additively manufactured AlSi10Mg on dynamic loading behavior
78. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: Comparison between virgin and recycled powders
79. Comparative investigation of microstructure, mechanical properties and strengthening mechanisms of Al-12Si/TiB2 fabricated by selective laser melting and hot pressing10.1016/j.ceramint.2018.06.225 ↗
80. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: Crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
81. A new crystal plasticity framework to simulate the large strain behaviour of aluminum alloys at warm temperatures10.1016/j.msea.2018.04.020 ↗
82. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
83. On the thermal stability of dislocation cellular structures in additively manufactured austenitic stainless steels: roles of heavy element segregation and stacking fault energy10.1007/s11837-020-04427-7 ↗
84. Design materials based on simulation results of silicon induced segregation at AlSi10Mg interface fabricated by selective laser melting10.1016/j.jmst.2020.01.037 ↗
85. Reducing hot tearing by grain boundary segregation engineering in additive manufacturing: example of an AlxCoCrFeNi high-entropy alloy10.1016/j.actamat.2020.116505 ↗
86. New alloy design approach to inhibiting hot cracking in laser additive manufactured nickel-based superalloys10.1016/j.actamat.2023.118736 ↗