The selection of scanning strategy and annealing schedule for the optimization of texture and magnetic properties of Fe-3.5 wt%Si alloy parts fabricated by laser powder bed fusion

Fanbo Meng, Konstantinos A. Liogas, Kwang Boon Lau, Yuheng Deng, Alexander M. Korsunsky, Pei Wang, Xiaojun Shen, Christopher H.T. Lee

Abstract

By careful selection of the scanning strategies (SS), researchers in this study were able to realize a simple algorithm to control the grain orientation with the extremely strong Rotated Cube and Cube texture obtained in laser powder bed fusion (LPBF) fabricated electrical steel. Microstructure was characterized by optical microscopy (OM) and electron backscatter diffraction (EBSD), and quasi-static magnetic properties were measured through DC closed magnetic circuit method. The findings show that sufficient remelting with a stable thermal field induces a strong < 001 > parallel to the building direction (BD) texture by promoting epitaxial growth aligned with BD. In-plane grain orientation rotates from < 011 > //X-axis towards < 001 > //X-axis (X-/Y-axis denote length/width directions of samples, respectively) with the reduction of the track length. By promoting < 001 > //BD and < 001 > //X-axis textures, double scanning introduced a strong Cube texture in the D-XY samples (double scan along X-axis and Y-axis successively in one layer). Sample heat treatment (HT) considered in this study only induced abnormal grain growth. Coarse grains and desirable texture components contribute to improving permeability during magnetization of domain wall displacement and rotation of the magnetization vector, respectively, and coarse grains also reduce coercivity (H c ). Benefitting from corresponding microstructure, D-XY samples annealed at 1000℃ for 2 h exhibited the highest maximum relative permeability (μ rmax ) of 4450, while S-X samples (single scan along X-axis) annealed at 1150℃ for 4 h showed the highest initial permeability (μ i ) of 0.34 mH/m and lowest H c of 44.5 A/m in this study. This study provides an insight into the relationship between the manufacturing route, microstructure, and magnetic properties of LPBFed electrical steel and establishes a firm basis for controlling the texture components and grain morphology of Fe-3.5 wt%Si via judicious selection of SS and HT.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (72)

Show source-provided references
1. Soft magnetic material status and trends in electric machines10.1109/TIE.2016.2613844 ↗
2. Review of Fe-6.5 wt%Si high silicon steel—a promising soft magnetic material for sub-kHz application10.1016/j.jmmm.2019.02.089 ↗
3. Additive manufacturing of soft magnets for electrical machines—a review
4. Additive manufacturing of magnetic materials10.1016/j.pmatsci.2020.100688 ↗
5. Magnetic properties of metals and alloys
6. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
7. Soft magnetic materials10.1109/5.56909 ↗
8. A comprehensive review of additive manufacturing in construction of electrical machines10.1109/TEC.2020.2964942 ↗
9. Additive manufacturing and topology optimization of magnetic materials for electrical machines—a review10.3390/en14020283 ↗
10. New trends in electric motors and selection for electric vehicle propulsion systems10.1049/els2.12018 ↗
11. Toward additively manufactured electrical machines: opportunities and challenges10.1109/TIA.2019.2960250 ↗
12. Y. Zhou, J. Liu, F. Meng, G. Yang, Y. He, D.K.B. Lau, P. Wang, C.H.T. Lee, Design of an Axial-Flux Synchronous Reluctance Machine with 3D-Printed Rotor, in: 2023 IEEE International Electric Machines & Drives Conference (IEMDC), IEEE, San Francisco, CA, USA, 2023: pp. 1–7. https://doi.org/10.1109/IEMDC55163.2023.10238945.10.1109/IEMDC55163.2023.10238945 ↗
13. Grain size dependence of coercivity and permeability in nanocrystalline ferromagnets10.1109/20.104389 ↗
14. Grain structure and magnetism of nanocrystalline ferromagnets10.1109/20.42292 ↗
15. Soft magnetic nanocrystalline materials10.1016/0956-716X(95)00397-E ↗
16. Anisotropies in soft magnetic nanocrystalline alloys10.1016/j.jmmm.2005.03.020 ↗
17. Effects of grain size distribution on coercivity and permeability of ferromagnets10.1016/j.jmmm.2008.01.004 ↗
18. Overview of microstructure and microtexture development in grain-oriented silicon steel10.1016/j.jmmm.2006.02.116 ↗
19. Microstructure and texture evolution of strip casting 3wt% Si non-oriented silicon steel with columnar structure10.1016/j.jmmm.2011.06.002 ↗
20. Strong cube recrystallization texture in silicon steel by twin-roll casting process10.1016/j.actamat.2014.05.020 ↗
21. Retaining {1 0 0} texture from initial columnar grains in 6.5 wt% Si electrical steels10.1016/j.jmmm.2017.05.092 ↗
22. Effect of hot rolling reduction on microstructure, texture and ductility of strip-cast grain-oriented silicon steel with different solidification structures10.1016/j.msea.2014.03.052 ↗
23. Texture evolution in twin-roll strip cast non-oriented electrical steel with strong Cube and Goss texture10.1016/j.actamat.2020.08.048 ↗
24. Influence of primary annealing condition on texture development in grain oriented electrical steels10.1016/S1359-6454(02)00034-4 ↗
25. Grain misorientations in theories of abnormal grain growth in silicon steel10.1016/S1359-6462(00)00403-6 ↗
26. Influence of neighbourhood on abnormal Goss grain growth in Fe–3% Si steels: formation of island grains in the large growing grain10.1016/j.scriptamat.2006.06.007 ↗
27. Abnormal grain growth induced by cyclic heat treatment10.1126/science.1238017 ↗
28. On abnormal growth of Goss grains in grain-oriented silicon steel10.1016/j.scriptamat.2010.11.013 ↗
29. Precipitates in electrical steels10.1016/j.jmmm.2008.03.062 ↗
30. Abnormal grain growth of Goss grains in Fe–3% Si steel driven by sub-boundary-enhanced solid-state wetting: analysis by Monte Carlo simulation10.1016/j.actamat.2010.04.038 ↗
31. On the growth of abnormal grains10.1016/S1359-6462(96)00501-5 ↗
32. Effects of topology on abnormal grain growth in silicon steel10.1016/S1359-6454(02)00574-8 ↗
33. On the theory of normal and abnormal grain growth10.1016/0001-6160(65)90200-2 ↗
34. Abnormal grain growth development from uniform grain size distributions10.1016/S1359-6454(96)00284-4 ↗
35. Mechanistic approach of Goss abnormal grain growth in electrical steel: theory and argument10.1016/j.actamat.2019.12.023 ↗
36. Texture and microstructure characterizations of Fe-3.5wt%Si soft magnetic alloy fabricated via laser powder bed fusion10.1016/j.matchar.2022.112012 ↗
37. Texture components and magnetic properties of laser powder bed fusion fabricated near grain-oriented and near non-oriented silicon steel10.1016/j.matdes.2023.112037 ↗
38. Additive manufacturing of Fe-6.5 wt%Si transformer steel toroidal cores: process optimization, design aspects, and performance10.1016/j.matdes.2024.112883 ↗
39. Metallurgy of high-silicon steel parts produced using selective laser melting10.1016/j.actamat.2016.03.037 ↗
40. Relationship between laser energy input, microstructures and magnetic properties of selective laser melted Fe-6.9%wt Si soft magnets10.1016/j.matchar.2018.01.016 ↗
41. Effect of annealing on the microstructure and magnetic properties of soft magnetic Fe-Si produced via laser additive manufacturing10.1016/j.scriptamat.2017.08.042 ↗
42. Properties of additively manufactured electric steel powder cores with increased Si content10.3390/ma14061489 ↗
43. Tailoring the microstructure of Fe-2.9wt%Si alloy in laser powder bed fusion using in-source beam shaping10.1016/j.optlastec.2024.110649 ↗
44. Optimizing magnetic performance of Fe–50Ni alloy for electric motor cores through LPBF: a study of as-built and heat-treated scenarios10.1016/j.jmrt.2024.02.011 ↗
45. Critical role of scan strategies on the development of microstructure, texture, and residual stresses during laser powder bed fusion additive manufacturing
46. The effect of laser scanning strategies on texture, mechanical properties, and site-specific grain orientation in selective laser melted 316L SS10.1016/j.matdes.2020.108852 ↗
47. Effect of scanning strategy on texture formation in Ni-25 at%Mo alloys fabricated by selective laser melting10.1016/j.matdes.2017.11.060 ↗
48. Role of scan strategies and heat treatment on grain structure evolution in Fe-Si soft magnetic alloys made by laser-powder bed fusion
49. Fracture behavior of laser powder bed fusion fabricated Ti41Nb via in-situ alloying10.1016/j.actamat.2021.117593 ↗
50. Resolving the porosity-unmelted inclusion dilemma during in-situ alloying of Ti34Nb via laser powder bed fusion10.1016/j.actamat.2020.116522 ↗
51. On the formation of “Fish-scale” morphology with curved grain interfacial microstructures during selective laser melting of dissimilar alloys10.1016/j.actamat.2021.117331 ↗
52. Recrystallization-based grain boundary engineering of 316L stainless steel produced via selective laser melting10.1016/j.actamat.2020.09.015 ↗
53. Fracture and fatigue in additively manufactured metals10.1016/j.actamat.2021.117240 ↗
54. Unnotched fatigue of Inconel 718 produced by laser beam-powder bed fusion at 25 and 600°C10.1016/j.actamat.2021.117565 ↗
55. Finite element analysis of single layer forming on metallic powder bed in rapid prototyping by selective laser processing10.1016/S0890-6955(01)00093-1 ↗
56. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
57. Effect of heat treatment on the microstructure and magnetic properties of laser powder bed fusion processed equiatomic Co-Fe
58. Hiperco_50A_Alloy_(E199).pdf, (n.d.). 〈https://f.hubspotusercontent20.net/hubfs/7407327/carpenter_electrification/Resources/Datasheets/Hiperco_50A_Alloy_〉(E199).pdf (accessed April 24, 2023).
59. Downloads | VAC, (n.d.). 〈https://vacuumschmelze.de/shared/quickNav/Downloads〉 (accessed April 24, 2023).
60. Design and performance of an additively manufactured high-Si transformer core10.1016/j.matdes.2020.108894 ↗
61. Influence of scan pattern and geometry on the microstructure and soft-magnetic performance of additively manufactured Fe-Si
62. Characterization of Fe-6Si soft magnetic alloy produced by laser-directed energy deposition additive manufacturing10.1007/s11837-023-06293-5 ↗
63. Experimental and thermodynamic studies of the Fe–Si binary system10.2355/isijinternational.52.540 ↗
64. Standard Test Method for Direct Current Magnetic Properties of Low Coercivity Magnetic Materials Using Hysteresigraphs, (n.d.). 〈https://www.astm.org/a0773_a0773m-21.html〉 (accessed September 24, 2023).
65. Tertiary grain growth driven by surface energy10.1016/S1359-6462(01)01017-X ↗
66. Effects of heat treatment on the microstructures and magnetic properties of selective laser melted Fe-3 wt%Si functional soft magnet10.1016/j.jallcom.2023.169840 ↗
67. Kou · 2003
68. Alloy design against the solidification cracking in fusion additive manufacturing: an application to a FeCrAl alloy10.1080/21663831.2021.1922945 ↗
69. Magnetic properties and dynamic domain behavior in grain-oriented 3% Si-Fe10.1109/20.486550 ↗
70. High temperature soft magnetic materials: FeCo alloys and composites10.1109/20.908809 ↗
71. The magnetocrystalline anisotropy constants of iron and iron-silicon alloys10.1088/0031-8949/11/6/010 ↗
72. F. Fiorillo, G. Bertotti, C. Appino, M. Pasquale, Soft Magnetic Materials, in: Wiley Encyclopedia of Electrical and Electronics Engineering, John Wiley & Sons, Inc., Hoboken, NJ, USA, 1999: pp. 1–42. https://doi.org/10.1002/047134608X.W4504.pub2.10.1002/047134608X.W4504.pub2 ↗