This article establishes the evolution of mechanical properties across temperatures ranging from ambient to 950°C for additively manufactured (AM) Haynes 214 alloy. Furthermore, it elucidates and discusses the specific temperature threshold at which ductility loss occurs and its correlation with mechanical strength. This study uses a holistic approach by investigating texture evolution, grain boundary crack initiation, and size effects across various temperatures to gain new insights into the deformation mechanisms that contribute to the alloy's macroscopic behavior and ductility loss. To exhibit property evolution as a function of temperature, the macroscopic stress-strain response of Laser Powder Bed Fusion (L-PBF) Haynes 214 from ambient temperature to 950°C is presented. The combined influence of size effect and thermomechanical response is leveraged to present a discussion on the microscopic deformation mechanisms that govern the characteristics of macroscopic response, including the Portevin-Le Châtelier (PLC) effect and ductility loss. The findings of this paper agree with the general notion that the interaction of mobile dislocations and solutes causes strain hardening and the PLC effect up to approximately 650°C. In addition, we found that such a mechanism is replaced by grain boundary cracking when the testing temperature exceeds approximately 600°C, which coincides with negligible slip activities within the grains. This argument is supported by texture analysis from fractured samples at 650°C, where the significant ductility drop coincides with the absence of the PLC effect. Texture analysis of the fractured 650°C samples shows no evidence of texture evolution or grain distortion but rather grain boundary cracking. This contrasts the fractured ambient specimens that exhibit significant texture evolution and grain distortion. When the temperature rises to approximately 870°C, the material experiences further ductility loss combined with significant strength loss. We hypothesize that at temperatures above approximately 900°C, the activation energy of the slip systems becomes considerably low so that the plastic deformation can be accommodated by a combination of slip and grain boundary sliding, thereby regaining some ductility. Another important piece of evidence provided in this article is that experiments were performed for samples with thicknesses varying from 1 to 2.5 mm at ambient, 600°C, 650°C, and 870°C. These are the temperatures at which we observed characteristic changes in the serrated plastic flow, ductility loss, and strength degradation. The data shows that in thinner samples, where smaller grain sizes were recorded and thus a larger relative grain boundary area, the behavior (still showing PLC serrations) departed from that of thicker samples at the same temperature. This departure suggests that grain boundary sliding and dislocation interaction with the precipitates at the grain boundary served as the dominant deformation mechanism in thinner samples, emphasizing the key role of grain boundary-dominated deformation in ductility losses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Alloy digest 35 (1986).
2. Carburization/oxidation behavior of alloy Haynes-214 in methane–hydrogen gas mixtures10.1007/s11085-009-9151-4 ↗
3. Oxidation behaviors of porous Haynes 214 alloy at high temperatures10.1016/j.matchar.2015.07.026 ↗
4. Tensile deformation mechanisms in a new directionally solidified Ni-base superalloy containing coarse γ′ precipitates at 650°C10.1016/j.msea.2017.07.025 ↗
5. Temperature dependence of deformation mechanisms and tensile strength of a new Ni-Fe-base superalloy10.1016/j.matchar.2018.05.032 ↗
6. The influence of coherency strain on the elevated temperature tensile behavior of Ni-15Cr-AI-Ti-Mo alloys10.1007/BF02643569 ↗
7. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties10.2514/1.18239 ↗
8. Reed · 2008
9. Tensile properties and deformation characteristics of a Ni-Fe-base superalloy for steam boiler applications10.1007/s11661-013-1959-5 ↗
10. Intermediate temperature brittleness and directional coarsening behavior of nickel-based single-crystal superalloy DD610.1016/j.matdes.2015.07.063 ↗
11. Temperature dependence of tensile behavior of Ni-based superalloy M95110.1016/j.msea.2008.02.013 ↗
12. Tensile deformation mechanisms at various temperatures in a new directionally solidified Ni-base superalloy10.1016/j.jallcom.2016.09.303 ↗
13. Tensile properties and deformation mechanisms of Haynes 282 at various temperatures10.1007/s11661-018-4515-5 ↗
14. The high-temperature decrease of the yield strength of the γ′-strengthened superalloys nimonic pe16 and nimonic 10510.1016/S0921-5093(03)00593-8 ↗
15. Serrated flow in Ni-C alloys10.1016/0001-6160(70)90129-X ↗
16. On the mechanism of delayed discontinuous plastic flow in an age-hardened nickel alloy10.1016/0001-6160(82)90148-1 ↗
17. On a proposed theory for the disappearance of serrated flow in fcc Ni alloys10.1016/0001-6160(83)90213-4 ↗
18. Oxidation induced intergranular cracking and Portevin–Le Chatelier effect in nickel base superalloy 71810.1016/S0921-5093(01)01224-2 ↗
19. Portevin-Le Châtelier effect in wrought Ni-based superalloys: Experiments and mechanisms10.1016/j.jmst.2020.03.023 ↗
20. Dynamic strain ageing in Ni-base superalloy 720Li10.1016/j.actamat.2008.11.005 ↗
21. Portevin-Le Châtelier effect in a wrought Ni–Co based superalloy10.1016/j.jallcom.2019.152863 ↗
22. Environmentally-assisted grain boundary attack as a mechanism of embrittlement in a nickel-based superalloy10.1016/j.actamat.2016.12.039 ↗
23. ASTM-International, ASTM B214-22, Standard Test Method for Sieve Analysis of Metal Powders, 2022.
24. ASTM-International, ASTM E8/E8M-22, Standard Test Methods for Tension Testing of Metallic Materials, 2022.
25. Additive manufacturing of nickel-based superalloys: A state-of-the-art review on process-structure-defect-property relationship10.1016/j.pmatsci.2023.101108 ↗
26. Gradl · 2022
27. G. Demeneghi, P. Gradl, J.R. Mayeur, K. Hazeli, Size effect characteristics and influences on fatigue behavior of laser powder bed fusion of grcop-42 copper alloy. Available at SSRN 4459393.
28. Texture analysis with MTEX–free and open source software toolbox10.4028/www.scientific.net/SSP.160.63 ↗
29. Size effects on microstructure and mechanical properties of additively manufactured copper–chromium–niobium alloy10.1016/j.msea.2021.141511 ↗
30. Directed energy deposition GRCop-42 copper alloy: Characterization and size effects10.1016/j.matdes.2022.111035 ↗
31. Effects of size, geometry, and testing temperature on additively manufactured Ti-6Al-4V titanium alloy
32. Quantifying the microstructure and mechanical property differences between bulk and thin-wall additively manufactured inconel 71810.1016/j.mtla.2023.101867 ↗
33. Size-dependent stochastic tensile properties in additively manufactured 316l stainless steel
34. On the size and orientation effect in additive manufactured Ti-6Al-4V10.1016/j.matdes.2019.108235 ↗
35. Quantification of porosity and microstructure and their effect on quasi-static and dynamic behavior of additively manufactured Inconel 718
36. Effect of hot isostatic pressing of laser powder bed fused Inconel 625 with purposely induced defects on the residual porosity and fatigue crack propagation behavior
37. Combined effects of porosity and stress state on the failure behavior of laser powder bed fusion stainless steel 316L
38. Spatial inhomogeneity of build defects across the build plate in laser powder bed fusion
39. Geometric feature reproducibility for laser powder bed fusion (L-PBF) additive manufacturing with Inconel 718
40. Characterization of bulk to thin wall mechanical response transition in powder bed AM10.1108/RPJ-10-2015-0146 ↗
41. A defect-resistant Co–Ni superalloy for 3D printing10.1038/s41467-020-18775-0 ↗
42. Microstructure and mechanical properties of Ni-Fe-Cr-Al wrought alumina forming superalloy heat-treated at 600–1100°C10.1016/j.matchar.2020.110737 ↗
43. Temperature-dependent tensile deformation and plasticity loss mechanism of a novel Ni-Cr-W-based superalloy prepared by laser powder bed fusion
44. Mechanical behavior and dynamic strain ageing in Haynes® 282 superalloy subjected to accelerated ageing10.1016/j.msea.2021.142486 ↗
45. Serrated tensile flow in inconel X750 sheets: Effect of heat treatment10.1016/j.msea.2017.08.093 ↗
46. Effects of temperature and strain rate on tensile deformation behavior of superalloy UNS N1027610.1016/j.msea.2017.05.085 ↗
47. Intermediate temperature embrittlement and Portevin-Le Châtelier effect of Inconel 625 alloy caused by carbides
48. Oxidation assisted intergranular cracking under loading at dynamic strain aging temperatures in Inconel 718 superalloy10.1016/j.jallcom.2014.12.279 ↗
49. Oxidation assisted intergranular cracking in 718 Nickel superalloy: on the mechanism of dynamic embrittlement10.1016/j.jmrt.2018.02.008 ↗
50. Effects of γ′ size and carbide distribution on fatigue crack growth mechanisms at 650°C in an advanced Ni-based superalloy10.1016/j.ijfatigue.2020.106086 ↗
51. Microstructural size effects on mechanical properties of high purity nickel10.1016/j.ijplas.2010.08.002 ↗
52. Sikka · 1995
53. Temperature-dependent mechanical properties and crystal plasticity parameters for additively manufactured Haynes-214 alloy: Experiments and numerical modeling