Enhancing ductility of laser powder bed fusion Ti-6Al-4V alloys by molybdenum addition: A study on microstructure and deformation mechanisms
Source abstract
Abstract
The limited ductility of laser powder bed fusion (LPBF) Ti-6Al-4V (Ti64) alloys, caused by their brittle α'-martensitic microstructure, significantly restricts their broader application. This study systematically investigates the influence of Mo additions (0, 1, 3, and 5 wt%) on the microstructure evolution, deformation mechanisms, and mechanical properties of LPBF Ti64 alloys. Incorporation of Mo notably transforms the phase composition from purely α'-martensitic (Ti64 and Ti64–1Mo) to a multi-phase structure containing metastable β and α" phases alongside α' (Ti64–3Mo and Ti64–5Mo). Ti64–3Mo exhibits an optimal balance of mechanical properties, achieving significant improvements in uniform elongation (9.5 %) and maintaining high yield strength (955 MPa). Enhanced ductility in Ti64–3Mo and Ti64–5Mo is attributed to the synergistic activation of multiple deformation mechanisms, including stress-induced martensite transformation in metastable β, and twinning coupled with multiple slip modes in the α' phase. However, early activation of twinning prior to basal slip reduces yield strength. These insights underscore the crucial role of Mo as a compositional modifier, providing a practical approach for engineering strength-ductility combinations in additively manufactured titanium alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
2. Additive manufacturing of metallic components–process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
3. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
4. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
5. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
6. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: a review10.1016/j.ijmachtools.2018.01.003 ↗
7. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
8. Developing ductile and isotropic ti alloy with tailored composition for laser powder bed fusion
9. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
10. High ductility in a fully martensitic microstructure: a paradox in a ti alloy produced by selective laser melting10.1080/21663831.2018.1525773 ↗
11. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
12. Design of titanium alloys by additive manufacturing: a critical review
13. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
14. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
15. Enhanced strength-ductility synergy and mechanisms of heterostructured Ti6Al4V-Cu alloys produced by laser powder bed fusion10.1016/j.actamat.2023.119112 ↗
16. Recent innovations in laser additive manufacturing of titanium alloys10.1088/2631-7990/ad2545 ↗
17. The interdependence theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
18. Controlling the microstructure and properties of wire arc additive manufactured Ti–6Al–4V with trace boron additions10.1016/j.actamat.2015.03.035 ↗
19. Grain refinement of alloys in fusion-based additive manufacturing processes10.1007/s11661-020-05880-4 ↗
20. A review of metastable beta titanium alloys10.3390/met8070506 ↗
21. The mo− ti (molybdenum-titanium) system10.1007/BF02881476 ↗
22. Titanium matrix composites
23. Effect of β-stabilizer elements on stacking faults energies and ductility of α-titanium using first-principles calculations10.1063/1.4966939 ↗
24. Simultaneously enhancing strength and ductility of LPBF ti alloy via trace Y2O3 nanoparticle addition10.1016/j.jmst.2024.01.011 ↗
25. GSAS-II: the genesis of a modern open-source all purpose crystallography software package10.1107/S0021889813003531 ↗
26. Ab initio molecular dynamics for liquid metals10.1016/0022-3093(95)00355-X ↗
27. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
28. Theoretical study of the effects of alloying elements on cu nanotwins10.1007/s11433-020-1543-8 ↗
29. A first principles investigation of zinc induced embrittlement at grain boundaries in bcc iron10.1016/j.actamat.2015.02.018 ↗
30. The influence of alloying on zn liquid metal embrittlement in steels10.1016/j.actamat.2020.06.001 ↗
31. Achieving superior strength-ductility combination in the heterogeneous microstructured Ti64 alloy via multi-eutectoid elements alloying with CoCrFeNiMn during laser powder bed fusion10.1080/17452759.2024.2375106 ↗
32. Parent grain reconstruction from partially or fully transformed microstructures in MTEX10.1107/S1600576721011560 ↗
33. Effects of cr and fe addition on microstructure and tensile properties of Ti–6Al–4V prepared by direct energy deposition10.1007/s12540-018-0148-x ↗
34. Evolution of lattice strain in Ti–6Al–4V during tensile loading at room temperature10.1016/j.actamat.2008.08.030 ↗
35. Twinning–detwinning behavior during the strain-controlled low-cycle fatigue testing of a wrought magnesium alloy, ZK60A10.1016/j.actamat.2007.10.030 ↗
36. Study of the mechanical properties of Mg-7.7 at% al by in-situ neutron diffraction10.1080/01418619908210386 ↗
37. Twinning and detwinning during cyclic deformation of mg alloy AZ31B
38. Phase stability and stress-induced transformations in beta titanium alloys10.1007/s11837-015-1411-y ↗
39. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
40. Reorientation induced plasticity in full α″ martensite Ti-9V-1Fe-4Al alloy10.1016/j.msea.2024.146870 ↗
41. Deformation twinning in the full-α ″martensitic Ti–25Ta–20Nb shape memory alloy10.1016/j.actamat.2015.12.001 ↗
42. Improved mechanical properties of β metastable ti alloys processed by laser powder bed fusion10.1016/j.msea.2023.145755 ↗
43. On the design of new β-metastable titanium alloys with improved work hardening rate thanks to simultaneous TRIP and TWIP effects10.1016/j.scriptamat.2012.01.049 ↗
44. Beta titanium alloys and their role in the titanium industry10.1007/BF03220742 ↗
45. Microstructures and properties of titanium alloys Ti-Mo for dental use10.1016/S1003-6326(06)60308-7 ↗
46. Martensitic transformations in Ti-Mo alloys10.1007/BF00772735 ↗
47. Study on the relationship between microstructure and mechanical property in a metastable β titanium alloy10.1016/j.jallcom.2014.12.100 ↗
48. Age-hardening behaviour of two metastable beta-titanium alloys10.1016/j.msea.2010.07.055 ↗
49. Mechanism of twinning-induced plasticity in β-type Ti–15Mo alloy10.1016/j.scriptamat.2013.05.027 ↗
50. Effects of mo concentration on recrystallization texture, deformation mechanism and mechanical properties of Ti–Mo binary alloys10.1016/j.jallcom.2019.153508 ↗
51. Relationship between phase stability and mechanical properties on near/metastable β-type Ti–Cr-(Mn) cast alloys10.1016/j.jallcom.2019.153516 ↗
52. Effect of nb content on the microstructure and mechanical properties of binary Ti-Nb alloys10.1016/j.matpr.2020.05.315 ↗
53. Deformation characteristics in β phase Ti-Nb alloys10.1007/BF02814829 ↗
54. The effect of molybdenum content on the microstructural evolution and tensile properties of as-cast Ti-Mo alloys
55. Dependence of stress-induced omega transition and mechanical twinning on phase stability in metastable β Ti–V alloys10.1016/j.matchar.2015.06.038 ↗
56. Effect of plastic deformation modes on tensile properties of beta titanium alloys10.2320/matertrans1960.27.496 ↗
57. Deformation behaviour of retained β phase in β-eutectoid Ti-Cr alloys10.1007/BF01106518 ↗
58. Effect of α ″martensite on the microstructure and mechanical properties of beta-type Ti–Fe–Ta alloys10.1016/j.matdes.2015.03.028 ↗
59. The improved strength and fracture mechanism of additive manufactured Ti-6Al-4 v alloys compared with corresponding as-rolled alloys10.1557/s43578-023-01278-1 ↗
60. Strength enhancement of a bi-lamellar PM Ti–6Al–4V alloy without sacrificing ductility by al partitioning and twinning-induced plasticity effect10.1016/j.msea.2021.142368 ↗