Oxidation behavior of the directed energy deposited 316L stainless steel in supercritical carbon dioxide environment: Effect of post-manufacturing heat treatment
Source abstract
Abstract
The oxidation behaviors of directed energy deposit (DED) 316L SS with various post-DED heat treatments (HTs) as well as commercial 316L SS were investigated in a 650 ℃/20 MPa sCO2 environment. In addition to the detailed microstructure analyses, ultraviolet photoelectron spectroscopy (UPS) analysis was performed to measure the valence electron configuration, and the results were considered in understanding the observed oxidation behavior. Compared to commercial 316L SS, the unique large columnar grains and decrease in valence electron density of DED 316L SS benefit the oxidation resistance by retarding cation and anion migrations, even though they have similar oxide layer consisting of a Fe-rich outer oxide layer and a Cr- and Fe-rich internal oxidation zone. After stress-relieving HT at 850 ℃, the oxidation resistance is further enhanced owing to the HT-induced dislocation density decrease, resulting in a thinner sandwich-like oxide layer with chromia-type outer and inner sublayers and a silicon oxide middle sublayer. Additional improvement in the oxidation resistance is observed after homogenization HT at 1150 °C, with a thinner oxide layer and less inward intergranular oxidation, which could be attributed to an additional decrease in valence electron density.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Entropy Alloys Studies · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Additive manufacturing for energy: a review10.1016/j.apenergy.2020.116041 ↗
2. Additive manufacturing of structural materials
3. Additive manufacturing in the nuclear reactor industry
4. Localised electrochemical processes on laser powder bed fused 316 stainless steel with various heat treatments in high-temperature water
5. Oxide inclusions in laser additive manufactured stainless steel and their effects on impact toughness and stress corrosion cracking behavior10.1016/j.jnucmat.2017.11.036 ↗
6. On the stress corrosion crack growth behaviour in high temperature water of 316L stainless steel made by laser powder bed fusion additive manufacturing10.1016/j.corsci.2017.09.017 ↗
7. Compositionally graded specimen made by laser additive manufacturing as a high-throughput method to study radiation damages and irradiation-assisted stress corrosion cracking10.1016/j.jnucmat.2021.153493 ↗
8. Investigation of the irradiation effects in additively manufactured 316L steel resulting in decreased irradiation assisted stress corrosion cracking susceptibility10.1016/j.jnucmat.2020.152739 ↗
9. Radiation damage and irradiation-assisted stress corrosion cracking of additively manufactured 316L stainless steels10.1016/j.jnucmat.2018.10.044 ↗
10. Corrosion fatigue crack growth of laser additively-manufactured 316L stainless steel in high temperature water10.1016/j.corsci.2017.08.023 ↗
11. Effects of heat treatment on corrosion fatigue and stress corrosion crack growth of additive-manufactured Alloy 800H in high-temperature water10.1016/j.corsci.2021.109739 ↗
12. Advanced manufacturing for nuclear energy10.1007/s11837-019-03607-4 ↗
13. Structural analysis of compact heat exchanger samples fabricated by additive manufacturing10.1016/j.ijpvp.2022.104714 ↗
14. Corrosion of structural materials for advanced supercritical carbon- dioxide brayton cycle
15. The performance of additively manufactured Haynes 282 in supercritical CO210.1016/j.msea.2022.143007 ↗
16. Initial stages of oxide growth on AM stainless steel exposed to a supercritical CO2 environment10.1016/j.corsci.2022.110259 ↗
17. Enhanced pitting resistance of directed energy deposition 316L stainless steel by post-manufacturing heat treatment10.1038/s41529-022-00237-1 ↗
18. Effect of heat treatment on corrosion behaviour of additively manufactured 316L stainless steel in high-temperature water10.1016/j.corsci.2022.110830 ↗
19. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
20. Corrosion and carburization behavior of Al-rich surface layer on Ni-base alloy in supercritical-carbon dioxide environment10.1016/j.apsusc.2015.11.162 ↗
21. Effect of matrix grain size on the oxidation and carburization resistance of alloy 800HT in high temperature CO2 environment
22. Characterization of alloy 600 joints exposed to a high-temperature supercritical-carbon dioxide environment10.1016/j.matchar.2018.02.025 ↗
23. Corrosion and carburization behaviour of Ni-xCr binary alloys in a high-temperature supercritical-carbon dioxide environment10.1007/s11085-017-9811-8 ↗
24. Corrosion behaviors of four stainless steels with similar chromium content in supercritical carbon dioxide environment at 650 °C10.1016/j.corsci.2019.04.043 ↗
25. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C10.1016/j.corsci.2020.108843 ↗
26. Supercritical-CO2 corrosion behavior of alumina- and chromia-forming heat resistant alloys with Ti10.1016/j.corsci.2021.109531 ↗
27. The carburization behavior of alloy 800HT in high temperature supercritical-CO210.1016/j.matlet.2021.130067 ↗
28. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
29. B. Beausir, J.-J. Fundenberger, Analysis Tools for Electron and X-ray diffraction, ATEX - software, 〈www.atex-software.eu〉, (2017).
30. Influence of the energy density for selective laser melting on the microstructure and mechanical properties of stainless steel10.3390/met10070919 ↗
31. On the limitations of volumetric energy density as a design parameter for selective laser melting10.1016/j.matdes.2016.10.037 ↗
32. Variation of texture anisotropy and hardness with build parameters and wall height in directed-energy-deposited 316L steel
33. The high-temperature oxidation of bulk nanocrystalline 304 stainless steel in air10.1016/j.corsci.2013.03.008 ↗
34. Enhanced localized and uniform corrosion resistances of bulk nanocrystalline 304 stainless steel in high-concentration hydrochloric acid solutions at room temperature10.1016/j.jmst.2018.06.006 ↗
35. The electronic structure characterization of oxide film on bulk nanocrystalline 304 stainless teel in hydrochloric acid solution10.1016/j.electacta.2013.09.001 ↗
36. Synchronous optimization of strengths, ductility and corrosion resistances of bulk nanocrystalline 304 stainless steel10.1016/j.jmst.2019.05.073 ↗
37. Effect of surface conditions and alloying elements on the early oxidation behaviour of two austenitic alloys in the pure steam environment10.1016/j.apsusc.2021.150314 ↗
38. Corrosion behaviors of heat-resisting alloys in high temperature carbon dioxide10.3390/ma15041331 ↗
39. Mechanical and corrosion response of 316SS in Supercritical CO210.1007/s11085-021-10026-x ↗
40. Alloys SS316 and Hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
41. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
42. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
43. Corrosion of materials in supercritical carbon dioxide environments
44. Initial oxidation and chromium diffusion. I. Effects of surface working on 9–20% Cr steels10.1016/j.corsci.2003.09.004 ↗
45. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
46. Grain-size effects on the high-temperature oxidation behaviour of chromium steels10.1007/s11085-010-9192-8 ↗
47. The effect of grain size on the corrosion behaviour of inconel 600 in high-temperature steam10.1016/0010-938X(81)90024-X ↗
48. Mechanisms of oxidation
49. Formation of protective oxide film on chromium-depleted stainless steel10.1179/msc.1981.15.6.267 ↗
50. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
51. Calculation of diffusion penetration curves for surface and grain boundary diffusion10.1063/1.1699825 ↗
52. Diffusion along grain boundaries and dislocations in oxides, alkali halides and carbides10.1016/0167-2738(84)90160-7 ↗
53. Grain-boundary diffusion
54. Corrosion behavior of stainless steels in simulated PWR primary water: the effect of composition and matrix phases10.1016/j.corsci.2020.108991 ↗
55. Corrosion mechanisms of 316L stainless steel in supercritical water: the significant effect of work hardening induced by surface finishes10.1016/j.corsci.2019.05.014 ↗
56. On the influence of cold work on the oxidation behavior of some austenitic stainless steels: high temperature oxidation10.1007/BF00656836 ↗
57. The electrochemical corrosion characterization of bulk nanocrystalline aluminium by X-ray photoelectron spectroscopy and ultra-violet photoelectron spectroscopy10.1016/j.jelechem.2014.04.014 ↗
58. The electrochemical corrosion of bulk nanocrystalline ingot iron in HCl solutions with different concentrations10.1016/j.matchemphys.2011.02.035 ↗