journal article·2018-12

Microstructure characterization and grain morphology of alloy 625 with 0.4 wt% boron modification manufactured by laser wire deposition

Y. Tian, N. Chekir, X. Wang, A. Nommeots-Nomm, R. Gauvin, M. Brochu

Publisher page

Abstract

Abstract Laser wire deposits using Alloy 625 modified with 0.4 wt% B were manufactured on stainless steel 304 substrates. A layer boundary with a thickness of around 250 μm was formed between the layer cores during deposition. Results show that the solidification features in the layer boundary were coarser than the layer core due to the recalescence mechanism. Continuous eutectics were observed segregating the inter-dendritic regions in both the layer boundary and the layer core. The eutectics consisted of mainly Laves phase with a small amount of NbC precipitates. Solidification front velocities (SFV) were calculated from the Kurz-Giovanola-Trivedi (KGT) model. Results showed that they developed in the layer boundary and in the layer core at 0.06 m/s and 0.1 m/s respectively. Electron backscattered diffraction (EBSD) mapping revealed that small equiaxed grains nucleated in the layer boundary, while large columnar grains were prevalent in the layer core. Pole figures showed a strong oriented texture was present along the (100) plane. The columnar to equiaxed transition (CET) model developed by Hunts was considered and the results were in good agreement with the observed grain morphologies.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. The welding and solidification metallurgy of Alloy 625
2. Valencia · 1997 · 753
3. V.S. Senthil Kumar, microstructural evolution of hydroformed inconel 625 bellows10.1016/j.jallcom.2016.02.011 ↗
4. Potential of direct metal deposition technology for manufacturing thick functionally graded coatings and parts for reactors components10.1016/j.jnucmat.2008.11.023 ↗
5. Fatigue behavior of laser consolidated IN-625 at room and elevated temperatures10.1016/j.msea.2009.03.056 ↗
6. Effect of precipitation on post-heat-treated Inconel 625 alloy after friction stir welding10.1016/j.matdes.2009.12.020 ↗
7. Fatigue and fracture toughness characteristics of laser rapid manufactured Inconel 625 structures10.1016/j.msea.2010.08.034 ↗
8. The effect of post-weld heat treatment temperature on the microstructure of Inconel 625 deposited metal10.1016/j.jallcom.2013.12.224 ↗
9. Long pulse laser wire deposition of hard steels10.1016/j.phpro.2016.08.074 ↗
10. Laser aided direct metal deposition of Inconel 625 superalloy: microstructural evolution and thermal stability10.1016/j.msea.2009.01.009 ↗
11. A parametric study of Inconel 625 wire laser deposition10.1016/j.jmatprotec.2013.06.007 ↗
12. Laser cladding of Inconel 625 wire for corrosion protection10.1016/j.jmatprotec.2014.10.024 ↗
13. In situ monitoring and characterization of distortion during laser cladding of Inconel® 62510.1016/j.jmatprotec.2014.12.029 ↗
14. Microstructure characteristics of inconel 625 superalloy manufactured by selective laser melting10.1016/j.jmst.2014.09.020 ↗
15. Effect of filler alloys on heat-affected zone cracking in preweld heat-treated IN-738 LC gas-tungsten-arc welds10.1007/s11661-005-0051-1 ↗
16. Laser engineered net shape (LENS) technology for the repair of Ni-Base superalloy turbine components10.1007/s11661-014-2397-8 ↗
17. DuPont · 2009
18. Weldability Studies of High-Cr, Ni-Base filler metals for power generation applications10.1007/BF03321288 ↗
19. Microstructure evolution of Inconel 625 with 0.4 wt% boron modification during gas tungsten arc deposition10.1016/j.jallcom.2016.10.019 ↗
20. Rationalization of microstructure heterogeneity in INCONEL 718 builds made by the direct laser additive manufacturing process10.1007/s11661-014-2370-6 ↗
21. Microstructural morphology and evolution of austenite stainless steel deposited using pulsed laser and wire10.1007/s00170-017-0625-2 ↗
22. Effect of heat treatments on microstructure evolution and mechanical properties of blended nickel-based superalloys powders fabricated by laser powder deposition10.1016/j.msea.2016.07.116 ↗
23. CASINO V2.42—a fast and easy-to-use modeling tool for scanning Electron microscopy and microanalysis users10.1002/sca.20000 ↗
24. Schneider · Nat. Methods · 2012 · 9 · 67110.1038/nmeth.2089 ↗
25. A. E1951, Standard Guide for Calibrating Reticles and Light Microscope Magnifications, 2014 Edition.
26. Microstructure evolution and rapid solidification behavior of blended nickel-based superalloy powders fabricated by laser powder deposition10.1007/s11661-016-3505-8 ↗
27. Additive manufacturing of Al-12Si alloy via pulsed selective laser melting10.1007/s11837-014-1272-9 ↗
28. Solidification of an alloy 625 weld overlay10.1007/BF02595452 ↗
29. Kou · 2003 · 37
30. Chapter 2 - crystallization processes
31. Theory of microstructural development during rapid solidification10.1016/0001-6160(86)90056-8 ↗
32. Dendrite growth at the limit of stability: tip radius and spacing10.1016/0001-6160(81)90082-1 ↗
33. Search for a solute-drag effect in dendritic solidification10.1016/0956-7151(94)90291-7 ↗
34. Study of the fusion zone and heat-affected zone microstructures in tungsten inert gas-welded INCONEL 738LC superalloy10.1007/s11661-006-0013-2 ↗
35. Microstructural Architecture, Microstructures, and Mechanical Properties for a Nickel-Base Superalloy Fabricated by Electron Beam Melting10.1007/s11661-011-0748-2 ↗
36. Microstructural and texture development in direct laser fabricated IN71810.1016/j.matchar.2013.12.012 ↗
37. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
38. Effect of growth rate and composition on the primary spacing, the dendrite tip radius and mushy zone depth in the directionally solidified succinonitrile–Salol alloys10.1016/S0022-0248(03)01214-4 ↗
39. Homogeneous crystal nucleation in binary metallic melts10.1016/0001-6160(83)90019-6 ↗
40. Grain refinement of aluminium and its alloys by heterogeneous nucleation and alloying10.1179/095066001225001049 ↗