Formation mechanisms of Sn-rich δ phase and its role in strengthening Cu-10Sn manufactured by laser powder bed fusion
Source abstract
Abstract
Cu-Sn alloys produced via laser powder bed fusion (L-PBF) additive manufacturing (AM) have gained significant attention because they combine the advantages of AM relevant to intricate component design with outstanding combinations of strength, ductility, and resistance to wear and corrosion. However, a detailed understanding of the microstructure that contributes to the enhancement of the mechanical properties of L-PBF Cu-10Sn alloys remains unclear. In particular, there is a lack of understanding of the formation mechanisms of the Sn-rich δ phase commonly observed in Cu-10Sn. This study reveals two distinct variants of the δ phase possessing unique morphological characteristics. These characteristics are attributed to the local solidification conditions inherent to the melt pool boundaries versus those at the interiors of melt pools. A phase transformation pathway that elucidates the origin of the morphological variants of the δ phase from the Sn-rich metastable phases during the cyclic heating of the AM process is proposed. We report superior mechanical properties in L-PBF Cu-10Sn compared to those of conventionally manufactured counterparts due to the synergistic contributions from grain boundaries, dislocations, and the δ phase. Notably, the δ phase alone contributes approximately 22% to the overall strength observed in the L-PBF Cu-10Sn alloy. The discovery of two types of distinct Sn-rich δ phase offers key insights into precise microstructural control in AM Cu-Sn alloys to enhance mechanical properties, providing practical strategies for improving material performance for diverse applications in automotive, aerospace, and machinery industries.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Advanced materials and composites · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. Use of metals in our society
2. Ayres · 2013
3. M. Bragagni, L. Xhaferraj, Copper and our sustainable future, 2021, available at 0.13140/RG.2.2.26384.53762.
4. Redesigning a reaction control thruster for metal-based additive manufacturing: a case study in design for additive manufacturing10.1115/1.4037250 ↗
5. Metal additive manufacturing in aerospace: a review10.1016/j.matdes.2021.110008 ↗
6. A. Jawad Qureshi, Large-scale metal additive manufacturing: a holistic review of the state of the art and challenges10.1080/09506608.2021.1971427 ↗
7. Additive manufacturing technology for porous metal implant applications and triple minimal surface structures: a review
8. An overview of additive manufacturing technologies—a review to technical synthesis in numerical study of selective laser melting10.3390/ma13173895 ↗
9. Functionally graded materials with grain-size gradients and heterogeneous microstructures achieved by additive manufacturing10.1016/j.scriptamat.2022.115197 ↗
10. Unique microstructure evolution of a novel Ti-modified Al-Cu alloy processed using laser powder bed fusion
11. In-situ alloying of stainless steel 316L by co-inoculation of Ti and Mn using LPBF additive manufacturing: Microstructural evolution and mechanical properties10.1016/j.msea.2022.144114 ↗
12. The role of texturing and microstructure evolution on the tensile behavior of heat-treated Inconel 625 produced via laser powder bed fusion10.1016/j.msea.2019.138500 ↗
13. Effect of cyclic rapid thermal loadings on the microstructural evolution of a CrMnFeCoNi high-entropy alloy manufactured by selective laser melting10.1016/j.actamat.2020.07.006 ↗
14. On the microstructure and texture evolution in 17-4 PH stainless steel during laser powder bed fusion: towards textural design10.1016/j.jmst.2021.12.015 ↗
15. Layer-wise engineering of grain orientation (LEGO) in laser powder bed fusion of stainless steel 316L
16. Application of single pan thermal analysis to Cu–Sn peritectic alloys10.1016/j.actamat.2007.12.006 ↗
17. A DSC analysis of thermodynamic properties and solidification characteristics for binary Cu–Sn alloys10.1016/j.actamat.2012.08.013 ↗
18. Additive manufacturing of Cu–10Sn bronze10.1016/j.matlet.2015.05.076 ↗
19. Mechanical, thermal, and corrosion properties of Cu-10Sn alloy prepared by laser-powder-bed-fusion additive manufacturing
20. Novel precipitation and enhanced tensile properties in selective laser melted Cu-Sn alloy10.1016/j.mtla.2020.100861 ↗
21. Processing optimisation, mechanical properties and microstructural evolution during selective laser melting of Cu-15Sn high-tin bronze10.1016/j.msea.2018.02.051 ↗
22. Investigation of selective laser melting process for Cu-5Sn alloy on surface roughness, microstructure and mechanical property10.1108/RPJ-12-2020-0307 ↗
23. Implication of peritectic composition in historical high-tin bronze metallurgy10.1016/j.matchar.2009.05.009 ↗
24. The Cu–Sn phase diagram, Part I: new experimental results10.1016/j.intermet.2012.10.004 ↗
25. Strength of joints produced by transient liquid phase bonding in the Cu–Sn system10.1016/j.actamat.2005.01.013 ↗
26. Microstructural characteristics and mechanical properties of additively manufactured Cu–10Sn alloys by laser powder bed fusion10.1016/j.msea.2022.142775 ↗
27. Phase and microstructure formation in rapidly solidified Cu-Sn and Cu-Sn-Ti alloys10.1016/j.jallcom.2017.11.237 ↗
28. Chapter 7-database for the microstructure of plated films
29. Microstructural morphology and phase structure of rapidly solidified Cu-Sn alloy
30. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
31. GSAS-II: the genesis of a modern open-source all-purpose crystallography software package10.1107/S0021889813003531 ↗
32. Phase transformations and microstructural development in the U-10 wt pct Mo alloy with varying Zr contents after heat treatments relevant to the monolithic fuel plate fabrication process10.1007/s11661-018-4987-3 ↗
33. Williams · 1996
34. Gault · 2012
35. 8. Standard test methods for tension testing of metallic materials
36. 92. Standard test methods for Vickers hardness and Knoop hardness of metallic materials
37. 99. Standard test method for wear and friction testing with a pin-on-disk or ball-on-disk apparatus
38. Effect of tin content and ECAP passes on the mechanical properties of Cu/Sn alloys
39. Comparison of wear and mechanical properties of cast and 3D printed CuSn10 bronze alloy10.1515/mt-2022-0443 ↗
40. Effects of Sn content and hot deformation on microstructure and mechanical properties of binary high Sn content Cu–Sn alloys10.1016/j.msea.2020.140054 ↗
41. Microstructure and mechanical properties of pure copper manufactured by selective laser melting10.1016/j.msea.2020.139615 ↗
42. Mechanical and electrical properties of selective laser-melted parts produced from surface-oxidized copper powder
43. Study on the selective laser melting of CuSn10 powder10.3390/ma11040614 ↗
44. Processing technologies and properties of Cu-10Sn formed by selective laser melting combined with heat treatment, 3
45. Selective laser melting of Cu–10Sn–0.4 P: Processing, microstructure, properties, and brief comparison with additively manufactured Cu–10Sn10.1002/adem.202100716 ↗
46. Study of the microstructure and mechanical properties of Cu–Sn alloys formed by selective laser melting with different Sn contents10.1016/j.jmrt.2023.04.198 ↗
47. Mechanical and electrical properties of selective laser-melted parts produced from surface-oxidized copper powder
48. Manufacturing of high strength and high conductivity copper with laser powder bed fusion10.1038/s41467-024-45732-y ↗
49. Enhanced strengthening and hardening via self-stabilized dislocation network in additively manufactured metals10.1016/j.mattod.2021.06.002 ↗
50. Laser-based powder bed fusion additive manufacturing of pure copper
51. Additive manufacturing of copper alloys: influence of process parameters and alloying elements10.1080/02670836.2019.1600840 ↗
52. In-situ synthesis via laser metal deposition of a lean Cu–3.4 Cr–0.6 Nb (at%) conductive alloy hardened by Cr nano-scale precipitates and by Laves phase micro-particles10.1016/j.actamat.2020.07.035 ↗
53. Microstructures and properties of SLM-manufactured Cu-15Ni-8Sn alloy
54. In situ high-temperature X-ray diffraction characterization of silver sulfide, Ag2S10.1154/1.3583564 ↗
55. New Jersey, USA
56. Jones · 1985
57. Understanding of process and material behaviours in additive manufacturing of Invar36/Cu10Sn multiple material components via laser-based powder bed fusion
58. Microstructure characteristics and strengthening mechanism of semisolid CuSn10P1 alloys10.1016/j.matchar.2021.110898 ↗
59. 5 - Postprocessing challenges in metal AM: Strategies for achieving homogeneous microstructure in Ni-based superalloys
60. An additively manufactured AlCuMnZr alloy microstructure and tensile mechanical properties10.1016/j.mtla.2020.100758 ↗
61. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
62. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
63. Novel cooling rate correlations in molten metal gas atomization10.1007/s11663-019-01508-0 ↗
64. Laser shape variation influence on melt pool dynamics and solidification microstructure in laser powder bed fusion
65. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
66. Phase transformations in metals and alloys (revised reprint)
67. Grain refinement of aluminum alloys: part I. the nucleant and solute paradigms—a review of the literature10.1007/s11661-999-0098-5 ↗
68. Insight into the mechanisms of columnar to equiaxed grain transition during metallic additive manufacturing
69. Simultaneously enhanced strength and ductility of Cu-15Ni-8Sn alloy with periodic heterogeneous microstructures fabricated by laser powder bed fusion
70. Strengthening mechanisms of Mg Si alloys10.1016/1359-6454(96)00072-9 ↗
71. Multiscale defects enable synergetic improvement in yield strength of CrCoNi-based medium-entropy alloy fabricated via laser-powder bed fusion
72. The role of equiaxed particles on the yield stress of composites10.1016/0956-716X(91)90345-2 ↗
73. The microstructure evolution and properties of a Cu–Cr–Ag alloy during thermal-mechanical treatment10.1557/jmr.2017.17 ↗
74. Precipitation hardening in metals10.1179/026708399773002782 ↗
75. A model of ductile fracture based on the nucleation and growth of voids10.1016/0001-6160(81)90185-1 ↗
76. Full-composition-gradient in-situ alloying of Cu–Ni through laser powder bed fusion
77. Lattice distortion or cocktail effect dominates the performance of Tantalum-based high-entropy nitride coatings10.1016/j.apsusc.2021.151894 ↗
78. Wear resistance and electroconductivity in copper processed by severe plastic deformation10.1016/j.wear.2013.06.001 ↗
79. Effect of tool pin profile on the microstructure and tribological properties of friction stir processed Al-20 wt% Mg2Si composite10.1115/1.4044672 ↗
80. Improving the dry sliding-wear resistance of as-cast Cu-10Sn-1P alloy through accumulative back extrusion (ABE) process10.1016/j.jmrt.2020.07.022 ↗
81. Influence of precipitation hardening on the high-temperature sliding wear resistance of an aluminium alloyed iron-nickel base alloy10.1016/j.triboint.2020.106342 ↗
82. Dry sliding friction and wear properties of zinc-based alloys10.1016/S0043-1648(02)00050-9 ↗