Kinetics of Surface Reactions of Metals
Source abstract
Abstract
The reaction of iron with dilute, aqueous acetic acid was studied in a closed system with a nitrogen atmosphere at 34°C. The solution was sprayed on the metal continuously for periods up to 24 hr. The extent of reaction, determined gravimetrically, was found to be directly proportional to exposure time. The reaction rate was a function of acidity, flow rate, gaseous atmosphere composition, temperature, and nature of the adherent reaction products. Total activity and type of local activity changed with exposure conditions. This can be explained in terms of the defect structure of the film on the metal. Identity and properties of the films check with those described by others. It was concluded that ferrous acetate, ferrous carbonate, monobasic ferric acetate, anddibasic ferric acetate protect the underlying metal when formed as adherent, continuous films on the surface.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: nanoparticles nucleation surface interactions · Molecular Junctions and Nanostructures · Thermal and Kinetic Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.