High speed thermal imaging and modeling of laser powder bed fusion manufactured WC–Ni cemented carbides
Source abstract
Abstract
Cemented carbides such as cemented tungsten carbide (WC) are known for their use in resilient wear-resistant applications where hardness and thermal stability are imperative. They are composed of carbide particles embedded in a metal binder. Laser Powder Bed Fusion (L-PBF) is a favorable method to form cemented carbides into complex geometries, but composites pose unique challenges relative to metals typically processed by L-PBF. Resolving the melt pool temperature distributions in L-PBF is key to understanding the underlying physics of the fusion process. Using a two-color thermal imaging method, melt pool thermal maps of WC 0.83 -Ni 0.17 were captured with linear energy densities ranging from 500–1750 J/m with and without powder. WC 0.83 -Ni 0.17 melt pools exhibit temperatures above 4000 K, which can lead to the generation of other WC phases. Compared to more common L-PBF materials such as 316L stainless steel (SS), WC 0.83 -Ni 0.17 melt pools reach higher temperatures. Our direct measurements find that the thermal conductivity of WC 0.83 -Ni 0.17 is 30 W/m-K at 300 K, which is higher than the thermal conductivity of 316L SS and suggests that other heat transfer limitations must cause the elevated melt pool temperatures. A FLOW-3D CFD model based on the composite properties was compared to both the melt pool centerline temperatures and width measurements of the samples fabricated by L-PBF. The simulations indicate that specifying the onset of fluidity is key to reproducing the high temperatures observed experimentally. Although Ni has a melting point of 1728 K, the simulations do not match experiments unless the onset of fluidity is set at the melting point of WC (3143 K). Within FLOW-3D, the onset of fluidity is controlled by the critical solid fraction, which is a uniquely important parameter for simulating composite materials.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Cemented carbide microstructures: A review10.1016/j.ijrmhm.2018.12.004 ↗
2. A comprehensive review on the cutting and abrasive machining of cemented carbide materials10.1016/j.jmapro.2023.10.042 ↗
3. Schubert · 2010
4. On the microstructure and properties of an advanced cemented carbide system processed by selective laser melting10.1016/j.jallcom.2018.12.187 ↗
5. Materials science of cemented carbides—An overview10.1016/S0261-3069(01)00007-3 ↗
6. High-temperature fatigue of cemented carbides under cyclic loads10.1016/S0263-4368(99)00014-1 ↗
7. Cemented carbides
8. Chapter 1 - The history of the invention and early development of cemented carbides
9. Cemented carbides and cermets
10. Additive manufacturing of cemented tungsten carbide with a cobalt-free alloy binder by selective laser melting for high-hardness applications10.1007/s11837-019-03366-2 ↗
11. Process development and scale up of cemented carbide production
12. Microstructure and wear properties of laser deposited WC-12%Co composites10.1016/j.msea.2010.07.006 ↗
13. Environmental life cycle assessment of cemented carbide (WC-Co) production10.1016/j.jclepro.2018.10.272 ↗
14. Obtaining crack-free WC-Co alloys by selective laser melting10.1016/j.phpro.2016.08.091 ↗
15. Investigation on additive manufacturingof tungsten carbide-cobalt by selective laser melting10.1016/j.procir.2015.08.060 ↗
16. Process chain development for additive manufacturing of cemented carbide10.1016/j.jmapro.2018.05.036 ↗
17. Process development for the laser powder bed fusion of WC-Ni cermets using sintered-agglomerated powder
18. Sintering of wc-12% co processed by binder jet 3d printing (bj3dp) technology10.1016/j.ijrmhm.2017.10.023 ↗
19. Additive manufacturing of WC-13%Co by selective electron beam melting: Achievements and challenges10.1016/j.ijrmhm.2019.105028 ↗
20. Postprocessing of tungsten carbide-nickel preforms fabricated via binder jetting of sintered-agglomerated powder10.1111/ijac.14636 ↗
21. Machine-learning assisted optimization of process parameters for controlling the microstructure in a laser powder bed fused WC/Co cemented carbide
22. Controlling WC/Co two-phase microstructure of cemented carbides additive-manufactured by laser powder bed fusion: Effect of powder composition and post heat-treatment10.1016/j.matdes.2021.110034 ↗
23. Melt pool temperature and cooling rates in laser powder bed fusion
24. Online defect detection method and system based on similarity of the temperature field in the melt pool
25. Real-time measurement method of melt pool temperature in the directed energy deposition process10.1016/j.applthermaleng.2020.115475 ↗
26. High-resolution melt pool thermal imaging for metals additive manufacturing using the two-color method with a color camera
27. Two-color thermal imaging of the melt pool in powder-blown laser-directed energy deposition
28. Effects of powder attributes and laser powder bed fusion (l-pbf) process conditions on the densification and mechanical properties of 17-4 ph stainless steel10.1007/s11837-015-1770-4 ↗
29. Use of non-spherical hydride-dehydride (hdh) powder in powder bed fusion additive manufacturing
30. Effect of powder bed preheating on the crack formation and microstructure in ceramic matrix composites fabricated by laser powder-bed fusion process
31. Correlation of spatter behavior and process zone formation in powder bed fusion of metals10.1016/j.cirp.2020.04.092 ↗
32. Tungsten carbides
33. On thermal properties of metallic powder in laser powder bed fusion additive manufacturing10.1016/j.jmapro.2019.09.012 ↗
34. Instrumentation of broadband frequency domain thermoreflectance for measuring thermal conductivity accumulation functions10.1063/1.4808055 ↗
35. Malen · 2011
36. Kim · 1975
37. Effective thermal conductivity of particulate composites with interfacial thermal resistance10.1063/1.365209 ↗
38. Reference correlations for the thermal conductivity of liquid copper, gallium, indium, iron, lead, nickel and tin
39. Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
40. The effective medium theory of diffusion in composite media10.1111/j.1151-2916.1977.tb14091.x ↗
41. Laser shape variation influence on melt pool dynamics and solidification microstructure in laser powder bed fusion
42. Heat capacity and entropy of tungsten carbide10.1016/0021-9614(75)90241-4 ↗
43. Density and thermal expansion of high purity nickel over the temperature range from 150 k to 2030 k10.1007/s10765-015-1839-x ↗
44. Density of liquid niobium and tungsten and the estimation of critical point data10.1007/s11661-019-05262-5 ↗
45. Reliable data for high-temperature viscosity and surface tension: results from a european project10.1068/htwu323 ↗
46. Thermophysical properties of molten tungsten measured with an electrostatic levitator
47. A novel model for calculating the melting process of composite phase change materials10.1016/j.est.2020.101504 ↗
48. Surface tension of liquid nickel: Re-evaluated and revised data10.32908/hthp.v49.855 ↗
49. Evaluation of the surface tension of tungsten carbides wc and wc-w 2 c by the results of the laser diffraction analysis of their milling with iron powder10.3103/S1067821213060035 ↗