journal article·2026-04

Coarsening- and creep behavior of supersaturated Al-Zr-X (X = Mn, Cr, V, Mo, W) alloys processed by laser powder-bed fusion

Clement N. Ekaputra, Ekin Senvardarli, Christian Leinenbach, David C. Dunand

Publisher page

Abstract

We characterize the high-temperature microstructural evolution and creep properties of binary Al-0.4Zr and ternary Al-0.4Zr-1X (at%) alloys fabricated by laser-powder bed fusion ( L -PBF), where X = Mn, Cr, V, Mo, and W are slow-diffusing transition metals added for solid-solution strengthening. All alloys contain strengthening L12-Al3Zr nanoprecipitates which form during aging at 400°C. In the as-fabricated alloys, the ternary solute is nearly all in solid solution in the Mn- and Cr-containing alloys, and partially in solution in the V-, Mo-, and W-containing alloys, but still in amounts well beyond the equilibrium solubility limit for these elements. Solid solutions of the ternary solutes decompose during long-term aging at 400°C to form binary Al-X precipitates. The relative rates of precipitation of these elements are consistent with their relative diffusivities in Al: the precipitation rate is fastest for Mn, followed by Cr, then V, Mo, and W (the latter three elements remain almost entirely in solid solution after 2016 h exposure at 400°C). Nevertheless, the strengthening contribution from the ternary solute at room temperature does not significantly differ among the five studied alloys or as a function of aging time at 400°C, indicating a stable strengthening contribution from Mn, Cr, V, Mo, and W in Al. During creep deformation at 400°C, all ternary alloys show significantly higher creep resistance than a binary Al-Zr alloy. Furthermore, their creep resistance is comparable to those of additively-manufactured alloys with significantly higher volume fractions of strengthening phases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing
2. Solute trapping and non-equilibrium microstructure during rapid solidification of additive manufacturing10.1038/s41467-023-43563-x ↗
3. Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
4. Modeling and measurements of creep deformation in laser-melted Al-Ti-Zr alloys with bimodal grain size10.1016/j.actamat.2023.119493 ↗
5. Microstructure and mechanical properties of as-processed scandium-modified aluminium using selective laser melting10.1016/j.cirp.2016.04.057 ↗
6. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
7. Intensive processing optimization for achieving strong and ductile Al-Mn-Mg-Sc-Zr alloy produced by selective laser melting
8. Al–Mn–Cr–Zr-based alloys tailored for powder bed fusion-laser beam process: Alloy design, printability, resulting microstructure and alloy properties10.1557/s43578-022-00533-1 ↗
9. An additively manufactured AlCuMnZr alloy microstructure and tensile mechanical properties10.1016/j.mtla.2020.100758 ↗
10. Additively manufactured novel Al-Cu-Sc-Zr alloy: Microstructure and mechanical properties
11. Microstructure and tensile property of a novel AlZnMgScZr alloy additively manufactured by gas atomization and laser powder bed fusion10.1016/j.scriptamat.2018.08.025 ↗
12. First-principles studies on lattice constants and local lattice distortions in solid solution aluminum alloys10.1016/j.commatsci.2012.08.037 ↗
13. Selective laser melting of a high strength Al Mn Sc alloy: Alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
14. Structure and Properties of Al-W, Al-Mo, and Al-Nb Alloys Obtained from Granules
15. Rapid Solidification of Aluminum-rich Al-V Alloys10.1016/0025-5416(88)90156-5 ↗
16. Metastable phase formation in rapidly solidified Al-Mo alloys10.1179/mst.1989.5.2.123 ↗
17. Phase transformations in Al-rich Al-W alloys rapidly quenched from the melt10.1007/BF00550695 ↗
18. Solute-induced strengthening during creep of an aged-hardened Al-Mn-Zr alloy10.1016/j.actamat.2021.117268 ↗
19. Combining solution-, precipitation-, and load-transfer strengthening in a cast Al-Ce-Mn-Sc-Zr alloy10.1016/j.actamat.2024.119683 ↗
20. Tensile creep mechanisms of Al-Mn-Sc alloy fabricated by additive manufacturing
21. Solute-diffusion-controlled dislocation creep in pure aluminium containing 0.026 at% Fe10.1080/14786430410001690006 ↗
22. Rate-controlling processes in creep of subgrain containing aluminum materials10.1016/j.msea.2005.08.077 ↗
23. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
24. Effects of Zn and Cr additions on precipitation and creep behavior of a dilute Al–Zr–Er–Si alloy10.1016/j.actamat.2019.09.055 ↗
25. Effect of vanadium micro-alloying on the microstructural evolution and creep behavior of Al-Er-Sc-Zr-Si alloys10.1016/j.actamat.2016.11.033 ↗
26. Individual and synergistic effects of Mn and Mo micro-additions on precipitation and strengthening of a dilute Al–Zr-Sc-Er-Si alloy10.1016/j.msea.2020.140288 ↗
27. Effect of microadditions of Mn and Mo on dual L12- and α-precipitation in a dilute Al-Zr-Sc-Er-Si alloy10.1016/j.matchar.2020.110585 ↗
28. Effects of W and Si microadditions on microstructure and the strength of dilute precipitation-strengthened Al–Zr–Er alloys10.1016/j.msea.2020.140159 ↗
29. Microstructure and mechanical properties of Al-Cu alloys fabricated by selective laser melting of powder mixtures10.1016/j.jallcom.2017.10.168 ↗
30. Efficacy of elemental mixing of in situ alloyed Al-33wt%Cu during laser powder bed fusion10.1016/j.jmatprotec.2021.117379 ↗
31. Thermodynamic re-assessment of the Al-Co-W system10.1016/j.calphad.2017.09.007 ↗
32. A high strength Al-2Ni-0.5Zr conductor alloy fabricated via laser powder bed fusion10.1016/j.msea.2025.149251 ↗
33. Precipitation evolution in Al–Zr and Al–Zr–Ti alloys during aging at 450–600°C10.1016/j.actamat.2007.11.011 ↗
34. A study of phase equilibria in the Al-rich part of the Al-Mn alloy system10.3139/146.101768 ↗
35. Al-Cr (Aluminum-Chromium)10.1007/s11669-007-9225-4 ↗
36. The Al-V Phase Diagram between 0 and 50 Atomic Percent Vanadium
37. Al-Mo (Aluminum-Molybdenum)10.1007/s11669-010-9758-9 ↗
38. On the threshold stress for dislocation creep in particle strengthened alloys10.1016/0001-6160(85)90018-5 ↗
39. Creep behavior and threshold stress of an extruded Al–6Mg–2Sc–1Zr alloy10.1016/j.msea.2004.05.025 ↗
40. Karnesky · 2007
41. Highly stable coherent nanoprecipitates via diffusion-dominated solute uptake and interstitial ordering10.1038/s41563-022-01420-0 ↗
42. Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion
43. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
44. An additively manufactured near-eutectic Al-Ce-Ni-Mn-Zr alloy with high creep resistance10.1016/j.actamat.2024.119787 ↗
45. Creep properties and microstructure evolution at 260–300 °C of AlSi10Mg manufactured via laser powder-bed fusion10.1016/j.msea.2022.143075 ↗
46. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
47. Precipitation in Rapidly Solidified Al-Mn Alloys10.1007/BF02646833 ↗
48. Microstructure and mechanical properties of rapidly solidified Al-Cr alloys10.1007/s11595-009-3424-2 ↗
49. Rapidly solidified Al-Cr alloys: structure and decomposition behavior10.1007/BF00547923 ↗
50. Continuous heating of rapidly solidified AI-Cr ribbons10.1007/BF01174508 ↗
51. Microstructures and mechanical properties of aluminum-transition metal binary alloys (Al-Fe, Al-Mn, and Al-Cr) processed by laser powder bed fusion10.1016/j.jallcom.2021.159680 ↗
52. Origin of non-uniform plasticity in a high-strength Al-Mn-Sc based alloy produced by laser powder bed fusion10.1016/j.jmst.2021.06.042 ↗
53. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
54. Precipitation sequence in Al-Sc-Zr alloys revisited10.1016/j.mtla.2022.101608 ↗
55. Synergetic effect of Er and Zr on the precipitation hardening of Al–Er–Zr alloy10.1016/j.scriptamat.2011.06.033 ↗
56. Role of silicon in accelerating the nucleation of Al3(Sc,Zr) precipitates in dilute Al–Sc–Zr alloys10.1016/j.actamat.2012.05.036 ↗
57. Enhanced dispersoid precipitation and dispersion strengthening in an Al alloy by microalloying with Cd10.1016/j.actamat.2018.07.001 ↗
58. Enhanced age-hardening response and creep resistance of an Al-0.5Mn-0.3Si (at%) alloy by Sn inoculation10.1016/j.actamat.2022.118344 ↗
59. Coarsening- and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
60. Glide and climb resistance to the motion of an edge dislocation due to dragging a Cottrell atmosphere10.1080/01418617908234833 ↗
61. Distribution of solute atoms round a slow dislocation
62. R. Sandstrom, Basic Modeling and Theory of Creep of Metallic Materials, Springer.
63. A. Liang, N. Bertin, X. Zhou, S. Aubry, V.V. Bulatov, Atomistic insights into solid solution strengthening: size misfit versus stiffness misfit, arXiv preprint arXiv:2502.19637 (2025).
64. First-principles study of solute-dislocation interaction in aluminum-rich alloys10.1103/PhysRevB.64.224203 ↗
65. Solute strengthening from first principles and application to aluminum alloys10.1016/j.actamat.2012.03.037 ↗
66. Modelling mechanical properties for non-hardenable aluminium alloys10.1016/j.commatsci.2007.03.013 ↗